Home / Glossary
Brass Machining Glossary
52 terms a buyer meets on a brass drawing, an RFQ or a quote, defined in plain language and linked to the page that goes deeper.
Alloy figures in these definitions are published typical values for the alloy. Machinability is rated against free-cutting brass C360 at 100. Nothing here is a promise from any shop.
- 4
- 4MSAlso 4MS Common Approach
A shared list of metallic material compositions accepted for drinking water contact, maintained by Germany, France, the Netherlands and the UK. It underlies the German UBA list and the coming EU positive lists. CW511L and CW724R are on it for wetted parts, CW614N and CW617N are not.
- A
- Across flatsAlso A/F, AF
The distance between two opposite faces of a hex. It sets the wrench size and, on a hex bar part, the stock size. Common brass hex bar is stocked in wrench sizes, so a part drawn at 22 mm across flats starts as 22 mm hex bar and needs no turning on the flats.
- Alpha brass
Brass with roughly 63 percent copper or more, a single phase structure that is ductile and cold works well. Cartridge brass C260 and red brass C230 are alpha brasses. They draw, spin and stamp well and machine slowly, with long chips.
- Alpha-beta brassAlso Duplex brass
Brass with roughly 55 to 63 percent copper, containing both alpha and beta phases. It hot works well, which makes it the forging structure, and it machines better than alpha brass. C377, CW617N and Muntz metal are alpha-beta brasses.
- Anti-tarnish treatmentAlso Benzotriazole dip, BTA
A thin chemical film, usually benzotriazole based, applied after cleaning to slow the oxidation that turns bright brass dull. It is invisible, it does not replace lacquer or plating and it lasts weeks to months depending on packaging and humidity.
- B
- Bar feeder
A magazine that pushes a length of bar stock into a lathe automatically, so parts are made one after another from a single bar without an operator loading blanks. Bar-fed lathes are the reason small brass parts are cheap in volume.
- Bismuth brass
A lead-free brass in which bismuth replaces lead as the chip breaker. Rated near 80 for machinability against C360 at 100, under 0.25 percent lead, and the closest drop-in for an existing C360 program. Bar is held in fewer sizes and costs more. C49300 and C49350 are the common grades.
- Brass
An alloy of copper and zinc, usually 55 to 90 percent copper. Small additions of lead, tin, silicon, arsenic or bismuth create the grades used in machined parts. Brass is not bronze, which is copper with tin, and not zinc die casting, which is mostly zinc.
- Bronze
Copper alloyed mainly with tin, aluminium or silicon rather than zinc. Bronzes are bearing, spring and marine alloys and machine differently from brass. Architectural bronze C385 is a misnomer, it is a brass. This site supplies brass parts only and does not take bronze parts.
brass vs bronze vs copper machining · c385 architectural bronze
- BSPP threadAlso G thread, ISO 228
British Standard Pipe Parallel, written G1/4 and defined in ISO 228-1. A 55 degree parallel thread that does not seal on the thread itself. The seal is a washer, O-ring or bonded seal on a face. Not interchangeable with NPT.
- BSPT threadAlso R thread, Rp thread, ISO 7
British Standard Pipe Taper, written R1/2 for the external taper and Rp1/2 for the internal parallel that accepts it, defined in ISO 7-1. Seals on the thread flanks with sealant. Same 55 degree form as BSPP but a different function, and never mated with 60 degree NPT.
- Built-up edge
Workpiece material welding itself to the cutting edge of a tool during a cut. It ruins surface finish and dimension. Free-cutting brass almost never forms one, which is part of why it finishes so well off the tool. Lead-free brass and copper are more prone to it.
- C
- Cartridge brassAlso 70/30 brass, C260, CuZn30
The 70 percent copper, 30 percent zinc alpha brass made for deep drawing and cold forming, named for ammunition cases. Rated 30 for machinability against C360 at 100. When it appears on a machining drawing it is usually inherited from a stamped design.
- Chip breaker
Anything that makes a chip snap into short pieces rather than form a long ribbon. In free-cutting brass the lead particles do it inside the metal. In lead-free brass the tool geometry and the feed have to do it instead, which is the practical difference between the two on a lathe.
- Copper Development AssociationAlso CDA
The industry body whose published alloy data most brass datasheets, this site included, draw on. It also administers the wrought copper alloy numbers that became the UNS C numbers. The CDA number of an alloy is the middle three digits of its UNS number.
- Cross-hole burr
The raised edge left where a drilled hole breaks through into a bore or another hole. It sits inside the part where tumbling cannot reach and a visual check cannot see it, and it is the most common reason a brass fitting fails a leak test after assembly.
- CW numberAlso EN 1412
The European material number for a wrought copper alloy, such as CW614N. CW means copper wrought, the three digits identify the alloy and the last letter gives the group, N for copper-zinc-lead. It pairs with a symbol such as CuZn39Pb3 under EN 1173.
