Home / Standards
Standards for Machined Brass Parts, by Market
45 standards, rules and naming systems a brass drawing can cite, with what each one covers and what to write. US, EU, UK, Japan, Korea and Australia.
This is a reference for buyers writing a drawing. Nothing here is a claim that any part, any shop or this site meets a standard. Where a rule sets a number we give the number and the date we checked it. None of it is legal advice.
Lead and drinking water
| Standard | Market | What it covers | What to write, or why it matters |
|---|---|---|---|
| NSF/ANSI/CAN 372Drinking water system components, lead content | US | Defines how the weighted average lead content of the wetted surfaces of a pipe, fitting or fixture is calculated and verified. The limit is 0.25 percent. Solder and flux carry a separate 0.2 percent limit. | Write "wetted surfaces to NSF/ANSI 372, 0.25 percent weighted average lead" and leave the alloy open to any grade that clears it. A single alloy name closes off cheaper compliant options.lead content calculator · nsf 61 372 brass fittings |
| NSF/ANSI/CAN 61Drinking water system components, health effects | US | A leaching standard. The finished product is tested for what it releases into water, lead included, rather than judged on composition alone. Certification is granted to a named product from a named manufacturer. | Name it if the end product will be certified. A subcontract shop cannot certify a custom part to NSF/ANSI 61 on its own, so the drawing should say who owns that step.nsf 61 372 brass fittings |
| SDWA Section 1417US Safe Drinking Water Act, use of lead free pipes, fittings, fixtures, solder and flux | US | The federal law behind the 0.25 percent figure since the Reduction of Lead in Drinking Water Act took effect in January 2014. The 2020 EPA rule under it requires third party certification of lead free status for covered products. Not legal advice. | You do not cite the Act on a drawing. You cite NSF/ANSI 372, which is how the Act is met in practice.nsf 61 372 brass fittings |
| California AB 1953California Health and Safety Code 116875, lead in plumbing | US | The 2006 California law, in force from 1 January 2010, that first set the 0.25 percent weighted average definition of lead free. The federal law later copied it. Vermont, Maryland and Louisiana passed similar rules. | Nothing extra once NSF/ANSI 372 is on the drawing. Worth knowing because older specifications still cite AB 1953 by name.nsf 61 372 brass fittings |
| California Proposition 65Safe Drinking Water and Toxic Enforcement Act of 1986 | US | A labelling law, not a material limit. Lead is a listed substance, so a leaded brass part sold into California may need a Proposition 65 warning on the product or packaging. Not legal advice. | A packaging and labelling question for the buyer, not the shop. Mention it in the RFQ if the shop is packaging the finished product. |
| Directive (EU) 2020/2184EU Drinking Water Directive, recast | EU | Sets hygiene requirements for materials in contact with drinking water across the EU and introduces European positive lists of permitted materials, replacing national schemes. The first positive lists apply from 31 December 2026. Not legal advice. | For an EU water fitting, specify a copper alloy on the relevant positive list. Until the European lists apply, national lists such as the German UBA list are what fitting makers work to.cw511l lead free brass · c69300 silicon brass |
| 4MS Common ApproachFour member state common approach, composition list for metallic materials | EU | A shared list of copper alloy compositions accepted for drinking water contact, maintained by Germany, France, the Netherlands and the UK. It is the basis of the German UBA metal list and the model for the EU positive lists. | Specify a listed alloy such as CW511L or CW724R and say "4MS listed composition". CW617N and CW614N are not on the list for wetted parts.cw511l lead free brass · cw617n cuzn40pb2 |
| UBA metal listUmweltbundesamt evaluation basis for metallic materials in contact with drinking water | Germany | The German positive list of metallic materials for drinking water, derived from the 4MS list. Only listed alloys may be used in German drinking water installations. | For a part sold into Germany, name the alloy by its CW number and state that it is on the UBA list. The shop supplies the alloy, the buyer owns the product approval. |
| WRASWater Regulations Approval Scheme | UK | The UK approval scheme for fittings and materials in contact with drinking water. Approval attaches to a product, and for brass the accepted compositions follow the 4MS list. | Name it only if the finished product will be submitted for approval. A machined component on its own is not WRAS approved. |
| ACSAttestation de Conformité Sanitaire | France | The French approval for materials and products in contact with drinking water. Copper alloys follow the 4MS composition list. | As for WRAS: name it when the product is going for approval, and specify a 4MS listed alloy. |
