Machining from bar gives a pore free part with no tooling, tight tolerances and a bright finish, in C360 or forged C377. Casting in C83600 or C85700 pays off on complex valve bodies with internal passages in real volume, but castings carry porosity risk, coarser tolerances and, in the leaded grades, far more lead than NSF/ANSI 372 allows.
A brass part can start life as a bar or as a casting. Most small fittings, adapters and connectors are cut from bar, because that route has no tooling, no porosity and the tightest tolerances. Castings earn their place on shapes a lathe cannot reach: valve bodies with cored passages, large thin walled housings, parts where turning from solid would throw away most of the metal.
The two routes use different alloys, carry different lead contents, hold different tolerances and are priced in different ways. This article sets them side by side so the route is chosen on the drawing rather than discovered in the quotes.
The two routes
Machined from bar. C360 free-cutting brass round or hex bar goes into a bar-fed lathe and the part comes off complete. On a bulky part in volume, a C377 forging brass blank is hot forged to near net shape first and only the sealing faces and threads are machined. Either way the metal is wrought: dense, uniform and with published mechanical properties that a mill certificate confirms. See forging or machining a brass part for the forging crossover.
Cast then machined. Molten brass is poured into a sand mould made from a pattern, into a ceramic shell built around a wax pattern for investment casting, or into a reusable metal mould for permanent mould casting. The casting is then machined for seats, ports, threads and faces. The casting alloys are not the bar alloys, and that is the first thing to understand.
The alloys are different
Bar stock brass is copper and zinc with lead for machinability. Casting brass usually adds tin for fluidity and strength in the mould, and the traditional grades carry far more lead than any bar alloy.
| Alloy | Route | Lead, nominal | Tensile, typical | Note |
|---|---|---|---|---|
| C360 free-cutting brass | Bar | 2.5 to 3.7 percent | 340 to 470 MPa | Machinability 100, the benchmark |
| C377 forging brass | Forged, then machined | 1.5 to 2.5 percent | 350 to 450 MPa | Machinability 80 |
| C83600 leaded red brass | Cast | about 5 percent | about 255 MPa | The classic valve body alloy, pressure tight |
| C84400 leaded semi-red brass | Cast | about 7 percent | about 235 MPa | Lower cost plumbing castings |
| C85700 leaded yellow brass | Cast | about 1 percent | about 345 MPa | Hardware and decorative castings |
| C89833 bismuth red brass | Cast | under 0.09 percent | about 235 MPa | Lead-free replacement for C83600 |
| C87850 silicon brass | Cast | under 0.09 percent | about 450 MPa | Lead-free, higher strength |
Published typical values for the alloys, cast values as sand cast, from the Copper Development Association casting alloy data. They describe the material, not a promise from any shop or foundry.
C83600, often called 85-5-5-5 for its 85 percent copper and 5 percent each of tin, lead and zinc, is the alloy inside most traditional bronze valves and pump bodies. Despite being sold as bronze it is a leaded red brass on the UNS system. Its machinability is published in the 80s on the same C360 scale, which is why cast valve bodies machine well.
Porosity and pressure tightness
A casting solidifies from liquid, and gas and shrinkage leave voids as it does. Most of them are harmless. One that connects an internal passage to a machined face is a leak, and it is usually found at pressure test after machining has opened it up.
C83600 became the valve body alloy because its lead fills the microporosity and makes the casting pressure tight. That is the property the lead-free casting grades have to earn instead through gating, pouring temperature and foundry discipline, and it is why fewer foundries pour them well. A porous casting can be rescued by vacuum resin impregnation, which is an extra process and an extra cost.
Bar has none of this. Wrought metal is dense all the way through, so a part turned from C360 or forged from C377 passes a pressure test on its geometry alone. On a pressure part, stay on bar or a forging unless the shape forces a casting. If it is cast, write the test pressure on the drawing and say whether impregnation is permitted. See the five checks a brass part needs.
Lead, and the potable water problem
C83600 carries about 5 percent lead. NSF/ANSI 372 sets a 0.25 percent weighted average lead limit across the wetted surfaces of a drinking water product, so the traditional valve body alloy is twenty times over the line on its own. On a valve body almost every surface is wetted, so there is no averaging to hide behind, and the weighted average calculator will show it in seconds.
That is why the lead-free casting alloys exist. C89833 bismuth red brass replaces the lead with bismuth and keeps the red brass character. C87850 silicon brass is the casting cousin of the C69300 bar alloy, stronger and highly dezincification resistant. Both are poured by fewer foundries than C83600 and both are harder to get pressure tight. The EPA describes the rule as it applies to pipes, fittings and fixtures. This is a description of the standard, not legal advice.
On the bar side the same split applies. C360 is also over the limit, and C69300 silicon brass bar is the usual lead-free answer, with wider stock and more shops that have run it than any lead-free casting grade. See NSF/ANSI 61 and 372 for brass fittings. For a potable water part that could take either route, bar is the easier compliance path.