- D
- Dezincification
Corrosion in which zinc leaches out of brass in water and leaves a porous copper sponge behind. The part keeps its shape and loses its strength. Hot water, chlorides and stagnant water accelerate it. Ordinary brasses above about 15 percent zinc are susceptible unless inhibited.
- DZR brassAlso Dezincification resistant brass, CW602N, CZ132
Brass with an arsenic addition and a controlled heat treatment that resist dezincification, tested to ISO 6509. CW602N is the common European grade. DZR answers corrosion, not the lead question: CW602N carries around 2 percent lead and does not meet US potable water limits.
- E
- Eco BrassAlso CW724R, C69300
The trade name under which silicon brass C69300 and CW724R were introduced. Lead-free, rated near 80 for machinability, roughly twice the strength of C360 and highly dezincification resistant. The usual lead-free answer for potable water parts.
- EN 10204 3.1 certificateAlso Mill certificate, Mill cert, Inspection certificate
An inspection certificate issued by the mill with actual test results for the specific lot of bar, composition included. It is the document that gives you the real lead figure for your material rather than the nominal range. A 2.1 or 2.2 is a statement, not a result.
- Extruded profileAlso Extrusion, Section
A bar with a custom cross section pushed through a die, so that a hinge, handle or trim part starts with its shape already there and needs only cutting to length and machining of features. C385 architectural bronze is the usual profile alloy.
- F
- First article inspectionAlso FAI
A full dimensional and material check of the first part or parts off a new setup, reported against the drawing, before the batch runs. On a brass part it catches a setup error or a wrong bar pull before a thousand pieces carry it.
- Forging brassAlso Hot stamping brass, C377, CW617N
An alpha-beta brass with moderate lead, around 2 percent, chosen because it flows well at forging temperature without hot shortness and still machines well afterwards. C377 in the US and CW617N in Europe. Used where a bulky part in real volume is forged to near net shape and then machined only on the features that matter.
c377 forging brass · cw617n cuzn40pb2 · brass hot forging vs machining
- Free-cutting brassAlso Free machining brass, C360, CW614N, CW603N
Brass with around 3 percent lead added purely to make it machine well. The lead breaks the chip and lubricates the cut. C360 is the benchmark that every other metal is rated against, at 100. It is not legal for wetted US potable water parts and it dezincifies in hot water.
- G
- Go and no-go gaugeAlso Thread gauge, Plug gauge, Ring gauge
A pair of hardened gauges cut to the two limits of a thread or bore. The go gauge must enter or thread on fully, the no-go must not. It is the only practical way to prove a thread is in class, because a thread can look perfect and be out of tolerance.
- H
- Half hardAlso H02 temper, Temper
The usual temper of free-cutting brass bar, cold drawn enough to be straight, stable and a little stronger than annealed, without being so hard it cracks on a knurl or a flare. ASTM B16 bar is normally supplied half hard.
- Hot shortness
Cracking during hot forging because a low melting constituent is liquid at forging temperature. In high lead brass the lead is molten at the grain boundaries, so C360 cracks when forged. Forging brass keeps the lead lower and the structure alpha-beta for this reason.
- I
- IACS conductivity
Electrical conductivity expressed as a percentage of the International Annealed Copper Standard. Pure copper is 100 percent. Free-cutting brass C360 sits near 26 percent as a published typical value, which is enough for terminals and connector bodies and why they are usually plated rather than made from copper.
- K
- Knurl
A pattern of ridges rolled or cut into a cylindrical surface for grip or for retention in a moulded plastic. Straight, diamond and helical patterns are specified by pitch under DIN 82 or by diametral pitch under ANSI B94.6. Brass knurls cleanly because it does not work harden much.
- L
- Leaching
Metal dissolving from a wetted surface into the water it touches. Lead leaching is the health concern behind the drinking water rules. Composition limits such as NSF/ANSI 372 control what is in the alloy. Leaching tests such as NSF/ANSI 61 measure what actually comes out of the finished product.
- Lead-free brass
In the US legal sense, brass whose weighted average lead content across the wetted surfaces of a product is not more than 0.25 percent, per NSF/ANSI 372 and the Safe Drinking Water Act. Silicon brass and bismuth brass qualify. It does not mean zero lead, and it is not legal advice.
- M
- Machinability rating
A relative index of how easily a material cuts, on this site and in most copper alloy data rated against free-cutting brass C360 at 100. Steel charts use free-cutting steel 12L14 as their 100, so figures from the two scales cannot be compared directly. Ratings are published typical values, not a cycle time.
- Muntz metalAlso 60/40 brass, C280, CuZn40
The 60 percent copper, 40 percent zinc alpha-beta brass supplied as plate and sheet for tube sheets, architectural work and heavy sections. Rated near 40 for machinability. Add 1 percent tin and it becomes naval brass.
