Guides / Materials
Brass Bar Stock: Forms, Sizes, Tempers and Tolerances
Published September 27, 2026. Reviewed for the facts in the corrections log.
Brass bar stock comes as round, hex, square and rectangular bar, tube, extruded profiles and forging billet. Free-cutting brass C360 is stocked in rounds from 3 to 100 mm and 1/8 to 3 inches, and in hex sizes that match wrench sizes, in 3 to 4 metre or 12 foot lengths. Lead-free grades come in fewer sizes.
A brass part is cut out of something, and what that something is settles a good part of the price before the first tool moves. Free-cutting brass C360 comes as round, hex, square and rectangular bar in a wide spread of sizes, and the cheapest part is usually the one drawn around a size that already exists.
This guide covers the forms, the common sizes, the temper and tolerance of drawn bar and what to write on the RFQ so a shop can use the stock it can actually get.
The forms brass comes in
Round bar. The default for turned parts and the form held in the most sizes. The Copper Development Association datasheets list the product forms each alloy is made in, and rod is on almost all of them. Drawn to size below roughly 50 mm, extruded above it.
Hex bar. For anything with a wrench flat. The hex is drawn onto the bar at the mill and the corners carry a small radius. The shop turns the round features and leaves the hex alone. Most brass fittings start here.
Square and rectangular bar. Blocks, manifolds, terminals and keys. Rectangular bar is often called flat bar and is sold by thickness and width.
Tube. Seamless or drawn, for sleeves, spacers and bodies where the bore is most of the part. Starting from tube saves drilling a deep hole and the metal that hole would have been.
Extruded profiles. Angles, channels, T sections and custom shapes, mostly in C385 architectural bronze, which despite the name is a brass. Hardware makers run their own dies so the profile arrives near net shape.
Forging billet. Slugs cut from C377 bar or extruded rod, sized to the die, for parts that are forged first and machined second.
Common round and hex sizes
Round bar is stocked in metric sizes from about 3 mm to 100 mm and imperial sizes from 1/8 inch to 3 inches. Hex bar is stocked by the distance across flats, in sizes chosen to match wrench sizes.
| Metric round, mm | Imperial round, in | Metric hex A/F, mm | Imperial hex A/F, in |
|---|---|---|---|
| 6 | 1/4 | 7 | 1/4 |
| 8 | 5/16 | 8 | 5/16 |
| 10 | 3/8 | 10 | 3/8 |
| 12 | 1/2 | 13 | 1/2 |
| 16 | 5/8 | 17 | 11/16 |
| 20 | 3/4 | 19 | 3/4 |
| 25 | 1 | 22 | 7/8 |
| 30 | 1 1/4 | 24 | 1 |
| 32 | 1 1/2 | 27 | 1 1/8 |
| 40 | 2 | 32 | 1 1/4 |
| 50 | 2 1/2 | 36 | 1 1/2 |
| 60 | 3 | 41 | 1 3/4 |
Common stock sizes for C360 bar. Each column is its own list, not a conversion of the one beside it. Stockist ranges vary and lead-free grades cover fewer of these.
Two hex facts. The corner to corner distance is 1.155 times the across flats size, which is what sets the round bar the hex was drawn from. And a round feature turned on a hex bar cannot be larger than the across flats size, or it carries flats. A part with a 22 mm hex and a 24 mm round shoulder next to it cannot come from 22 mm hex bar.
Lengths and what a bar feeder can take
Drawn bar is sold in 12 foot lengths in the United States and in 3 or 4 metre lengths in Europe. Swiss and fixed headstock lathes with bar feeders take a full 3 metre or 12 foot bar. Short loaders take 1 to 1.5 metres and the shop cuts the bar down. Either way the last 100 to 300 mm of every bar cannot be pushed through the collet and is consumed as remnant.
Bar capacity is the other limit. Common Swiss machines take 20, 26 or 32 mm bar, and fixed headstock bar feeders go larger. A part that fits inside a 32 mm bar has the most machines available to it, as the guide to Swiss turning brass parts sets out.
Temper
Drawn bar arrives cold worked, and how much is the temper. ASTM B16 is the specification for free-cutting brass rod, bar and shapes for use in screw machines, and its European counterpart is EN 12164 for copper alloy rod for free machining purposes. In the ASTM system, what a stockist means by C360 bar is half hard, H02. EN 12164 designates the condition by minimum tensile strength instead, so the same bar carries an R number on a European certificate.
Hard temper, H04, is stocked in smaller sizes. It is stiffer, holds a thread form well and is a little harder to cut. Soft or annealed bar is supplied on request for parts that will be bent, flared or staked after machining.
Above roughly 50 mm the bar is extruded rather than drawn. It is softer, rougher and looser in tolerance, so a large part usually gets a cleanup pass over its whole surface.
Need a quote for this part? Get a quote for your brass parts
Tolerance of drawn bar
Drawn round bar holds its diameter closely. On C360 round bar plan on roughly plus or minus 0.04 mm up to 12 mm, 0.05 mm up to 25 mm and 0.08 mm up to 50 mm. Hex across flats runs looser than round diameter, and extruded bar looser again. The exact figures are in the ASTM and EN specifications and on the stockist’s mill certificate. Use those, not these.
