Home / Processes
How Machined Brass Parts Are Made, Process by Process
Most machined brass parts follow one route: bar stock is turned on a bar-fed or Swiss lathe, cross drilled and milled, threaded, deburred, stress relieved where needed, finished and inspected. Free-cutting brass C360 makes every cutting step fast. The steps that decide cost and rejects are threading, internal deburring and testing.
Figures are published typical values for free-cutting brass with modern tooling, never a promise from a shop.
The usual route for a turned part
Not every part uses every step. A plain pin skips threading and stress relief. A valve fitting uses all of them.
- 1Bar stock. Round or hex, cut to length.
- 2Turn or Swiss. Outside, bore, parting off.
- 3Cross drill and mill. Ports, flats, hex.
- 4Thread. Tap, roll or single point.
- 5Deburr. Inside and outside.
- 6Stress relieve. Where cracking is a risk.
- 7Finish. Tumble, plate, mark.
- 8Inspect and pack. Gauges, tests, anti-tarnish.
Cut
Where the shape comes from. Most brass parts start as bar and are turned, drilled and milled.
CNC turning
The bar spins and a fixed tool cuts the outside and the bore. It is the base process for round brass parts: fittings, pins, bushings, nozzles, valve stems. Bar-fed lathes run unattended, which is where the low piece price on small brass parts comes from.
- Why brassFree-cutting brass C360 breaks into short chips and puts little force on the tool, so a lathe can run at the top of its speed range. Lead-free grades need slower speeds and sharper tools.
- Commonly seenDiameters commonly held to ±0.01 mm and lengths to ±0.05 mm. As machined finish Ra 1.6 to 3.2. Starting surface speed for C360 in carbide is roughly 200 to 400 m/min.
- On the RFQMaterial and bar form, critical diameters boxed, general tolerance ISO 2768-m, quantity at two or three breaks.
- Read nextBrass speeds and feeds, Tolerances and surface finish
Swiss turning
A sliding headstock feeds the bar through a guide bushing and the tools cut within a few millimetres of it. With live tooling and a sub spindle the part comes off complete: turned, cross drilled, tapped, hex milled and parted off in one cycle.
- Why brassIt keeps long thin parts straight and removes second operations. Brass gives the short chip a Swiss machine needs. The setup is longer than a conventional lathe, so it rarely pays below about 100 pieces.
- Commonly seenBar up to about 32 mm on common machines, larger on some. Parts under 20 mm are the natural territory.
- On the RFQSay whether the part needs to be complete off the machine, list every cross hole and flat, give annual volume.
- Read nextSwiss machining for brass parts, Multi-spindle screw machines
CNC milling
A rotating cutter removes material from a stationary or indexed part. Used for flats, slots, pockets, hex forms and prismatic brass parts such as manifolds, valve bodies and hardware plates, and for second operations on turned parts.
- Why brassBrass mills cleanly with two or three flute carbide cutters and needs little coolant. Multi-axis machines reach cross ports and angled faces in one setup.
- Commonly seenFeatures commonly held to ±0.05 mm. Solid carbide end mill starting speed for C360 is roughly 150 to 300 m/min at 0.03 to 0.12 mm per tooth.
- On the RFQStarting form (bar, plate or forging), number of faces to machine, datum scheme, any 5-axis need.
- Read nextBrass speeds and feeds
Drilling, boring and reaming
Drills make the hole, boring bars and reamers bring it to size and finish. On brass fittings the cross hole that meets a bore is the feature that decides the leak rate.
- Why brassBrass drills fast, but a standard drill can grab on breakthrough. Shops dub the lips to zero rake. A drilled cross hole leaves an internal burr that tumbling cannot reach.
- Commonly seenDrilled holes commonly held to ±0.05 mm, reamed holes tighter. Solid carbide drilling starts at roughly 100 to 200 m/min.
- On the RFQHole depth to diameter ratio, reamed or drilled, and the burr condition at every intersection.
- Read nextDeburring cross holes, O-ring grooves and bore finish
Thread and form
Threads, knurls and other features added to the cut blank.
Threading and tapping
Internal threads are cut with a tap or formed with a roll tap. External threads are single-pointed on a lathe, milled or rolled. Pipe threads add a taper and a sealing rule.
- Why brassRoll tapping makes a smoother, stronger thread with no chip and suits blind holes and ductile lead-free brass, but it needs a larger drill. Cut taps are the default on C360. NPT and BSPP do not mate.
- Commonly seenThread class 6H or 2B is normal for a machine screw. Tap speed in C360 is roughly 15 to 30 m/min for a cut tap.
- On the RFQThread standard and class, gauge to use, through or blind, and whether a sealing thread is gauged at the L1 plane.
- Read nextRoll tap or cut tap, NPT against BSPP, Thread chart
Knurling
A hardened wheel presses a pattern into the surface for grip or for a press fit. Used on knobs, caps, inserts and fasteners.
- Why brassBrass is ductile and does not work harden much, so a form knurl raises a clean pattern in one pass. Form knurling grows the diameter, so the blank is turned smaller.
