Brass Alloy Cross Reference: UNS, EN, DIN, JIS and BS

A US drawing says C36000. A German one says CuZn39Pb3 or 2.0401. A Japanese one says C3604BD. This table puts them side by side for 16 brasses.

Equivalents are nearest matches, not identical specifications. Composition ranges and impurity limits differ between systems, so confirm against the standard before you substitute. Where a system has no close grade the cell says so. Free to use and to cite.

Leaded machining and forging brasses

Common nameUNSEN symbol / CWDINJISBSLead %Mach.
C360 free-cutting brassFree machining brassC36000CuZn36Pb3 / CW603N2.0375 CuZn36Pb3C3601 / C3602 (nearest)CZ1242.5 to 3.7100
C385 architectural bronzeArchitectural bronzeC38500CuZn39Pb3 / CW614N2.0401 CuZn39Pb3C3604 (nearest)CZ121 Pb32.5 to 3.590
C377 forging brassForging brassC37700CuZn39Pb2 / CW612N2.0380 CuZn39Pb2C3771CZ1221.5 to 2.580
CW602N DZR brassCZ132No direct UNS equivalentCuZn36Pb2As / CW602N2.0371 CuZn36Pb2AsNo direct JIS gradeCZ1321.7 to 2.880
C353 high-leaded brassHigh leaded brassC35300CuZn37Pb2 / CW608N (nearest)2.0380 CuZn37Pb2 (nearest)C3560 (nearest)CZ1191.5 to 2.590
C345 leaded brassLeaded brassC34500CuZn37Pb2 / CW608N (nearest)2.0380 CuZn37Pb2 (nearest)C3601 (nearest)CZ1191.5 to 2.590
C330 low-leaded brass tubeLow leaded brassC33000No close EN gradeNoneNone listedNone0.25 to 0.760
CW617N CuZn40Pb2CuZn40Pb2C37700 (nearest)CuZn40Pb2 / CW617N2.0402 CuZn40Pb2C3771CZ1221.6 to 2.580

Lead-free brasses

Common nameUNSEN symbol / CWDINJISBSLead %Mach.
C69300 silicon brassEco BrassC69300CuZn21Si3P / CW724RNo DIN number, sold as Eco BrassNo JIS grade, sold as Eco BrassNoneunder 0.0980
Bismuth brassFederalloyC49300 / C49350No single EN equivalent, see supplier specNoneNoneNoneunder 0.2580
CW511L lead-free brassCuZn38AsC27450 (nearest, without arsenic)CuZn38As / CW511LNone in common useNoneNoneunder 0.240

Tin brasses for water

Common nameUNSEN symbol / CWDINJISBSLead %Mach.
C464 naval brassNaval brassC46400CuZn38Sn1 / CW712R2.0530 CuZn38Sn1C4641CZ112under 0.2030
C443 admiralty brassAdmiralty brassC44300CuZn28Sn1As / CW706R2.0470 CuZn28Sn1C4430CZ111under 0.0730

Forming brasses

Common nameUNSEN symbol / CWDINJISBSLead %Mach.
C260 cartridge brassCartridge brassC26000CuZn30 / CW505L2.0265 CuZn30C2600CZ106trace30
C230 red brassRed brassC23000CuZn15 / CW502L2.0240 CuZn15C2300CZ102under 0.0530
C280 Muntz metalMuntz metalC28000CuZn40 / CW509L2.0360 CuZn40C2800CZ1090.30 max40

Three traps in brass naming

Each of these has put the wrong bar on a lathe.

  • JIS is not UNSJIS C3604 looks like C360 with a digit moved. It is closer to CW614N and C385, with less copper. JIS C3601 and C3602 are the nearer matches for C360.
  • Bronze that is brassC385 is sold as architectural bronze and is a leaded brass. Read the UNS number, not the trade name.
  • Same symbol, different leadCuZn39Pb3 (CW614N) and CuZn39Pb2 (CW612N) differ by one digit and by about 1 percent lead. On a drinking water part that digit is the whole question.

How to read each system

  • UNSC plus five digits. C1xxxx to C7xxxx wrought, C8xxxx and C9xxxx cast. C36000 is written C360 in speech and on most drawings.
  • ENA six character number under EN 1412, CW614N, paired with a symbol under EN 1173, CuZn39Pb3. CW is copper wrought. The last letter is the alloy group: L for copper-zinc, N for copper-zinc-lead, R for other copper-zinc alloys.
  • DINThe older German material number, 2.0401, with the same symbol. Still on many drawings and datasheets.
  • JISC plus four digits under JIS H 3250 for bar, H 3100 for sheet, H 3300 for tube. A suffix gives the form: BD drawn bar, BE extruded bar, T tube.
  • BSThe withdrawn BS 2874 CZ numbers, CZ121, CZ132. UK drawings still carry them and the EN grade is the current equivalent.

The standards themselves are listed on the standards index. Each alloy has a full datasheet on the alloy reference.

Drawing in another system? Send it as it is.

We read UNS, EN, DIN and JIS callouts and match the part to shops that stock the nearest grade. Reply within 24 business hours.

Get a quote