Skip to content
Brass CNC Parts

Brass reference / Lead-free brass

CW511L lead-free brass

The European lead-free drinking water brass, dezincification resistant through arsenic, and much slower to machine than C360.

Also known as CuZn38As, Arsenical lead-free brass, EU drinking water brass. Published typical values for the alloy, never a promise from a shop.

40Machinability, C360 = 100
under 0.2%Lead, under the 0.25% line
HighDezincification resistance
320 to 440 MPaTypical tensile strength

Composition

ElementNominal weight %
Copper61.5 to 63.5
Arsenic0.02 to 0.15
Lead0.2 max
Iron0.1 max
Zincremainder

Properties

  • UNSC27450 (nearest, without arsenic)
  • EN equivalentCuZn38As / CW511L
  • DINNone in common use
  • JISNone
  • BSNone
  • Hardness50 to 70 HRB
  • Density8.44 g/cm3
  • Typical tolerance±0.02 mm typical, slower to hold than C360
  • Common formsRod, bar and hot stamping billet

What it is for, and what it is not

Specify it for

  • EU drinking water fittings under the 4MS common approach and national lists such as the German UBA list
  • Hot stamped water fittings that must be lead-free and DZR
  • Parts where corrosion resistance matters more than cycle time

Do not specify it for

  • High volume turned parts on cost, it is rated near 40
  • Shops that have not tuned tooling for a long chipping brass
  • Parts that need the strength of C69300 silicon brass

What a buyer should know

A plain 62/38 brass with an arsenic addition and the lead taken out. The arsenic gives dezincification resistance, and the missing lead makes it a long chipping alloy that wants sharp positive tooling, chip breakers and lower feeds. It is one of the two alloys European water fitting makers moved to when the 4MS lead limits arrived, the other being CW724R silicon brass, which cuts better and costs more.

Closest alternatives

AlloyLead %Mach.DZRWhy you might switch
C280 Muntz metalC280000.30 max40PoorThe 60/40 hot working brass, supplied as plate and sheet, machinable but not free cutting.
C464 naval brassC46400under 0.2030HighAbout 1 percent tin added for seawater and dezincification resistance, at a heavy cost in machinability.
C260 cartridge brassC26000trace30PoorMade for deep drawing and cold forming, not for cutting, and rated 30 against C360 at 100.

All 16 alloys compared · Cross reference

Need a shop that runs CW511L?

Send the drawing. We reply within 24 business hours with one itemised quote for the finished parts.