- N
- NPT threadAlso National Pipe Taper, ASME B1.20.1
The US tapered pipe thread, 60 degree form, defined in ASME B1.20.1. It seals on the thread flanks with a sealant and is gauged with L1 ring and plug gauges. Not interchangeable with 55 degree BSP threads even where the diameters look the same.
- NSF/ANSI 372
The North American standard that defines how the weighted average lead content of the wetted surfaces of a plumbing product is calculated and verified against the 0.25 percent limit. It is an arithmetic and verification standard, not a leaching test.
- NSF/ANSI 61
The North American health effects standard for drinking water system components. A product is tested for what it leaches into water. Certification is granted to a named product from a named manufacturer, so a subcontract machine shop cannot certify a custom part to it on its own.
- P
- Positive list
A list of materials that are permitted for drinking water contact. Anything not on the list is not allowed. The 4MS list, the German UBA list and the EU lists under Directive 2020/2184 are all positive lists. The US approach is different: a composition limit plus a leaching test.
- R
- Red brassAlso C230, 85/15 brass, CuZn15
A high copper wrought brass, 85 percent copper, supplied mostly as tube and pipe. Its copper level puts it above the zinc content where dezincification occurs. Rated 30 for machinability. Not the same as the red brass casting alloys such as C83600, which are leaded.
- RoHS exemption 6(c)
The exemption in Annex III of the EU RoHS Directive that allows copper alloys containing up to 4 percent lead in electrical and electronic equipment. Its expiry was set at 30 June 2027 and a renewal request submitted in December 2025 suspends that date pending a decision. Status as of September 2026, not legal advice.
- S
- Season crackingAlso Stress corrosion cracking, SCC
Cracking of brass under the combination of residual tensile stress and a corrosive agent, classically ammonia. Named after cartridge cases that split in monsoon season. Prevented by a stress relief anneal after machining, typically 330 to 350 C, and tested for with ISO 6957 or ASTM B858.
- Silicon brassAlso C69300, CW724R, CuZn21Si3P
A lead-free brass in which silicon provides the machinability, rated near 80 against C360 at 100. Roughly twice the tensile strength of C360, highly dezincification resistant and the usual lead-free grade for potable water. It work hardens, so it wants sharp positive tooling.
- Stress relief
A low temperature anneal, typically 330 to 350 C for brass, that removes the residual stress left by cold drawing and machining without softening the part. Specified on cold worked or heavily machined brass parts that will see ammonia, moisture or seawater, to prevent season cracking.
- Swiss latheAlso Sliding headstock lathe, Swiss type lathe
A lathe in which the bar is fed through a guide bushing and the tools cut right at the bushing, so long slender parts are supported at the cut. The cheapest way to make small round brass parts, roughly under 32 mm diameter, in the hundreds or thousands.
- T
- Tarnish
The dull brown or greenish film that forms on bright brass as copper at the surface oxidises and reacts with sulphur in the air, fingerprints and packaging. Cosmetic on most parts, a real problem on electrical contacts and under plating. Slowed by cleaning, anti-tarnish dips and VCI packaging.
- Tin brass
Brass with a small tin addition, around 1 percent, for corrosion resistance in water. Naval brass C464 and admiralty brass C443 are the common grades. Tin suppresses dezincification and costs machinability, both rated near 30.
- TumblingAlso Vibratory finishing, Barrel finishing, Mass finishing
Deburring or polishing many parts at once by agitating them with an abrasive or polishing media in a barrel or vibratory bowl. Brass responds well. It reaches outside edges and open surfaces, and it does not reach a burr inside a bore or at a cross hole.
brass tumbling vibratory finishing · brass deburring cross holes
- U
- UNS number
The Unified Numbering System designation for a metal, such as C36000. For copper alloys, C1xxxx to C7xxxx are wrought and C8xxxx and C9xxxx are cast. The common short name, C360, is the middle of the number. JIS numbers look similar and are not the same system.
- V
- VCI packagingAlso Vapour corrosion inhibitor
Paper or film impregnated with a compound that evaporates slowly and forms a protective layer on metal inside a closed package. The standard way to ship bright brass parts without tarnish. Rubber bands, untreated cardboard and PVC should be kept away from brass in transit.
- W
- Wetted surface
The surface of a component that is in contact with the water in normal use. Only wetted surfaces count in the NSF/ANSI 372 weighted average. External surfaces, dry faces and threads outside the water path are excluded, bores, seats and internal passages are included.
- Y
- Yellow brass
A loose trade name for brasses around 60 to 70 percent copper with the familiar yellow colour, covering C260, C360 and most machining grades. It is a colour, not a specification. A drawing that says yellow brass has not chosen an alloy.
Missing a term?
Tell us which word on your drawing is not here and we add it. Corrections are logged on the corrections page.