Brass Contact Pins, Sockets and Terminals

Brass contact pins, sockets, terminals and lugs are turned from C360 free-cutting brass on Swiss lathes and plated with tin, nickel or gold flash over nickel. C360 conducts at roughly 26 percent IACS, a published typical value. Brass has limited spring properties, so sprung contacts are stamped from C260 strip or phosphor bronze rather than turned from C360.

  • Usual gradesC360 free-cutting brass, C260 cartridge brass
  • Machine classSwiss lathe, bar fed, most pins under 6 mm diameter, turret lathe for lugs and larger terminals
  • Typical sizes0.6 to 6 mm pin diameter, 2 to 40 mm long, terminal lugs to M12 stud, banana plugs 4 mm
  • Commonly heldPin diameter commonly held to ±0.01 mm before plating, socket bore to ±0.02 mm, length to ±0.1 mm
  • FinishesTin, bright or matte, nickel, gold flash over nickel, silver on high current parts, all to a stated thickness
  • Standards to nameASTM B545 tin, ASTM B488 gold and ASTM B689 nickel plating thickness and class, IEC 60512 contact resistance and mating force tests where a connector maker requires them, RoHS Directive 2011/65/EU exemption 6(c) and REACH SVHC declaration for lead. See the standards index.
  • IndustriesConnector manufacturing, Test and measurement, Audio and consumer electronics, Battery packs and chargers, Automotive electrical, Industrial controls

What a brass contact does and where it goes

A contact pin is a turned pin that carries current across a separable joint. Its partner is a socket, a turned tube with a bore that the pin enters. Terminals and lugs carry current from a wire to a stud or a board. Banana plugs, test probe tips and battery contacts are the same idea in different shapes.

The turned brass part is the body. The contact surface is nearly always a plating, and the two are specified separately. Brass gives the shape, the thread and the crimp barrel. Tin, nickel, gold or silver gives the low resistance, corrosion free surface at the point where the two halves touch.

Why brass, and its limits

C360 free-cutting brass conducts at roughly 26 percent IACS, a published typical value for the alloy. Pure copper is 100 percent. That sounds poor until the geometry is considered. A contact pin is short and thick relative to the current it carries, so its resistance is small compared with the plating interface and the crimp, and 26 percent is plenty for signal and low power contacts. High current lugs and battery contacts sometimes move to copper or a high copper alloy, which this site does not match.

Brass is chosen over copper because it turns fast and holds a thread and a knurl. C360 is rated 100 for machinability, with a nominal 2.5 to 3.7 percent lead, a published typical value. Copper is rated around 20 and smears. For a pin bought by the hundred thousand the machinability sets the price.

Brass has limited spring properties. A socket that grips a pin by elastic force, or a leaf contact, needs a material that springs back after many cycles. Those are stamped from C260 cartridge brass strip, beryllium copper or phosphor bronze. This site matches turned brass parts, so a stamped spring contact needs another source. A turned socket in C360 gets its grip from a slotted, slightly closed bore rather than from spring temper, and that works for low cycle counts.

How contacts are made and what drives the price

Nearly all contact pins are Swiss turned from bar under 6 mm. The cycle is turn the pin, cut the retention groove or shoulder, drill the crimp or solder cup at the back, chamfer the nose and part off. A socket adds a bored contact hole and often a saw slot cut on the sub spindle. Cycle times are seconds, and the tooling for a slot or a fine thread sets the difference between shops.

Plating is the second price. Tin is the cheapest and suits most signal and power contacts. Nickel underplate with a gold flash of 0.1 to 0.25 micron is the usual choice for low level signals and long mating life. Thick gold is specified only where a standard demands it, because the price scales with the thickness. Plating is done in barrels for small pins and on racks for larger parts, and the plater is usually a separate business from the machine shop.

Volume decides everything. Setup on a Swiss lathe is the same for one thousand and for one hundred thousand pins, so the piece price falls steeply with quantity. Ask for two or three quantity breaks.