| JIS S 3200-7Water supply equipment, test method for leaching performance | Japan | The Japanese leaching test for water supply fittings, referenced by the water quality standards for tap water. A Japanese water fitting is tested for what it releases rather than judged on composition alone. | Japanese buyers will normally specify a lead free brass developed for their market and the leaching test on the finished product. The shop supplies the alloy on the drawing. |
| AS/NZS 4020 and NCC lead limitTesting of products for use in contact with drinking water, and the National Construction Code lead free requirement | Australia | AS/NZS 4020 is the leaching test. The National Construction Code separately requires copper alloy plumbing products in contact with drinking water to have a weighted average lead content of not more than 0.25 percent, with the transition period ending 1 May 2026. Not legal advice. | Same wording as NSF/ANSI 372: 0.25 percent weighted average lead on wetted surfaces. Name AS/NZS 4020 if the product goes for WaterMark certification. |
Alloy composition and product forms
| Standard | Market | What it covers | What to write, or why it matters |
|---|---|---|---|
| ASTM B16/B16MFree-cutting brass rod, bar and shapes for use in screw machines | US | The product standard for C360 bar. Composition, tempers (half hard is the usual), dimensional tolerances and straightness for round, hex and square bar. | Write "C36000 per ASTM B16, half hard" rather than "brass". That is a complete material callout a shop can buy against.c360 free cutting brass |
| ASTM B453/B453MCopper-zinc-lead alloy (leaded brass) rod, bar and shapes | US | The product standard for the lower lead leaded brasses such as C345 and C353, in rod and bar form. | Cite it when the drawing calls for a leaded grade other than C360.c345 leaded brass · c353 high leaded brass · astm b453 |
| ASTM B124/B124MCopper and copper alloy forging rod, bar and shapes | US | The stock standard for forging brass, C377 included. Covers the rod and bar a forge buys before it becomes a near net shape. | For a forged then machined part write the alloy per B124 for the stock and B283 for the forging itself.c377 forging brass · brass hot forging vs machining |
| ASTM B283/B283MDie forgings, copper and copper alloy, hot pressed | US | The standard for the hot pressed forging as delivered: alloy, mechanical properties and the inspection the forging is supplied to. | Cite it on the forging drawing. The machining drawing then references the forging drawing.brass hot forging vs machining |
| ASTM B371/B371MCopper-zinc-silicon alloy rod | US | The product standard for silicon brass rod, including C69300, the usual lead free grade for potable water parts. | Write "C69300 per ASTM B371". It tells the shop the bar is a standard product rather than a special order.c69300 silicon brass · astm b371 |
| ASTM B135/B135MSeamless brass tube | US | Covers seamless brass tube in grades such as C230, C260 and C330, for parts that start as tube rather than solid bar. | Cite it when a hollow part should be made from tube. Ask the shop first whether tube or bar is cheaper for the geometry.c330 low leaded brass tube · brass bar stock sizes forms · astm b135 |
| EN 12164Copper and copper alloys, rod for free machining purposes | EU | The European counterpart of ASTM B16. Composition, tempers and tolerances for free machining rod, with CW614N and CW603N the common grades. | European drawings write "CW614N per EN 12164, R430" where R430 is the minimum tensile strength in MPa. Match that form.cross reference |
| EN 12165Copper and copper alloys, wrought and unwrought forging stock | EU | The European stock standard for hot stamping brass. CW617N is the usual grade. | Cite it for the billet on a European hot stamped part.cw617n cuzn40pb2 · en 12165 |
| EN 12167Copper and copper alloys, profiles and bars for general purposes | EU | Covers extruded profiles and bars that are not sold specifically as free machining rod, including architectural sections. | Cite it when the part starts as an extruded profile rather than round or hex bar.c385 architectural bronze |
| EN 12168Copper and copper alloys, hollow rod for free machining purposes | EU | Free machining brass supplied as hollow rod, so a part with a large bore starts with most of the material already removed. | Worth asking about on any part with a through bore over roughly half the outside diameter, in volume. |
| EN 1254Copper and copper alloys, plumbing fittings | EU | The product standard series for European plumbing fittings: capillary, compression, press and threaded ends, with the materials and tests each type needs. | Cite the relevant part if the machined part is itself a plumbing fitting sold into the EU.en 1254 |
