Guides / Process
How Brass Fitting Threads Are Gauged: Plugs, Rings and the Notch
Published November 21, 2026. Reviewed for the facts in the corrections log.

A brass fitting thread passes when the GO gauge turns on fully and the NO GO gauge starts no more than a few turns. Straight threads use plug and ring gauges. Tapered NPT threads use a notched L1 gauge and judge the thread by how far it enters. Plating changes the reading, so gauge after plating.
A brass fitting exists to make a seal. Almost everything about it can be forgiven if the thread is wrong by a small amount except the thread. A thread that is slightly too loose leaks. One that is slightly too tight cracks the female part or cannot be started. So the thread is the one feature that every shop checks on every lot, and it is checked with gauges that give a pass or fail rather than a number.
This post explains the common gauges, what each one proves and what to write on a drawing so the shop and the buyer agree on the test.
What a go/no-go gauge proves
A limit gauge does not measure. It answers one question, which is whether the thread lies between two limits. Each gauge pair has a GO member and a NO GO member.
The GO gauge is built to the maximum material limit. On an internal thread it is a plug that must screw in the full length of the thread. On an external thread it is a ring that must screw over the full length. If it does, the thread form, the lead and the diameters are all inside the limit at once, because the gauge has a full thread profile that touches every flank.
The NO GO gauge checks the other limit, the minimum material condition of the pitch diameter. It is cut with a short or truncated profile so that it touches only the pitch diameter. A good thread lets it start for one or two turns and then stops it. If it runs on freely, the thread is too loose.
Passing both gauges is the test. Passing GO and failing NO GO means the thread is worn out or cut oversize. Failing GO means material is left where it should not be, or the lead is wrong.
Straight threads
On parallel threads such as unified UNC and UNF, metric ISO threads and BSPP (G), the gauge pair is the full story. A shop with a lot of fittings holds working gauges for each thread and a master set kept clean for calibration.
The gauge standards worth naming on a drawing are ASME B1.2 for inch unified threads, ISO 1502 for metric threads and ISO 228-2 for BSPP threads. ISO 228-2 describes the verification of parallel pipe threads by limit gauges. Naming the standard stops arguments over which gauge limits apply.
Tolerance class matters. A 2A and 2B fit gives a normal allowance between bolt and nut thread, and the gauge limits follow. A drawing that gives a thread size but no class leaves the shop to guess, and the guess is usually the common medium fit.
Tapered threads and the notched gauge
Pipe fittings in the US use NPT, a 1 in 16 taper on the diameter. A taper does not have a fixed pitch diameter, so a GO and NO GO pair cannot describe it. The fit is described by how far one part enters the other.
ASME B1.20.1 sets the working gauge for this (see also national pipe thread), called the L1 plug or ring. It is screwed in by hand until it stops. On the gauge there is a notch, or a step, marking the basic position. A good thread ends flush with that reference, within a tolerance of plus or minus one turn. If the part goes in more than one turn past the notch, the thread is too small. If it stops more than one turn short of the notch, the thread is too large.
Because a taper wedges, the gauge reading depends on the wear of the gauge and on hand pressure. A shop should screw the gauge by hand and stop at first firm contact, and should not force it. Plug and ring gauges for tapers are also checked against masters on a regular schedule, as they wear faster than straight gauges.
The difference between NPT and BSP is covered at length in NPT vs BSP brass fittings, and the brass thread chart lists the sizes and tap drills.
What typically goes wrong on brass
Brass cuts cleanly, so the usual thread faults come from a small number of causes.
| Fault | What the gauge shows | Typical cause |
|---|---|---|
| Thread too loose | NO GO runs on past two turns | Worn die or tap, tool set oversize |
| Thread too tight | GO will not start or stops | Tool undersize, plating added after cutting |
| Torn or rough flank | GO binds partway | Dull tool, chips packed in the thread |
| Wrong lead | GO stops after a few turns | Wrong change gear or feed, wrong tap |
| Tapered thread off the notch | L1 face sits outside one turn | Die set wrong, wear on the die |
| Burr at the thread start | GO will not start by hand | Missing chamfer or deburr |
Typical causes, not a diagnosis. A shop’s own process records settle each case.
