Skip to content
Brass CNC Parts

Guides / Process

How to Specify a Knurl on a Brass Thumb Screw, Knob or Insert

Published September 27, 2026. Reviewed for the facts in the corrections log.

Brass knurls well because it is ductile and does not work harden much, so a form knurl raises a clean pattern in one pass. Specify the pattern and pitch to DIN 82 or ANSI B94.6, the finished diameter with a wide tolerance and whether the knurl is plated. Leave the blank diameter to the shop, because form knurling grows it.

Brass is the metal that knurling was made for. It is ductile, it hardly work hardens and it takes a form knurl in one pass without tearing. That is why thumb screws, instrument knobs, threaded inserts and hand grips are so often brass, and why a knurl on a brass drawing is rarely a problem for a shop.

The problems come from the callout. A knurl specified by a picture, by a pitch with no standard or with a tight finished diameter sends the shop back with questions or a part that fails inspection for no functional reason. This post covers what to write and why.

The three patterns

Straight knurl. Parallel ridges along the axis. It gives grip against rotation and none against pull. Used on inserts that must resist torque, on press fit bushes and on grips where a diamond would look wrong.

Diamond knurl. Two helical patterns crossed, one left hand and one right hand, leaving raised or recessed pyramids. Grip in every direction. The usual choice for thumb screws, knobs and moulded-in inserts. Raised diamond, where the pyramids stand proud, is the common one. Recessed diamond, where the pattern is grooves and the flats stay at the original diameter, is used where a smooth top surface is wanted.

Helical knurl. A single hand helix at about 30 degrees. Half a diamond. It looks decorative and gives some grip in both directions. Less common on functional parts.

DIN 82, the German standard most metric drawings use, names them RAA (straight), RBL and RBR (helical left and right), RGE (diamond raised) and RGV (diamond recessed), followed by the pitch in millimetres. ASME B94.6 is the US equivalent and specifies the pattern by diametral pitch, with 64, 96, 128 and 160 DP as the common sizes. The Wikipedia page on knurling has diagrams of each.

Cut knurling and form knurling

A form knurl presses the pattern into the surface. Hardened wheels are forced against the turning blank, the metal flows into the tooth spaces and the surface rises. It is fast, the tool is cheap, and on brass it produces a crisp pattern in one or two passes. It also needs force. A long thin part bends away from the wheels, a thin walled tube swells and a part held only in a collet can push back into the spindle.

A cut knurl shears the pattern instead. The wheels are set at an angle so their teeth cut a chip, much like a small milling cutter. Radial force is low, so thin walls, long shafts and parts near a tolerance feature can be knurled without distortion. The pattern is full depth and sharp, and the diameter hardly grows. The tool costs more and the cycle is a little longer.

On a small brass thumb screw the form knurl is right. On a knurled band 5 mm from a ground bore, or on a thin brass tube, the cut knurl is right. A shop that has both will choose. If you only want one, say so.

Blank diameter and growth

Form knurling raises the surface, so the finished diameter over the knurl is larger than the blank. The growth depends on the pitch, the depth and the alloy. It is why the finished diameter over a knurl should carry a wide tolerance and why the blank diameter should be left to the shop.

There is a second rule. On a form knurl the wheel teeth must land in the same grooves on every revolution of the part, so the blank circumference has to be close to a whole number of pitches. A 10 mm blank at 1.0 mm pitch has a circumference of 31.4 mm, which is 31.4 pitches, and the wheel double tracks. The shop turns the blank to 9.87 mm (31 pitches) or 10.19 mm (32 pitches) and the pattern comes out clean. On a cut knurl this rule largely falls away, which is another reason shops reach for it on odd diameters.

DIN 82 pitch Nearest ASME B94.6 Typical growth, form knurl on brass Typical use
0.5 mm 160 DP 0.15 to 0.25 mm Thumb screws under 6 mm, small inserts
0.6 mm 128 DP 0.2 to 0.3 mm Instrument knobs, inserts
0.8 mm 96 DP 0.25 to 0.4 mm Thumb screws and knobs 8 to 20 mm
1.0 mm 80 DP 0.3 to 0.5 mm Knobs and grips 15 to 30 mm
1.2 mm 64 DP 0.4 to 0.6 mm Grips and hand wheels
1.6 mm 48 DP 0.5 to 0.8 mm Large hand wheels

Published typical values for diameter growth on free-cutting brass. The exact figure depends on the wheel, the depth and the alloy, and the knurl tool maker’s chart takes precedence. Pitch should scale with diameter: a coarse pitch on a small diameter leaves only a few pyramids around the part and looks wrong.

Need a quote for this part? Get a quote for your brass parts

Why brass knurls so well

Free-cutting brass C360 is soft, ductile and has a low rate of work hardening, so the metal flows into the wheel without cracking at the pyramid tips and without hardening enough to resist the second pass. The lead particles help the chip on a cut knurl and do no harm on a form knurl. Finish straight off the wheel is bright.

