Guides / Process
Machined Brass Refrigeration and HVAC Fittings: Flare Nuts, Valves, Brazing and Tests
Published November 21, 2026. Reviewed for the facts in the corrections log.

Brass refrigeration fittings are flare nuts, flare unions, service valves, access valve bodies and ball valves on copper refrigerant lines. Bodies are usually forged CW617N or C377, small parts turned from C360. The flare cone, the thread and the seat decide the seal. Parts must be clean, dry and capped, and ammonia systems cannot use brass.
Almost every split air conditioner, heat pump, cold room and commercial fridge holds brass. The flare nuts on the line set, the service valves on the outdoor unit, the access port where a technician connects gauges and the ball valve that isolates a section are all machined brass parts on copper tube.
Refrigeration asks more of these parts than plumbing does. The circuit runs at high pressure, it must stay sealed for years and it must stay dry inside. This post covers the parts, the grades, the flare, brazing near brass, testing and the cleanliness a drawing should require.
The parts
A refrigerant line set and its valves use a short list of brass parts.
| Part | Typical grade and route | Critical feature | Typical check |
|---|---|---|---|
| Flare nut | C377 or CW617N forged, or C360 turned from hex bar | 45 degree cone, thread, bore | Thread gauge, cone gauge |
| Flare union, elbow, tee | CW617N forged, then machined | Male flare cone, thread | Thread gauge, visual on cone |
| Service valve body | CW617N or C377 hot stamped | Seat, stem bore, port threads | Pressure and leak test |
| Valve stem and cap | C360 turned | Thread, seat face, cap seal face | Gauge, visual |
| Access valve body | C360 turned | Core thread and seat, flare cone | Gauge, leak test |
| Refrigerant ball valve body | CW617N forged | Ball seat pockets, end connections | Leak test across seat |
| Ball | Brass, chrome plated | Roundness, finish | Gauge, leak test |
Typical practice. The equipment maker’s drawing and the product standard take precedence.
Valve bodies and most flare unions are hot stamped from CW617N or C377 forging brass and then machined on the seats, threads and cones. Small turned parts such as stems, caps and access valve bodies use C360 free-cutting brass. Flare nuts are made both ways. A forged nut uses less bar and has grain flow around the hex. A nut turned from hex bar needs no die, which suits short runs and odd sizes. The cost trade is covered in brass hot forging vs machining, and the body side in brass valve bodies and components.
The SAE 45 degree flare
A refrigeration flare fitting seals metal to metal. The end of a soft copper tube is flared to a 45 degree cone. The male fitting carries a matching 45 degree cone, and the nut clamps the tube flare between the two. No sealant, no O-ring. The finish of the cones decides the joint.
SAE J513 covers refrigeration tube fittings, including the flare angle, the thread and the nut. Most sizes use unified fine threads. A 1/4 inch tube flare, for example, uses a 7/16-20 UNF thread. Check the table in the edition of the standard you work to, or the thread data in the brass thread chart.
Two mix-ups cause most flare leaks in the field.
37 against 45 degrees. Hydraulic JIC fittings use a 37 degree flare. A 45 degree refrigeration flare seated on a 37 degree cone touches on a line, not a face, and it leaks. The drawing should name the angle and the standard, not “flare” alone.
Short and long nuts. Flare nuts come in short and long patterns. The long nut supports the tube further back from the flare and resists vibration. The equipment maker picks the pattern, so the drawing should show the nut length, not leave it to the shop.
What a shop controls on the flare:
- Cone angle and cone finish. A smooth cone, free of tool marks across the sealing band, typically Ra 0.8 micrometre or finer on the sealing face.
- A sharp but burr-free edge where the cone meets the bore. A burr here cuts the tube flare.
- Thread start and class. A damaged first thread cross-threads and galls on install. See thread gauging.
- Concentricity of the cone to the thread, so the flare seats evenly all round.