| JIS H 3250Copper and copper alloy rods and bars | Japan | The Japanese rod and bar standard, where C3604 free cutting brass and C3771 forging brass are defined. | A Japanese drawing says "C3604BD" for drawn free cutting brass bar. The cross reference page maps it to UNS and EN.cross reference |
| JIS H 3100Copper and copper alloy sheets, plates and strips | Japan | The Japanese flat product standard, covering C2600 and the other forming brasses in sheet and plate. | Cite it for a Japanese drawing of a milled plate part. |
| KS D 5101Copper and copper alloy rods and bars | Korea | The Korean rod and bar standard, closely aligned with JIS H 3250, using the same C3604 and C3771 style designations. | Treat a KS designation as its JIS counterpart on the cross reference page and confirm with the buyer.cross reference |
Corrosion and stress tests
| Standard | Market | What it covers | What to write, or why it matters |
|---|---|---|---|
| ISO 6509-1Corrosion of metals and alloys, determination of dezincification resistance of copper alloys with zinc | International | The dezincification test. A sample is exposed to copper chloride solution for 24 hours and sectioned to measure how deep the zinc has leached. A maximum depth, commonly 200 micrometres, is the acceptance criterion. | For a hot water or marine part write "dezincification resistant to ISO 6509, max depth 200 um" and ask for the result on the mill certificate.dezincification resistant brass · cw602n dzr brass |
| ISO 6957Copper alloys, ammonia test for stress corrosion resistance | International | Exposes a part to ammonia vapour to reveal residual tensile stress that would cause stress corrosion cracking in service. | Specify a stress relief after machining, typically 330 to 350 C, on any cold worked or heavily machined brass part going into an ammonia or moist environment, and name this test if you want proof.brass stress corrosion cracking · scc tests iso 6957 astm b858 |
| ASTM B858Ammonia vapor test for determining susceptibility to stress corrosion cracking in copper alloys | US | The US equivalent of ISO 6957, using ammonia vapour at a controlled pH. | Interchangeable with ISO 6957 in intent. Cite whichever the end customer recognises.brass stress corrosion cracking · scc tests iso 6957 astm b858 |
| ASTM B154Mercurous nitrate test for copper alloys | US | The older residual stress test. Still cited on legacy drawings, but most laboratories have replaced it with the ammonia test because of the mercury. | If an old drawing cites B154, ask whether B858 or ISO 6957 is acceptable instead.scc tests iso 6957 astm b858 |
Threads and features
| Standard | Market | What it covers | What to write, or why it matters |
|---|---|---|---|
| ASME B1.20.1Pipe threads, general purpose, inch (NPT) | US | Defines NPT, the tapered thread that seals on the thread flanks with a sealant. Gauging is by L1 ring and plug gauges. | Write "1/2-14 NPT per ASME B1.20.1" and state that it is a sealing thread so the shop quotes gauging.brass thread standards npt bspp · brass thread chart · asme b1 20 1 npt |
| ISO 228-1Pipe threads where pressure tight joints are not made on the threads (G, BSPP) | International | The parallel pipe thread. It does not seal on the thread, so a washer, O-ring or bonded seal does the work. | Write "G1/4 per ISO 228-1, class A" and show the sealing face. A G thread mated to an NPT is the classic leak.brass thread standards npt bspp · brass thread chart · iso 228 1 g threads |
| ISO 7-1 and EN 10226-1Pipe threads where pressure tight joints are made on the threads (R, Rp, BSPT) | International | The tapered BSP thread. R is the external taper, Rp the internal parallel that accepts it. Same 55 degree form as G, different function. | Write "R1/2 per ISO 7-1" for the taper and never mix it with NPT, which is 60 degrees.brass thread standards npt bspp |
| ASME B1.1Unified inch screw threads (UN and UNR) | US | The standard for UNC and UNF threads and their classes, 2A and 2B being the common fit. | Write the class. "1/4-20 UNC-2A" is complete, "1/4-20" is not.brass thread chart |
| ISO 965-1ISO general purpose metric screw threads, tolerances | International | Defines the tolerance classes for metric threads. 6g external and 6H internal are the defaults. | Write "M10 x 1.0-6g". A thread with no class is quoted as 6g and gauged as 6g.brass thread chart |
| DIN 82Knurls | Germany | The European knurl standard. Defines the pattern codes such as RAA for straight and RGE for diamond, and the pitch series. | Write "RGE 1.0 DIN 82" rather than "diamond knurl". The shop then knows the pattern, the pitch and the tooling.knurling brass parts · brass knurled knobs thumb screws |
| ANSI B94.6Knurling | US | The US knurl standard, based on diametral pitch and tooth count rather than linear pitch. | Write the diametral pitch and pattern, for example "96 DP diamond knurl per ANSI B94.6". Give the blank diameter and the finished diameter as a reference.knurling brass parts |
