Brass reference / Leaded brass
C330 low-leaded brass tube
A tube grade with just enough lead to machine cleanly, for parts made from tube rather than solid bar.
Also known as Low leaded brass, Leaded brass tube, Alloy 330. Published typical values for the alloy, never a promise from a shop.
Composition
| Element | Nominal weight % |
|---|---|
| Copper | 65.0 to 68.0 |
| Lead | 0.25 to 0.7 |
| Iron | 0.07 max |
| Zinc | remainder |
Properties
- UNSC33000
- EN equivalentNo close EN grade
- DINNone
- JISNone listed
- BSNone
- Hardness50 to 80 HRB
- Density8.50 g/cm3
- Typical tolerance±0.05 mm on wall, tighter where machined
- Common formsSeamless tube
What it is for, and what it is not
Specify it for
- Cylinders, liners, sleeves and bushings machined from tube
- Fittings where a tube blank saves most of the material
- Pump and power cylinder bodies
Do not specify it for
- Parts that could be turned from solid bar, C360 cuts faster
- Potable water parts, it sits above the 0.25 percent line and dezincifies
- Hot water service
What a buyer should know
Tube is the cheapest way to start a hollow brass part, and this is the tube grade made for machining. The small lead addition breaks the chip enough to bore and part off cleanly without the ductility loss of a full 3 percent. Ask the shop whether tube or bar is cheaper for your part before you specify either.
Nominal lead is 0.25 to 0.7 percent, which is above the 0.25 percent weighted average limit that NSF/ANSI 372 sets for wetted potable water surfaces. See NSF/ANSI 61 and 372 and RoHS exemption 6(c).
Dezincification resistance is poor, so this alloy is the wrong choice sitting in hot water or seawater regardless of how well it machines. See dezincification and the grades that resist it.
Closest alternatives
| Alloy | Lead % | Mach. | DZR | Why you might switch |
|---|---|---|---|---|
| C377 forging brassC37700 | 1.5 to 2.5 | 80 | Poor | Hot forged to a near net shape then machined only where a sealing face or thread requires it. |
| C69300 silicon brassC69300 | under 0.09 | 80 | High | The usual lead-free answer for potable water, roughly twice as strong as C360 and highly dezincification resistant. |
| Bismuth brassC49300 / C49350 | under 0.25 | 80 | Moderate | Bismuth replaces lead as the chip breaker, so it behaves closest to C360 on an existing C360 program. |
Need a shop that runs C330?
Send the drawing. We reply within 24 business hours with one itemised quote for the finished parts.