Service valves and access valves
Service valves. The outdoor unit of a split system carries two service valves, one on the liquid line and one on the suction line. Each has a hot stamped body, a stem that seats on a machined face, a flare or brazed connection to the line set and an access port. The seat face and the stem bore are the critical machined features. The cap often seals too, on a metal face or a small O-ring, so its sealing face needs the same care as the seat.
Access valves. The access port is a small turned body with a 45 degree flare cone outside and a spring valve core inside, the same type of core found in a Schrader valve. The core comes from a core maker. The shop machines the body, so the core thread and the seat that the core seals against must follow the core maker’s drawing. Ask for that drawing before quoting. Some equipment for newer refrigerants uses a different access port size so that service hoses for different gases do not get mixed up. The equipment maker’s drawing names it.
Ball valves. Refrigerant ball valves are full port or reduced port, with a forged brass body, a chrome plated brass ball and PTFE seats. Many carry an access port on the body and copper extension tubes on the ends for brazing. Seat pockets, stem bore and the ball finish decide the leak rate across the seat.
Brazing near brass
Most refrigerant joints are brazed, and brass parts sit right next to the flame.
Zinc boil-off. Forging brass is close to 40 percent zinc, and zinc boils at a much lower temperature than copper melts. Overheat a brass body and zinc leaves the surface as white zinc oxide fume. The surface goes porous and spongy, and a sealing area nearby can be ruined. The cure is control: the lowest heat that flows the filler, for the shortest time.
Copper extensions. This is why many valves come with copper stub tubes brazed on at the valve maker. The installer brazes copper to copper, away from the brass body. Seats and PTFE parts inside the valve are also wrapped with a wet cloth or a heat sink paste during field brazing.
Leaded brass and braze joints. Lead in free-cutting brass can cause cracking and poor wetting when a joint is brazed. Where the drawing calls for a braze joint on the brass itself, ask the valve maker which grade and filler they have qualified. The filler matters too. Silver-bearing brazing alloys with flux are common on brass. Copper-phosphorus fillers are self-fluxing on copper but need flux on brass.
Nitrogen purge. Brazing without a purge leaves oxide scale inside the tube, which breaks loose and blocks filters and expansion devices. Installers flow dry nitrogen through the line while brazing. That is a field step, but it explains why the inside of a valve must arrive clean.
Need a quote for this part? Get a quote for your brass parts
Pressure and leak testing
Refrigeration parts are tested twice: for strength and for tightness.
| Test | Typical method | What it finds |
|---|---|---|
| Strength | Pressure test, often with dry nitrogen, or hydrostatic on bodies | Weak walls, porosity in forgings |
| Tightness, production | Helium mass spectrometer, vacuum or sniffer | Very small leak paths |
| Tightness, simpler | Pressure decay with dry air or nitrogen | Larger leaks |
| Tightness, trace gas | Nitrogen with hydrogen trace gas, sniffer | Small leaks at joints |
| Seat | Pressure one side, measure leak on the other | Leak across a valve seat |
Typical practice for refrigeration components. The product standard and the equipment maker’s specification set the pressure, hold time and leak limit and take precedence.
Refrigerant pressures vary a lot between gases, and newer gases often run higher than older ones. Never take a fitting rating from an older design without checking it against the gas. Standards in this area include UL 207 for refrigerant-containing components and ISO 14903 for the tightness of components and joints. The equipment maker names the one that applies and its edition. A machine shop supplies parts to the drawing and the test written on it. It does not certify the finished valve. See leak and pressure testing brass valve bodies for the methods.
Cleanliness and dryness
A refrigeration circuit is a closed, dry system with its own oil. Contamination from a machined part ends up inside it.
Moisture. Water reacts with refrigerant and oil to form acids, and with polyolester oils it also breaks down the oil. It can freeze at the expansion device. Parts are washed, dried and capped or bagged so they stay dry in storage.
