The alloy figures, dates and limits on this site are published typical values and rules as of the date checked. When one moves, or a reader shows one is wrong, the fix is recorded here.

Found something wrong? Reply to any email from us, or send a note through the RFQ form with "correction" in the part description. We fix it and log it.

DateWhat changedWhere
2026-10-20Lead range for C36000 stated as CDA lists it: 2.5 to 3.0 percent, with C36010 at 3.1 to 3.7. The 2.5 to 3.7 figure on this site covers both numbers. C353 datasheet now notes rod and bar under ASTM B453/B453M. C69300 datasheet notes that published machinability ratings run from 80 to 85; the site keeps 80. CW617N datasheet notes the EN 12165:2024 composition change. Stress relief range in the season cracking guide softened to a common range, since a CW617N mill sheet lists 280 to 330 C./brass/
2026-10-20RoHS exemption 6(c) guide: added the footnote that the exemption does not cover equipment supplied to the general public that children may place in the mouth, unless the lead release limit is met./blog/rohs-exemption-6c-leaded-brass-2027/
2026-10-06Brass machining processes page published. Speeds, tolerances, stress relief range and forging crossover repeat the figures already in the guides./processes/
2026-09-27Alloy reference extended from 8 to 16 datasheets, with DIN, JIS and BS cross reference added to every one. Machinability ratings for the new grades are published typical values: C353 90, C345 90, C330 60, C230 30, C280 40, C443 30, CW617N 80, CW511L 40./brass/cross-reference/
2026-09-27Standards index, glossary, part type pages and three tools published. Every guide now carries a direct answer under its headline, the datasheets it relies on and the sources it cites./standards/
2026-09-25RoHS exemption 6(c) status updated: renewal request submitted December 2025 suspends the 30 June 2027 expiry pending a Commission decision./blog/rohs-exemption-6c-leaded-brass-2027/
2026-09-21Site published with 24 guides and 8 alloy datasheets./

What counts as a fact here

  • Alloy numbersComposition ranges, machinability ratings, tensile and hardness figures on the datasheets and in the guides. All published typical values for the alloy.
  • Rules and datesThe NSF/ANSI 372 limit, the RoHS 6(c) expiry, the EU positive list date, the Australian lead free transition. Stated as of the month checked and never as legal advice.
  • StandardsWhat a standard covers and what to write. We name them. We do not claim any part, shop or this site meets them.
  • Not factsWhich grade to pick for a part and what a shop will quote. Those are judgement and the shop's call, and they are written that way.

Reply within 24 business hours to any correction, same as an RFQ.