Skip to content
Brass CNC Parts

Brass reference / Leaded brass

C353 high-leaded brass

The sheet and plate version of free-cutting brass, used where a flat part is milled, engraved or blanked rather than turned.

Also known as High leaded brass, Engraving brass, Clock brass, Alloy 353. Published typical values for the alloy, never a promise from a shop.

90Machinability, C360 = 100
1.5 to 2.5%Lead, over the 0.25% line
PoorDezincification resistance
340 to 470 MPa depending on temperTypical tensile strength

Composition

ElementNominal weight %
Copper60.0 to 63.0
Lead1.5 to 2.5
Iron0.10 max
Zincremainder

Properties

  • UNSC35300
  • EN equivalentCuZn37Pb2 / CW608N (nearest)
  • DIN2.0380 CuZn37Pb2 (nearest)
  • JISC3560 (nearest)
  • BSCZ119
  • Hardness55 to 80 HRB
  • Density8.47 g/cm3
  • Typical tolerance±0.02 mm typical on milled features
  • Common formsPlate, sheet and strip; also rod and bar (ASTM B453/B453M)

What it is for, and what it is not

Specify it for

  • Flat parts milled from plate: clock plates, gears, wheels, escutcheons
  • Engraved plates, dials and nameplates
  • Parts blanked from strip then machined
  • Anything that would be C360 if it came as bar

Do not specify it for

  • Turned parts from bar, where C360 is the stocked grade
  • Wetted potable water parts in the US
  • Hot water and seawater service
  • Parts formed after machining, the lead makes it less ductile

What a buyer should know

Same idea as C360, slightly less lead, supplied as plate, sheet and strip rather than bar. It exists because a milled or engraved flat part wants the free-cutting behaviour of C360 in a form C360 is rarely stocked in. If a drawing calls for C360 plate, this is usually what the supplier will offer. The alloy is also sold as rod, bar, wire and shapes, which ASTM B453/B453M covers; ask which product standard applies to the form you buy.

Nominal lead is 1.5 to 2.5 percent, which is above the 0.25 percent weighted average limit that NSF/ANSI 372 sets for wetted potable water surfaces. See NSF/ANSI 61 and 372 and RoHS exemption 6(c).

Dezincification resistance is poor, so this alloy is the wrong choice sitting in hot water or seawater regardless of how well it machines. See dezincification and the grades that resist it.

Closest alternatives

AlloyLead %Mach.DZRWhy you might switch
C385 architectural bronzeC385002.5 to 3.590PoorA brass despite the name, supplied mainly as extruded shapes and the default where the part is seen.
C345 leaded brassC345001.5 to 2.590PoorA lower lead cousin of C360 that keeps enough ductility to be lightly formed after machining.
C360 free-cutting brassC360002.5 to 3.7100PoorThe benchmark every other metal is rated against for machinability, and the default for turned brass parts.

All 16 alloys compared · Cross reference

Need a shop that runs C353?

Send the drawing. We reply within 24 business hours with one itemised quote for the finished parts.