Brass does not gall the way stainless does, so a gauge on brass wears slowly. It does collect fine chips and oil in the root, and a gauge reading is only as good as the clean part it checks. A thread that is oily or has packed swarf can fail a gauge that a clean part passes.
Need a quote for this part? Get a quote for your brass parts
Gauging and plating
Plating changes the answer, and many drawings forget it. A layer of nickel or chrome deposits on the thread flanks, not just on the crest. For a 60 degree thread the pitch diameter grows by about four times the thickness of the layer, because the flank is inclined. A 10 micron nickel layer adds about 40 microns to the pitch diameter of an external thread. On a fine thread, that can take a part from a good fit to the point where the GO ring will not go on.
There are two ways to handle this. The first is to write the thread tolerance as applying after plating and let the shop cut the thread to a size that leaves room. The second is to mask the thread so that it stays bare. Both need to be on the drawing. More on plating and its side effects is in brass surface finishes and plating.
Thread gauging after plating is the only way to catch it. A shop that gauges only after cutting will ship parts that fail at the customer.
Sampling and first articles
A drawing should also say how often threads are gauged. On a first article, every thread feature is checked with the full gauge set. On a production run, a shop may check on a sampling plan, such as a set number every hour of running, or every part for safety critical threads such as gas valves. If you need every thread checked at a hundred percent, say so, and expect it to be a line on the quote. See brass part quality checks for how inspection plans are written.
What to write on the drawing
Thread 1/2-14 NPT per ASME B1.20.1. Gauge with L1 plug, within 1 turn of notch.
Thread M12 x 1.0 6g per ISO 965. Gauge GO and NO GO.
Threads to gauge after plating. Mask thread during plating if plating is required elsewhere.
100 percent thread gauging on lot.
Pick the lines that apply. Naming the standard, the class and the gauge type removes most of the ambiguity.
Checklist
- Standard and class named for every thread.
- Tapered threads call for an L1 gauge and the position tolerance.
- Plating and gauging order is stated.
- Gauge frequency is stated: first article, sample or all parts.
- Thread start has a chamfer or deburr callout.
- Gauge calibration is asked for if the lot is for a regulated market.
Have a fitting drawing with threads to check? Send it with the thread standards marked. We quote the finished parts within 24 business hours and place the work with one of the partner shops that turn brass.
Frequently asked questions
What do GO and NO GO mean on a thread gauge?
The GO end checks the maximum material limit. It must thread on or in over the full length of the thread, which proves the thread form and pitch fit together. The NO GO end checks the minimum material limit of the pitch diameter. It may start on one or two turns of a good thread but must not go further.
Why do NPT threads use a different gauge?
An NPT thread is tapered, so its fit depends on how deep the mating part goes, not on a fixed diameter. The usual check is an L1 plug or ring gauge that is screwed in by hand, and the end of the fitting must land within one turn either way of a notch or step on the gauge. A parallel GO and NO GO pair does not describe a taper.
Should I gauge threads before or after plating?
After. A plating layer adds thickness to the thread flanks, and the pitch diameter grows by about four times the layer thickness. A thread that passes before nickel plating can fail after it. If the drawing calls for plating, write that the thread must gauge after plating.
Alloys in this guide
| Alloy | Lead % | Mach. | DZR |
|---|---|---|---|
| C360 free-cutting brassC36000 · CuZn36Pb3 / CW603N | 2.5 to 3.7 | 100 | Poor |
Published typical values for the alloy. Machinability against C360 at 100. Not a promise from a shop.
Sources
- Wikipedia, Screw thread en.wikipedia.org
- Wikipedia, National pipe thread en.wikipedia.org
Need a quote for this part?
Send the drawing. We read it, send one itemised quote for the finished parts within 24 business hours and place the work with a partner shop that turns brass. Brass only.
Get a quote for your brass parts