C280 Muntz metal

The 60/40 hot working brass, supplied as plate and sheet, machinable but not free cutting.

Also known as Muntz metal, 60/40 brass, Alloy 280, Yellow metal. Published typical values for the alloy, never a promise from a shop.

40Machinability, C360 = 100
0.30 max%Lead, over the 0.25% line
PoorDezincification resistance
370 to 510 MPa depending on temperTypical tensile strength

Composition

ElementNominal weight %
Copper59.0 to 63.0
Lead0.30 max
Iron0.07 max
Zincremainder

Properties

  • UNSC28000
  • EN equivalentCuZn40 / CW509L
  • DIN2.0360 CuZn40
  • JISC2800
  • BSCZ109
  • Hardness55 to 80 HRB
  • Density8.39 g/cm3
  • Typical tolerance±0.05 mm typical on plate
  • Common formsPlate, sheet, rod, brazing rod

What it is for, and what it is not

Specify it for

  • Condenser tube sheets and plates
  • Large architectural panels and trim
  • Brazing rod and heavy sections hot formed then machined
  • Large nuts, bolts and marine hardware in plate form

Do not specify it for

  • Turned parts from bar, C360 or C385 are the stocked bar grades
  • Potable water parts, the lead limit is marginal and it dezincifies
  • Seawater without cathodic protection, use naval brass instead

What a buyer should know

Same copper level as C360 with the lead taken out, which turns it from a free-cutting bar alloy into an alpha-beta plate alloy that hot works well and machines moderately. It is the alloy behind naval brass: add 1 percent tin to Muntz metal and you have C464. When it appears on a machining drawing it is almost always a plate part.

Nominal lead is 0.30 max percent, which is above the 0.25 percent weighted average limit that NSF/ANSI 372 sets for wetted potable water surfaces. See NSF/ANSI 61 and 372 and RoHS exemption 6(c).

Dezincification resistance is poor, so this alloy is the wrong choice sitting in hot water or seawater regardless of how well it machines. See dezincification and the grades that resist it.

Closest alternatives

AlloyLead %Mach.DZRWhy you might switch
CW511L lead-free brassC27450 (nearest, without arsenic)under 0.240HighThe European lead-free drinking water brass, dezincification resistant through arsenic, and much slower to machine than C360.
C464 naval brassC46400under 0.2030HighAbout 1 percent tin added for seawater and dezincification resistance, at a heavy cost in machinability.
C260 cartridge brassC26000trace30PoorMade for deep drawing and cold forming, not for cutting, and rated 30 against C360 at 100.

All 16 alloys compared · Cross reference