Oil residue. Cutting oil left in a bore mixes with the system oil. Chlorinated or sulfurized cutting fluids are a particular risk. Ask the shop what coolant and cleaning it uses, and state a cleanliness requirement on the drawing.
Chips and burrs. A chip trapped in a cross hole or a valve seat comes loose later and blocks a filter or holds a valve open. See deburring cross holes for the methods.
Caps and packing. Flare ends and ports are capped. Ball valves ship in the open position so the seats are not loaded in transit. Brass also tarnishes in damp transit, so a sealed bag with a desiccant is common.
Ammonia: not brass
Large industrial refrigeration often uses ammonia (R717). Ammonia attacks copper and its alloys and drives stress corrosion cracking in brass. Ammonia plants are built in steel for that reason. This site quotes brass only and does not quote parts for ammonia systems. The same cracking risk applies to ammonia-based cleaners and leak detectors used on brass fittings, so use non-ammoniated products.
What to write on the drawing
Material: CW617N (CuZn40Pb2), hot stamped, or C360 turned for nuts and caps.
Flare: 45 degree per SAE J513, 1/4 inch tube, thread 7/16-20 UNF-2B.
Cone sealing face Ra 0.8 max, free of burrs and tool marks across the band.
Clean, dry, free of oil and chips. Ends capped. Packed in sealed bags.
Strength test with dry nitrogen and leak test per equipment maker's spec.
Not for ammonia service.
Checklist
- Part role named: flare nut, union, service valve, access valve or ball valve.
- Flare angle and standard named, nut pattern shown.
- Refrigerant named, with the pressure rating it must meet.
- Forged or turned route agreed, and the grade stated.
- Braze joints on brass identified, with grade and filler agreed.
- Strength test, leak test method and leak limit stated.
- Cleanliness, dryness, caps and packing written on the drawing.
Need machined brass refrigeration fittings or valve parts? Send the drawing with the refrigerant and test marked. We quote the finished parts within 24 business hours and place the work with one of the partner shops that turn brass.
Frequently asked questions
Can brass fittings be used with ammonia refrigerant?
No. Ammonia attacks copper and its alloys, and it causes stress corrosion cracking in brass. Ammonia refrigeration plants use steel pipe, steel valves and steel fittings for that reason. This site quotes brass only, so it does not quote parts for ammonia systems.
Is a 45 degree refrigeration flare the same as a 37 degree JIC flare?
No. Refrigeration flare fittings use a 45 degree flare, covered by SAE J513. Hydraulic JIC fittings use a 37 degree flare. The threads can look alike in some sizes, but the cone angles do not seal against each other. Name the flare standard and angle on the drawing.
Why do refrigeration fittings have to be dry and capped?
Moisture in a refrigerant circuit reacts with the oil and refrigerant to form acids, and it can freeze at the expansion device. Cutting oil and chips contaminate the system oil and block small passages. Refrigeration parts are washed, dried and capped or bagged so they reach the assembler clean and dry.
Alloys in this guide
| Alloy | Lead % | Mach. | DZR |
|---|---|---|---|
| C377 forging brassC37700 · CuZn39Pb2 / CW612N | 1.5 to 2.5 | 80 | Poor |
| CW617N CuZn40Pb2C37700 (nearest) · CuZn40Pb2 / CW617N | 1.6 to 2.5 | 80 | Poor |
| C360 free-cutting brassC36000 · CuZn36Pb3 / CW603N | 2.5 to 3.7 | 100 | Poor |
Published typical values for the alloy. Machinability against C360 at 100. Not a promise from a shop.
Sources
- Wikipedia, Flare fitting en.wikipedia.org
- Wikipedia, Schrader valve en.wikipedia.org
Need a quote for this part?
Send the drawing. We read it, send one itemised quote for the finished parts within 24 business hours and place the work with a partner shop that turns brass. Brass only.
Get a quote for your brass parts