Lead-free silicon brass C69300 is roughly twice as strong, so it needs more force on a form knurl and the wheels wear faster, but it forms a sharper and harder wearing pattern. Cartridge brass C260 is softer still and knurls easily but smears on a cut knurl. Naval brass C464 is tougher and is usually cut knurled.

Plating over a knurl

A knurl is usually the last machining operation before the part goes for finishing. Plating over it works, with two notes.

Plating deposits faster on peaks than in valleys, because the current density is higher on a sharp edge. A nickel layer of 5 to 15 microns on the flats is thicker on the pyramid tips and thinner in the grooves, and the pattern softens slightly. Heavier plating, above about 25 microns, starts to fill a fine pitch. Specify plating thickness on a flat surface, not over the knurl, and use a coarser pitch if a thick coating is needed. Plating options and how to write them are in brass surface finishes and plating.

The knurl must also be free of the fine burr that a form knurl leaves at each end. A light tumble or a chamfer cut after knurling removes it. If it stays, the plating bridges it and it flakes later.

Knurled inserts for plastic moulding

Brass inserts are moulded in, pressed in, heat staked or ultrasonically driven into plastic housings, and the knurl is what holds them. A straight knurl resists rotation. A diamond knurl resists rotation and some pull-out. For real pull-out strength the insert needs a groove or an undercut that the plastic fills, and most catalogue inserts combine a diamond knurl with one or two grooves.

Heat staked inserts use two opposed helical bands so the plastic locks in both directions as it flows. Brass is the material because it turns quickly, conducts heat into the plastic during staking and does not corrode in a housing. One caution for electronics housings: leaded brass inserts fall under RoHS exemption 6(c), and that exemption has an expiry date. See RoHS exemption 6(c) and leaded brass. This is not legal advice.

What to put on the drawing

Knurl, diamond raised, DIN 82 RGE 0.8, over length 12.
Finished diameter over knurl 10.4 +/- 0.15.
Blank diameter at shop discretion.
Ends chamfered 0.5 x 45 after knurling. Knurl free of burrs.
Knurl before plating. Nickel 8 to 12 microns measured on flat surfaces.

Or on an inch drawing:

Knurl, diamond, 96 DP, per ASME B94.6, raised pattern.
Finished diameter over knurl .410 +/- .006.

Name the standard and the pitch. Give the finished diameter a tolerance the process can hold. Say whether the ends are chamfered, because a bare knurl end is sharp. Say whether plating follows. Do not draw the pattern to scale, and do not give the blank diameter unless a feature next to the knurl depends on it.

Have a knurled brass part to quote? Send the drawing with the pitch and standard marked. We quote the finished parts within 24 business hours and place the work with one of the partner shops that turn brass.

Frequently asked questions

What is the difference between DIN 82 and ANSI B94.6 knurls?

DIN 82 specifies the knurl by pattern code and pitch in millimetres, so RGE 1.0 is a raised diamond at 1.0 mm pitch. ASME B94.6 specifies it by diametral pitch, so 96 DP is a pitch of about 0.83 mm. They are close but not identical, and a shop with metric wheels will offer the nearest DIN pitch to an inch callout. Naming one standard avoids the argument.

Why does the shop want to change my blank diameter?

Because a form knurl only tracks cleanly when the circumference of the blank is close to a whole number of pitches. A 10 mm blank at 1.0 mm pitch gives 31.4 pitches, and the wheel double tracks. Turning the blank to 9.87 mm or 10.19 mm fixes it. Leave the blank diameter to the shop and tolerance the finished diameter over the knurl instead.

Can a knurled brass part be plated?

Yes. Nickel and chrome both plate over a knurl. Plating builds thicker on the pyramid tips than in the grooves, so the pattern softens a little and a heavy coating can fill a fine pitch. Specify the plating thickness on a flat surface, use a coarser pitch if the coating is thick and make sure the knurl is deburred before it goes to the plater.

Which knurl holds a brass insert in plastic?

A straight knurl resists rotation. A diamond knurl resists rotation and some pull-out. For pull-out strength the insert needs a groove or undercut the plastic can fill, which is why most catalogue inserts pair a diamond knurl with one or two grooves. Heat staked inserts use two opposed helical bands. Brass is the usual material because it turns fast and conducts heat into the plastic.

Alloys in this guide

AlloyLead %Mach.DZR
C360 free-cutting brassC36000 · CuZn36Pb3 / CW603N2.5 to 3.7100Poor

Published typical values for the alloy. Machinability against C360 at 100. Not a promise from a shop.

Sources

  1. ASME B94.6, Knurling asme.org
  2. Wikipedia, Knurling en.wikipedia.org

Need a quote for this part?

Send the drawing. We read it, send one itemised quote for the finished parts within 24 business hours and place the work with a partner shop that turns brass. Brass only.

Get a quote for your brass parts

Keep reading

Get a quote