Why it matters: the as-drawn surface is often left on the finished part. The hex on a fitting is usually never machined. If the drawing tolerances it to plus or minus 0.02 mm, the shop has to mill it, and a feature that was free now costs a live tooling operation on every piece. Tolerance as-drawn features to what bar holds, and put the tight numbers on the features that are cut.
Pick the stock size and keep the metal
Bar is bought by weight, and everything outside the part’s largest diameter leaves as chips at scrap value. Metal goes with the square of the diameter, so a part with a 24 mm largest feature made from 30 mm bar instead of 25 mm bar buys 44 percent more metal for the same part.
Three habits follow.
Design the largest diameter to a stock size, less a cleanup. A finished 25.0 mm turned diameter needs 28 or 30 mm bar, because the bar surface has to be cleaned. A 24 mm finished diameter comes from 25 mm bar. If the outer surface can stay as drawn, 25 mm bar makes a 25 mm part with no cleanup at all.
If the largest feature is a hex, start from hex. Choose an across flats size that matches a wrench and exists as stock, and keep every round feature at or under it.
Weigh it. The bar weight calculator turns a stock size and a part length into grams, which is what the shop prices.
Lead-free bar is thinner on the ground
C360 is held in every size on the table above by most brass stockists. C69300 silicon brass is held in the common fitting sizes, in fewer in-between sizes, often with longer lead times and mill minimums on anything unusual. Bismuth brass is thinner still.
The consequence for a drawing is simple. On a lead-free part, do not specify a stock size. State the alloy requirement and the reason, give the finished dimensions and let the shop choose the bar it can actually buy this week. Naming 26 mm hex in C69300 on a drawing when the stockist holds 24 and 27 turns a quote into a question.
What to put on the RFQ
- The alloy and the reason for it. C360 for a dry service fitting, a lead-free grade with the standard named for potable water.
- The largest round diameter and the largest hex on the part. That is what decides the bar.
- Whether as-drawn surfaces are acceptable, and if so, tolerance them to what bar holds.
- Temper only if it matters, with a word on why, so the shop does not order soft bar for a part that wanted half hard.
- Stock size at the shop’s discretion unless a feature depends on it.
Material: C360 (CW603N) to ASTM B16 or EN 12164,
half hard. 22 mm hex A/F as drawn, flats not
machined. Round stock size at shop's discretion.
That note tells a shop everything it needs to pick the bar and nothing that stops it from picking the one it has.
Ready to quote a turned brass part? Send the drawing with the largest diameter and the quantity. We place the work with a partner shop whose bar feeders and stock racks fit the part.
Frequently asked questions
What sizes does brass round bar come in?
Free-cutting brass C360 is stocked in metric rounds from about 3 mm up to 100 mm, stepping by 1 or 2 mm at the small end and by 5 or 10 mm above 30 mm, and in imperial rounds from 1/8 inch to 3 inches in sixteenths and eighths. Above roughly 50 mm the bar is usually extruded rather than drawn, with a looser tolerance. Lead-free grades cover fewer of these sizes.
What does half hard mean on a brass bar?
It is the temper, the amount of cold work left in the bar after drawing. Half hard, H02 in the ASTM system, is the standard supply condition for C360 bar and gives the tensile and hardness figures on most datasheets. Hard, H04, is available in smaller sizes and is stiffer and slightly harder to thread. Soft, or annealed, is supplied on request for parts that will be bent or staked after machining.
Can a hex fitting be made from round bar?
Yes, by milling the flats, and it costs more. Hex bar arrives with the flats already there, so the shop turns the round features and leaves the hex as drawn. Milling a hex from round adds a live tooling operation and time on every part. The rule is to choose a hex across flats size that matches a wrench and exists as stock, then keep every round feature at or under that size.
Should I specify the bar size on the drawing?
Only when an as-drawn surface is a functional feature, such as a hex that stays unmachined. Otherwise give the finished dimensions and leave the stock size to the shop. A shop can see which bar it holds and which it can get this week, and on lead-free grades that choice can be the difference between a two-week lead time and a mill order. Naming a stock size the shop cannot buy just adds a question to the quote.
Alloys in this guide
| Alloy | Lead % | Mach. | DZR |
|---|---|---|---|
| C360 free-cutting brassC36000 · CuZn36Pb3 / CW603N | 2.5 to 3.7 | 100 | Poor |
| C385 architectural bronzeC38500 · CuZn39Pb3 / CW614N | 2.5 to 3.5 | 90 | Poor |
| C69300 silicon brassC69300 · CuZn21Si3P / CW724R | under 0.09 | 80 | High |
Published typical values for the alloy. Machinability against C360 at 100. Not a promise from a shop.
Sources
- ASTM B16, free-cutting brass rod, bar and shapes for use in screw machines astm.org
- Copper Development Association, product forms by alloy copper.org
Need a quote for this part?
Send the drawing. We read it, send one itemised quote for the finished parts within 24 business hours and place the work with a partner shop that turns brass. Brass only.
Get a quote for your brass parts