Skip to content
Brass CNC Parts

Guides / Choosing a Supplier

The Five Checks a Brass Fitting Needs Before It Ships

Published September 27, 2026. Reviewed for the facts in the corrections log.

Quality control on a machined brass part comes down to five checks. Dimensional inspection, go and no-go thread gauging and a spectrometer check of composition apply to almost any part. A hydrostatic or pneumatic pressure test applies where the part seals. ISO 6509 dezincification testing applies where it sits in water. Name the checks that apply on the RFQ.

A brass part can look correct and still fail in the field. Most of the failure modes that matter on a machined brass fitting do not show up by eye, which is why the checks below exist rather than a visual inspection alone.

This is not a certification claim. None of this describes a standard this site holds, and it is not a promise about any specific shop. It is what to ask for on the RFQ and to expect back with the parts.

1. Dimensional inspection

The most basic check and the one buyers assume happens by default. Every toleranced feature on the drawing, bore diameter, length, concentricity, thread pitch diameter, gets measured against the print, usually with a CMM on tighter tolerances or gauges and a height stand on looser ones.

What it catches: tool wear drifting a dimension over a long run, a fixture that was not holding the part square, a setup error on the first article that nobody caught before the batch ran.

What to ask for: a dimensional report on the first article at minimum, and on the full batch if the tolerance is tight enough that drift across a run is a real risk. See reading tolerances and surface finish callouts for how to write the tolerance so this check has something specific to measure against.

2. Thread gauging

A thread that looks clean under a loupe can still be out of class. Go and no-go gauges check the thread against its pitch diameter tolerance band, the go gauge should thread on smoothly and the no-go gauge should not enter more than a turn or two.

This matters more on brass than it sounds like it should, because brass threads easily enough that a worn tool can keep cutting a thread that looks fine and passes a casual check, while quietly drifting out of the gauge tolerance. On a sealing thread, NPT or BSPT, gauging is what actually predicts whether the joint seals rather than just looking threaded. See NPT vs BSP thread standards for how the classes differ.

What it catches: an out-of-tolerance pitch diameter, a worn thread-cutting tool nobody swapped in time, a joint that will leak or over-torque on assembly even though it looks correct.

What to ask for: confirmation that go and no-go gauges were used, and to which class. A shop running sealing threads in volume should be able to answer this without hesitating.

3. Composition verification

The mill certificate states what the bar was supposed to be. Composition verification confirms the finished part actually matches it, usually with a handheld or bench spectrometer (XRF or optical emission) checking copper, zinc, lead and any alloying element against the specified range.

This matters most where the alloy is doing regulatory work rather than just mechanical work, a lead-free brass on a drinking water part, a DZR grade on a water fitting. Bar stock does occasionally get mixed up between grades that look identical once cut, especially between C360 and a lead-free look-alike bar of similar size.

What it catches: a mixed-up bar pull, a grade substitution nobody flagged, a lead-free claim that does not hold up under test. See material certificates and EN 10204 3.1 for what the certificate itself should say before the part is even cut.

What to ask for: a spectrometer reading on a sample from the batch when the alloy is doing compliance work, not just a repeated statement of the bar’s nominal composition.

Need a quote for this part? Get a quote for your brass parts

4. Pressure or leak testing

Only relevant where the part actually holds a fluid or gas under pressure: valve bodies, fittings, manifold blocks. A hydrostatic test holds the part at a specified pressure with water or another liquid and checks for a drop or visible weep. A pneumatic test does the same with air or another gas, usually at lower pressure, sometimes under water to see bubbles.

What it catches: a porous casting or forging that machining exposed, a thread that looks fine on the gauge but does not seal, a cross hole or drilled passage with a burr breaking the seal.

What to ask for: the test pressure and hold time relative to the part’s rated working pressure, and whether it was a hydrostatic or pneumatic test. A part rated for 200 psi tested at 210 psi for five seconds is not the same assurance as one held at 300 psi for a minute, and the drawing should say which is expected.

5. Dezincification testing where the part is a water or marine part

The one check that is not about the individual part but about the alloy’s resistance to a specific failure mode. ISO 6509 exposes a sample to a copper chloride solution for 24 hours, then sections it to measure how deep the zinc leached out. This is a batch or bar-level test, not something run on every finished part, and it is usually the mill’s result rather than the machining shop’s.

What it catches: an ordinary yellow brass supplied where a DZR or silicon brass grade was specified, which will not show up on a spectrometer reading of copper and zinc content the way a lead mix-up would, because the difference is structural rather than purely compositional in some cases.

What to ask for: the ISO 6509 result on the mill certificate, not just a composition statement, whenever the part is going into hot water, a recirculating loop or a marine environment.

What this looks like on an RFQ

Naming the checks that apply, rather than writing “inspect all parts,” gets a more specific answer back:

Dimensional report on first article and one piece per 500 thereafter.
Thread: 3/8-18 NPT, go/no-go gauge required, record pass/fail.
Alloy: C69300 silicon brass, spectrometer check on batch sample.
Pressure test: hydrostatic, 250 psi, 60 second hold, no visible weep.
Water service, hot recirculating loop: ISO 6509 result required on
mill certificate, max depth 200 micrometres.

Not every part needs all five. A dry electrical terminal needs dimensional and maybe composition, nothing else on this list. A valve body in a hot water loop needs all five. The RFQ checklist for a brass drawing covers what else belongs on the print alongside this.

Not sure which checks apply to your part? Send the drawing and describe the service, sealing requirement and environment. That is what decides which of these five actually matter, and which partner shop we place the part with.

Frequently asked questions

Who runs these checks, the buyer or the shop?

The shop, as part of making the part. A buyer's role is to say which checks apply to the part on the RFQ and ask what paperwork comes back with the shipment. Asking after the parts arrive is asking too late, since some checks, like a destructive dezincification test, are done on a sample from the batch rather than on every piece.

Is a material certificate the same thing as a quality check?

No. A mill certificate, often called a 3.1 certificate, states what the bar stock is: composition and sometimes mechanical properties, tested by the mill before the shop ever cuts it. The five checks here are about the finished part after machining. A brass bar can carry a clean certificate and still leave the lathe with a torn thread or a cross hole burr, so the two are not substitutes for each other.

Do all five checks apply to every brass part?

No. Pressure testing only makes sense on a part that seals a fluid or gas, a valve body or a fitting rather than a flat bracket. Dezincification testing to ISO 6509 only matters where the part sits in water, and it is usually a batch or bar-level check rather than a per-part one. Dimensional inspection and thread gauging apply to almost anything with a toleranced feature or a thread.

What paperwork should actually come back with the parts?

At minimum, a certificate of conformance stating the parts were made to the drawing. On a tolerance-critical part, ask for a dimensional report against the print, either a CMM printout or a manual inspection sheet. On a threaded fitting, ask whether go and no-go gauges were used and to what class. On a water or marine part, ask for the mill certificate with any ISO 6509 result, not just a composition statement.

Sources

  1. Hydrostatic test, Wikipedia en.wikipedia.org
  2. X-ray fluorescence, Wikipedia en.wikipedia.org
  3. ISO 6509-1, dezincification resistance of copper alloys with zinc iso.org

Need a quote for this part?

Send the drawing. We read it, send one itemised quote for the finished parts within 24 business hours and place the work with a partner shop that turns brass. Brass only.

Get a quote for your brass parts