- Commonly seenPattern and pitch follow DIN 82 or ANSI B94.6. The finished diameter over the knurl takes a wider tolerance than a turned diameter.
- On the RFQPattern, pitch, finished diameter with a tolerance, and whether the knurl is plated after.
- Read nextKnurling brass parts
Hot forging, then machining
A heated brass billet is pressed to near net shape and the forging is machined only where it has to be exact: threads, sealing faces and bores. C377 forging brass is the usual alloy.
- Why brassIt saves metal and cycle time on bulky parts such as valve bodies, but the die costs money. Turning from bar wins at lower volumes.
- Commonly seenForging temperature is around 700 to 800 C. The crossover from bar is around 5,000 pieces a year for a bulky part.
- On the RFQAnnual volume, and whether you accept a forged blank or want bar.
- Read nextHot forging against machining, Machined against cast
Finish
Burrs, stress, surface and marking. Where a good part and a rejected one often part ways.
Deburring
Removal of the raised edges every cutting process leaves. Outside burrs yield to tumbling or brushing. Inside burrs at cross holes need a brush, abrasive flow, thermal or water jet deburring, or a chamfer that stops the burr forming.
- Why brassAn unremoved burr stops a screw starting, breaks off into a system or leaks at a seal. It is the most common reason a good looking fitting is rejected.
- Commonly seenNot a measured figure. State the condition: break edges, no burr at the bore intersection, checked by borescope.
- On the RFQBurr condition at every intersection and how it is verified.
- Read nextDeburring cross holes
Tumbling and vibratory finishing
Parts move in a bowl or barrel with abrasive or polishing media. It rounds outside edges and gives an even matte or bright surface on many parts at once.
- Why brassBrass responds fast because it is soft, which also means thin or sharp parts dent on contact. It does not reach inside a bore.
- Commonly seen20 minutes to a few hours, depending on the media and the finish wanted.
- On the RFQFinish wanted (matte or bright), and any face that must not touch media.
- Read nextTumbling brass parts
Stress relief annealing
A low temperature heat treatment after the last cold working step that relaxes residual stress without changing the alloy.
- Why brassHigh zinc brass under residual stress cracks in the presence of ammonia or amines, weeks or months after it passes inspection. The relief anneal removes the stress that feeds that cracking.
- Commonly seenUsually around 330 to 350 C for two to four hours, then cooled. The exact schedule depends on the alloy and the cold work.
- On the RFQSay it is required, name the test if one applies (ISO 6957), and leave the schedule to the shop.
- Read nextStress corrosion cracking
Cleaning, plating and passivation
Parts are degreased, rinsed and activated, then plated with nickel, chrome, tin, silver or gold, or given a thin clear finish. Plating is thin and follows the surface, so it shows every tool mark.
- Why brassCleaning decides whether the plate sticks. A better machined surface goes under a plated part. Plating usually runs at an outside house.
- Commonly seenAllow about two weeks for an outside plating house. Thickness and masking go on the drawing.
- On the RFQPlating type and thickness, whether dimensions apply before or after plating, masked areas.
- Read nextSurface finishes and plating, Cleaning before plating
Laser marking
A fiber laser engraves, textures or ablates the surface for logos, serial numbers and codes.
- Why brassBrass does not take the dark annealing mark seen on stainless. Contrast comes from engraving, a matte texture, or lasering through plating to expose the yellow metal.
- Commonly seenDepth and size are set per job. Decide whether marking comes before or after plating.
- On the RFQContent, location, size, depth, and order against plating.
- Read nextLaser marking brass
Check
What proves the part is right before it ships.
Inspection and testing
Dimensional inspection against the drawing, go and no-go thread gauging and a spectrometer check of composition cover most parts. Where a part seals, a pressure test is added. Where it sits in water, an ISO 6509 dezincification test applies.
- Why brassThe checks that apply depend on the part. A quote that does not name them is not comparable with one that does.
- Commonly seenPressure and hold time come from the product standard, not from the shop.
- On the RFQName each check, the sample size and the certificate type (for example EN 10204 3.1).
- Read nextQuality checks, Leak and pressure testing, Material certificates
Questions buyers ask about brass processes
Related references: alloy datasheets, part types, standards index and the glossary.
Which process makes most machined brass parts?
CNC turning from bar, usually on a bar-fed lathe or a Swiss lathe, followed by cross drilling, threading and deburring. Milling is added for flats and prismatic parts. Hot forging replaces bar only where a bulky part runs in volume.
Is a Swiss lathe always cheaper than a conventional lathe?
No. Swiss wins on small, slender parts with several features, made in the hundreds or more. Below about 100 pieces the longer setup usually costs more than the saving, and a stubby large part gains little.
Does lead-free brass need a different process?
The processes are the same, the settings change. Lead-free grades start at 60 to 80 percent of the C360 speed, need sharp positive rake tools and chip control, and a shop that has not run them before learns on the first bar. Say so on the RFQ.
Which finishing steps should I name on the drawing?
Name the burr condition at internal intersections, the stress relief if the part sees ammonia or amines, plating thickness with the before or after rule, and the pressure test if the part seals. The rest a shop will choose to fit the price.
Have a brass drawing?