The features that go wrong

Burrs at the crimp cup and at the slot are the usual reject. A burr inside the crimp cup cuts wire strands, and a burr on a socket slot scores the pin plating. Ask for both to be deburred and inspected on a sample.

Plating thickness and adhesion are the second. A gold flash thinner than specified wears through in a few mating cycles and the nickel underneath tarnishes, so contact resistance climbs. Put the plating thickness on the drawing and ask for a plating certificate from the plater.

Diameter before and after plating are two different numbers. A pin turned to its finished diameter and then plated is oversize. State whether the drawing dimension applies before or after plating. Values quoted here are commonly held on this class of part, not a promise from any single shop.

Standards and compliance to name

Plating thickness and class follow ASTM B545 for tin, ASTM B488 for gold and ASTM B689 for nickel. Contact resistance and mating force tests follow IEC 60512 where a connector maker requires them.

For electrical and electronic equipment sold in the EU, leaded brass is permitted under RoHS exemption 6(c), which allows up to 4 percent lead in copper alloys. That exemption carries an expiry set for 30 June 2027 and a renewal request was submitted in December 2025. A contact pin in C360 is exactly the part the exemption exists for, and a product compliance file should record it. REACH may require an SVHC declaration for lead above 0.1 percent. This is not legal advice.

What to put on the RFQ

The lines that make a quote for this part comparable across shops.

  • 1Drawing with pin diameter, retention feature and crimp or solder cup size
  • 2Whether dimensions apply before or after plating
  • 3Plating: metal, underplate and thickness in microns, with a certificate if required
  • 4Current and voltage, so the shop can say whether brass is right
  • 5Mating cycles expected, because a turned socket suits low counts
  • 6Alloy: C360 unless the customer specification says otherwise
  • 7Quantity per order and annual volume

Grades for this part

AlloyLead %Mach.DZRWhy for this part
C360 free-cutting brassC36000 · CuZn36Pb3 / CW603N2.5 to 3.7100PoorThe benchmark every other metal is rated against for machinability, and the default for turned brass parts.
C260 cartridge brassC26000 · CuZn30 / CW505Ltrace30PoorMade for deep drawing and cold forming, not for cutting, and rated 30 against C360 at 100.

Published typical values for the alloy. Not a promise from a shop.

Is brass conductive enough for a connector pin?

For signal and low to moderate power contacts, yes. C360 conducts at roughly 26 percent IACS, a published typical value, and a short thick pin has so little resistance that the plated interface and the crimp dominate. High current lugs and battery contacts that run warm sometimes need copper or a high copper alloy at 80 percent IACS or more. Those are not brass and this site does not match them.

Which plating should a brass contact have?

Tin for most power and signal contacts that mate a few dozen times. Nickel where the part is handled or needs a hard surface. Gold flash over nickel, typically 0.1 to 0.25 micron, for low level signals and contacts that mate hundreds of times. Thicker gold only where a specification demands it, because the cost scales with thickness. Plate over a nickel barrier on brass, because zinc otherwise migrates into gold or tin and the surface tarnishes.

Can a brass socket be a spring contact?

Only in a limited way. A turned C360 socket can be slotted and slightly closed so the pin enters with an interference, and that works for a few hundred mating cycles. It is not a spring. Sockets that must grip through thousands of cycles are stamped and formed from C260 cartridge brass strip, phosphor bronze or beryllium copper and often carry a separate spring sleeve. This site matches turned brass parts only.

Does RoHS allow lead in a brass contact pin?

Yes, at present. RoHS exemption 6(c) allows up to 4 percent lead in copper alloys, which covers C360 at a nominal 2.5 to 3.7 percent. The exemption has an expiry set for 30 June 2027 and a renewal request was submitted in December 2025. If a renewal is refused, contact pins would need a lead-free brass such as C69300, which turns differently and is worth trialling early. This is not legal advice.

Have a drawing for this kind of part?

Send it. We place the work with a partner shop that has shipped this class of brass part and reply within 24 business hours with one itemised quote. Brass only.

Get a quote