Certificates and inspection
| Standard | Market | What it covers | What to write, or why it matters |
|---|---|---|---|
| EN 10204Metallic products, types of inspection documents | EU | Defines the certificate types. A 2.1 is a statement of compliance, a 2.2 a test report from non specific inspection, a 3.1 an inspection certificate from the mill with actual results for the lot, a 3.2 the same countersigned by an independent inspector. | Ask for a 3.1 on any part where the alloy is doing compliance work. It gives you the lead figure for your lot, which is the number for a real NSF/ANSI 372 submission.brass material certificates en 10204 · brass part quality checks |
| ISO 9001Quality management systems, requirements | International | A management system standard, not a product standard. A shop may hold a certificate. This site holds none and never states that a shop does. Ask the shop for its certificate directly. | It belongs in the supplier questionnaire, not on the drawing. Ask for the certificate number and the certifying body and check it.how to choose brass machining supplier |
| ISO 2768-1General tolerances for linear and angular dimensions without individual tolerance indications | International | The default tolerance classes, f, m, c and v, that apply to every untoleranced dimension on a drawing that cites it. | Write "ISO 2768-m" in the title block. Without it, every untoleranced dimension is a negotiation.brass tolerances surface finish |
Electronics and chemicals
| Standard | Market | What it covers | What to write, or why it matters |
|---|---|---|---|
| RoHS Directive 2011/65/EU, Annex III 6(c)Exemption for copper alloy containing up to 4 percent lead by weight | EU | The exemption that lets leaded brass be used in electrical and electronic equipment sold in the EU. Its expiry was set at 30 June 2027, and a renewal request submitted in December 2025 suspends the date pending a Commission decision. Status as of September 2026. Not legal advice. | For an electronic part write the RoHS requirement and say whether the 6(c) exemption is being relied on. If not, the alloy has to be lead free.rohs exemption 6c leaded brass 2027 |
| REACH Regulation (EC) 1907/2006Registration, evaluation, authorisation and restriction of chemicals | EU | Lead metal is on the Candidate List of substances of very high concern, so an article containing over 0.1 percent lead by weight carries a communication duty down the supply chain under Article 33. Annex XVII also restricts lead in specific consumer articles. Not legal advice. | Ask the shop for the alloy composition on the certificate so you can meet your own Article 33 duty. That is a paperwork request, not a machining one.rohs exemption 6c leaded brass 2027 |
Naming systems
| Standard | Market | What it covers | What to write, or why it matters |
|---|---|---|---|
| UNS (ASTM E527, SAE J1086)Unified Numbering System for metals and alloys | US | The C36000 style numbers. C1xxxx to C7xxxx are wrought, C8xxxx and C9xxxx are cast. The common three digit names (C360) are the middle of the UNS number. | Write the full UNS number once. "C36000" is unambiguous, "brass 360" and "yellow brass" are not.cross reference |
| EN 1412 and EN 1173European material designation: CW numbers and symbols | EU | EN 1412 gives the six character number, CW614N, where CW means copper wrought and the last letter is the alloy group. EN 1173 gives the symbol, CuZn39Pb3. Older DIN numbers such as 2.0401 still appear. | Write the CW number and the symbol together. The cross reference page maps them to UNS and JIS.cross reference |
| JIS designationsJapanese Industrial Standards copper alloy numbering | Japan | Four digit C numbers that resemble UNS but do not match it. JIS C3604 is a free cutting brass close to CW614N and C385, not C360. The trailing letters give the product form, BD for drawn bar, BE for extruded. | Never assume a JIS number is the UNS number with a digit dropped. Check the cross reference.cross reference |
How to cite a standard on a brass drawing
Three lines in the title block cover most of it. The rest goes on the feature it applies to.
Material: C69300 per ASTM B371, or CW724R per EN 12164
Wetted surfaces: NSF/ANSI 372, 0.25% weighted average lead
Certificate: EN 10204 3.1 with composition per lot
General tolerance: ISO 2768-m
At the feature:
1/2-14 NPT per ASME B1.20.1, sealing thread, L1 gauge
Bore: no burrs at cross hole, see note 4
Dezincification: ISO 6509, max 200 um (hot water parts)Write the standard and leave the alloy open where a standard decides it. A shop can then offer the cheapest grade that passes, and the grade selector shows which grades those are.
Drawing cites a standard? Say so on the RFQ.
We place compliance parts only with shops that have shipped that class of part. Reply within 24 business hours with one itemised quote or a clear no.