Brass RFQ Checklist
Everything a shop needs to quote a brass part once, without a round of questions. Print it or save it as a PDF, tick it off against the drawing, then send.
Material
- Alloy by UNS or EN number, not "brass"
- Why that alloy: a standard, an environment or a preference
- If a standard decides it, write the standard and leave the grade open
- Certificate type needed: EN 10204 2.2 or 3.1
- Stock form if it matters: bar, hex, tube, forging
Geometry and tolerance
- General tolerance class in the title block, ISO 2768-m or similar
- Tight tolerances only on the features that need them
- Concentricity or runout where a seal or a bearing needs it
- Wall thickness under 1 mm and length to diameter over 8 flagged
- STEP file plus a PDF drawing, not one or the other
Threads
- Standard and class on every thread: NPT per ASME B1.20.1, G per ISO 228-1, M10 x 1.0-6g
- Which threads seal and which only hold
- Gauge requirement on sealing threads
- Whether a rolled thread is acceptable
- Thread start chamfer and burr condition
Bores and edges
- Burr condition inside bores and at cross holes
- Edge break where not otherwise stated
- Surface finish only where it matters, with an Ra value
- Which faces are sealing faces
Finish and marking
- Plating type and thickness, or none
- Anti-tarnish, lacquer or bare
- Marking content, method and location
- Packaging: VCI, bulk or individually bagged
Compliance
- Potable water: NSF/ANSI 372 and 61, or 4MS listed alloy for the EU
- RoHS and whether exemption 6(c) is relied on
- REACH composition statement if lead is over 0.1 percent
- Dezincification to ISO 6509 for hot water and marine parts
- Stress relief for cold worked parts in ammonia or moisture
Quantity and delivery
- Quantity now and whether it repeats, and how often
- Prototype and production pricing together if it will repeat
- Needed by date, with the first article date separately
- Region or country of supply if it matters
- Inspection paperwork to ship with the parts
brasscncparts.com, brass only. Background for each line is in the guides at https://brasscncparts.com/blog/ and the standards index at https://brasscncparts.com/standards/.
Background for each line: the RFQ checklist guide, the standards index and the thread chart. Brass only.