Skip to content
Brass CNC Parts

Brass reference / Leaded brass

C345 leaded brass

A lower lead cousin of C360 that keeps enough ductility to be lightly formed after machining.

Also known as Leaded brass, Alloy 345, Medium leaded brass. Published typical values for the alloy, never a promise from a shop.

90Machinability, C360 = 100
1.5 to 2.5%Lead, over the 0.25% line
PoorDezincification resistance
340 to 470 MPa depending on temperTypical tensile strength

Composition

ElementNominal weight %
Copper62.0 to 65.0
Lead1.5 to 2.5
Iron0.15 max
Zincremainder

Properties

  • UNSC34500
  • EN equivalentCuZn37Pb2 / CW608N (nearest)
  • DIN2.0380 CuZn37Pb2 (nearest)
  • JISC3601 (nearest)
  • BSCZ119
  • Hardness55 to 80 HRB
  • Density8.47 g/cm3
  • Typical tolerance±0.02 mm typical
  • Common formsRound and hex bar, some sheet

What it is for, and what it is not

Specify it for

  • Screw machine parts that are staked, crimped or flared after turning
  • Clock and instrument parts
  • Parts that need a little cold work after machining

Do not specify it for

  • Pure turning jobs where C360 is stocked and cuts faster
  • Wetted potable water parts in the US
  • Hot water and seawater service

What a buyer should know

Halfway between C360 and a plain forming brass. The lead is still there, so it cuts nearly as well, but there is less of it and more copper, so the part can take a rivet, a flare or a light crimp after machining without cracking. Specify it when the drawing shows a formed feature after turning. Otherwise C360 is the easier grade to source.

Nominal lead is 1.5 to 2.5 percent, which is above the 0.25 percent weighted average limit that NSF/ANSI 372 sets for wetted potable water surfaces. See NSF/ANSI 61 and 372 and RoHS exemption 6(c).

Dezincification resistance is poor, so this alloy is the wrong choice sitting in hot water or seawater regardless of how well it machines. See dezincification and the grades that resist it.

Closest alternatives

AlloyLead %Mach.DZRWhy you might switch
C385 architectural bronzeC385002.5 to 3.590PoorA brass despite the name, supplied mainly as extruded shapes and the default where the part is seen.
C353 high-leaded brassC353001.5 to 2.590PoorThe sheet and plate version of free-cutting brass, used where a flat part is milled, engraved or blanked rather than turned.
C360 free-cutting brassC360002.5 to 3.7100PoorThe benchmark every other metal is rated against for machinability, and the default for turned brass parts.

All 16 alloys compared · Cross reference

Need a shop that runs C345?

Send the drawing. We reply within 24 business hours with one itemised quote for the finished parts.