Skip to content
Brass CNC Parts

Brass reference / Forming brass

C230 red brass

A high copper brass that does not dezincify, supplied mostly as tube and pipe, and slow to machine.

Also known as Red brass, 85/15 brass, Alloy 230, Rich low brass. Published typical values for the alloy, never a promise from a shop.

30Machinability, C360 = 100
under 0.05%Lead, under the 0.25% line
HighDezincification resistance
270 to 500 MPa depending on temperTypical tensile strength

Composition

ElementNominal weight %
Copper84.0 to 86.0
Lead0.05 max
Iron0.05 max
Zincremainder

Properties

  • UNSC23000
  • EN equivalentCuZn15 / CW502L
  • DIN2.0240 CuZn15
  • JISC2300
  • BSCZ102
  • Hardness45 to 80 HRB
  • Density8.75 g/cm3
  • Typical tolerance±0.05 mm, tighter needs a finish pass
  • Common formsTube, pipe, sheet, strip, some rod

What it is for, and what it is not

Specify it for

  • Plumbing pipe and fittings machined from red brass tube
  • Heat exchanger and radiator tube
  • Parts that need dezincification resistance without arsenic or tin
  • Weatherstrip, conduit and drawn shapes

Do not specify it for

  • Turned parts from bar, it is rated 30 against C360
  • Anything chosen for machinability
  • Parts where the reddish colour is not wanted after polishing

What a buyer should know

With 85 percent copper this alloy sits above the zinc level where dezincification happens, which is why it has been the plumbing tube brass for a century. It is a forming and drawing alloy, single phase and ductile, and it machines like a soft copper: long chips and slow speeds. Do not confuse it with the red brass casting alloys such as C83600, which are leaded and behave completely differently.

Closest alternatives

AlloyLead %Mach.DZRWhy you might switch
C464 naval brassC46400under 0.2030HighAbout 1 percent tin added for seawater and dezincification resistance, at a heavy cost in machinability.
C260 cartridge brassC26000trace30PoorMade for deep drawing and cold forming, not for cutting, and rated 30 against C360 at 100.
C443 admiralty brassC44300under 0.0730HighA 70/30 brass with tin and arsenic for condenser tubes, highly dezincification resistant and slow to cut.

All 16 alloys compared · Cross reference

Need a shop that runs C230?

Send the drawing. We reply within 24 business hours with one itemised quote for the finished parts.

Get a quote