Skip to content
Brass CNC Parts

Request a Brass Machining Quote

Tell us about the part. We reply within 24 business hours with a written read of it and one itemised quote. Brass only. Send aluminium, steel or plastic and we will say no.

Not sure the drawing is complete? The one page checklist covers what a shop needs to quote once.

What happens next

  1. We read your RFQ

    We check the drawing, the grade, the threads and the finish. If something is missing we ask before we quote.

  2. We quote the finished parts

    One itemised quote: material, machining, finish, inspection, packing and freight. Potable water parts are placed only with shops that run lead-free grades.

  3. Made, inspected and shipped

    We place the work with a partner shop and an engineer follows the run. You get a progress update every week and one invoice. Payment terms are confirmed on your quote.

Not sure which grade to ask for? Run the grade selector, or describe where the part ends up and which standard it has to meet and leave the grade as Not sure. A shop can offer the alloy that passes for less.

What the reply looks like

A sample, not a real RFQ. Every reply carries these five parts, whether the answer is a quote or a clear no.

Subject: Your brass RFQ: hose barb adapter, C69300, 2,500 pcsSample

Thanks for the drawing. Here is our read of the part before it goes anywhere.

Machine class: bar-fed turret lathe, 25 mm hex bar. Not a Swiss job at 48 mm long and not a mill job at this quantity.

Alloy: you asked for C69300 and the part is wetted, so that is right. C360 would not clear NSF/ANSI 372. A bismuth brass would also pass and may be cheaper, so we have left the grade open to both.

Compliance flags: NSF/ANSI 61 and 372 named on the drawing, 3.1 certificate requested. We will only place this with a shop that has shipped lead-free potable water parts.

Watch points: the 1/2-14 NPT is a sealing thread, so we have asked for gauge class on the quote. The barb bore meets a cross hole, so internal burr condition is called out.

Quote: one itemised price for the 2,500 finished parts is attached, with inspection, packing and freight as separate lines. Once you approve it, an engineer follows the run and you get a progress update every week.

Potable water, gas and medical parts are placed only with shops that already run lead-free brass with certificates.

We place the work in your preferred region when a partner shop there fits the part.

STEP, IGES, PDF, DWG or DXF. Keep the total under about 10 MB. Larger files, or uploading from a phone, can fail silently: send the form without them and email the files to after, quoting the part name.
Reply within 24 business hours.