Need a quote for this part? Get a quote for your brass parts
Tooling and volume
Bar needs no tooling. Setup on a bar-fed lathe is the only fixed cost.
A sand casting pattern is cheap, wood or plastic, and can pay for itself in a few dozen pieces if the shape is bad enough for bar. Investment casting needs a wax injection tool and repays it in the hundreds. Permanent mould casting needs a machined metal mould and repays it in the thousands. Every casting also needs a machining fixture, because a casting has no reference surface until the shop makes one.
The crossover is therefore about shape before it is about count. A round part with threads and no internal passages stays on bar at any volume, because the lathe already makes it complete in one operation. A tee shaped valve body with three ported bores and a cored waterway goes to casting early, because turning it from a solid bar the size of its widest point throws away most of the metal and still cannot reach the inside.
Surface finish and tolerance
As made, a sand casting comes out at roughly Ra 12.5 to 25 µm with a tolerance around plus or minus 0.5 to 1 mm on a small part. Investment casting is finer, roughly Ra 1.6 to 3.2 µm and plus or minus 0.1 to 0.25 mm. A turned bar part comes off at Ra 0.8 to 1.6 µm and holds plus or minus 0.01 to 0.05 mm without trying. Those are planning figures for the process, not a promise from any shop.
Plating shows every pore in a cast surface, so a casting that will be plated needs a finer process or more polishing. See tolerances and surface finish on brass parts.
When a casting is right
- Valve bodies with cored internal passages, tees, crosses and angled ports that no tool can reach from outside.
- Large parts where bar waste is excessive, such as a housing 120 mm across with a thin wall.
- Thin walls at size, which bar machining cannot leave without distortion.
- Real volume and a stable design, hundreds and up for sand casting, thousands for the other methods.
When bar is right
- Anything round with threads, which is most fittings, adapters and connectors.
- Under a few thousand pieces, or a design that will change.
- Pressure tight parts where porosity is not acceptable.
- Tight tolerance across most of the part.
- Potable water parts, where lead-free bar is easier to source than lead-free castings.
What to put on the RFQ
Say the route, or leave it open on purpose. Send the drawing, the annual quantity, the test pressure and the fluid, and ask the shops to quote the route they would choose. Write the lead requirement as the standard, NSF/ANSI 372, not only as an alloy name. If the part is already a casting and only needs machining, say so and attach the casting drawing with its datum, because it changes which partner shop we place it with.
This site matches machined brass parts. Whether the route is bar, a forging or a casting you already have, send the drawing with the quantity and the pressure, and we quote the finished parts and place the work with one of the partner shops that machine brass.
Frequently asked questions
Is a cast brass part weaker than a machined one?
Usually, yes. The common casting alloys are rated lower in tensile strength than C360 bar, C83600 red brass at about 255 MPa against 340 to 470 MPa for C360, and a casting can carry porosity that bar never has. A sound casting in the right alloy is strong enough for valve bodies and pump housings, which is what the alloys were designed for. Strength is rarely what decides the route. Shape, volume and lead content decide it.
Can a brass casting be pressure tight?
Yes, and C83600 leaded red brass is the classic valve body alloy precisely because its lead fills the microporosity and makes castings pressure tight. The lead-free casting grades such as C89833 and C87850 have to earn the same result through foundry practice, and a porous casting can be rescued by vacuum resin impregnation at extra cost. Write the test pressure on the drawing and ask who runs the test, because a leak is usually found after machining has opened the void.
Do brass castings meet the NSF/ANSI 372 lead limit?
Not the traditional ones. C83600 carries about 5 percent lead and C84400 about 7 percent, against a 0.25 percent weighted average limit across wetted surfaces. On a valve body almost every surface is wetted, so there is no averaging to hide behind. Lead-free casting alloys, C89833 bismuth red brass and C87850 silicon brass among them, are made for this, and fewer foundries pour them. The standard describes the limit. This is not legal advice.
Where is the volume crossover between casting and machining from bar?
Lower than for forging, because a sand casting pattern is cheap. A complex shape can justify sand casting from a few dozen pieces if turning it from solid would waste most of a large bar. Investment casting needs hundreds of pieces to repay its wax tooling and permanent mould casting needs thousands. A round part with threads and no internal passages stays on bar at any volume, because the lathe already makes it complete in one operation.
Alloys in this guide
| Alloy | Lead % | Mach. | DZR |
|---|---|---|---|
| C360 free-cutting brassC36000 · CuZn36Pb3 / CW603N | 2.5 to 3.7 | 100 | Poor |
| C377 forging brassC37700 · CuZn39Pb2 / CW612N | 1.5 to 2.5 | 80 | Poor |
Published typical values for the alloy. Machinability against C360 at 100. Not a promise from a shop.
Sources
- Copper Development Association, C83600 casting alloy data alloys.copper.org
- US EPA, use of lead free pipes, fittings, fixtures, solder and flux for drinking water epa.gov
Need a quote for this part?
Send the drawing. We read it, send one itemised quote for the finished parts within 24 business hours and place the work with a partner shop that turns brass. Brass only.
Get a quote for your brass parts