Part types / Brass knurled knobs and thumb screws
Brass Knurled Knobs, Thumb Screws and Knurled Nuts
Brass knurled knobs and thumb screws are turned parts with a rolled knurl for finger grip, made from C360 free-cutting brass or C385 architectural bronze on Swiss and turret lathes. Knurl patterns follow DIN 82 or ANSI B94.6. They are polished, plated or lacquered and carry a threaded stud, a blind tapped hole or a set screw.
- Usual gradesC360 free-cutting brass, C385 architectural bronze
- Machine classSwiss lathe under 20 mm diameter, bar fed turret lathe with a knurling tool above, second operation for cross drilled set screw holes
- Typical sizes6 to 50 mm knurl diameter, M3 to M10 stud or tapped hole, 4-40 to 3/8-16 unified
- Commonly heldKnurl outside diameter commonly held to ±0.1 mm, bore or stud to standard thread class, faces to ±0.05 mm
- FinishesBright polished with clear lacquer, satin, bright nickel, chrome over nickel, black oxide, antique or aged finishes on decorative work
- Standards to nameDIN 82 knurl profiles and pitches, ANSI B94.6 knurling, the US equivalent, ISO 965 and ASME B1.1 thread classes, DIN 464 and DIN 465 knurled thumb screws, DIN 466 and DIN 467 knurled nuts, where a catalogue size will do. See the standards index.
- IndustriesScientific and laboratory instruments, Audio equipment, Cameras and optics, Machine guards and fixtures, Furniture and lighting, Musical instruments
What these parts are and where they go
A thumb screw is a screw with a head large enough to be tightened by hand, and the knurl on the head gives the fingers grip. A knurled nut is the female version. An adjustment knob carries a threaded stud or a tapped hole and moves something: a stop, a slide, a valve stem. An instrument knob sits on a shaft with a set screw or a grub screw and is the part the user touches.
They appear on laboratory instruments, audio equipment, cameras and optics, machine guards, jigs and fixtures, lighting and furniture. On most of these the part is seen, so the finish is specified as carefully as the thread.
Which alloy and why
C360 free-cutting brass is the default for a knob that will be plated or lacquered. It is rated 100 for machinability, it knurls cleanly because the lead breaks the chip, and it takes nickel and chrome well. Nominal lead is 2.5 to 3.7 percent, a published typical value for the alloy.
C385 architectural bronze is chosen where the part is left bright and polished, because it takes a slightly deeper colour and a higher polish, and where the knob starts as an extruded shape. It is a brass despite the name, rated 90 for machinability. It costs a little more per kilogram and is held in fewer bar sizes.
Neither is a potable water alloy, and a knob is rarely wetted, so lead-free grades are seldom needed here. If the knob is a valve handle in a drinking water system and touches the water, ask for C69300.
How knurled parts are made and what drives the price
The knurl is rolled, not cut, on all but the largest parts. A knurling tool with two or three hardened wheels is pressed against the turning bar and displaces the metal into ridges. On a Swiss lathe this is one pass before the part is turned, drilled and threaded. Straight, diagonal and diamond patterns are all rolled. The knurl raises the diameter, so the bar is turned slightly under the finished size first.
Cost sits in three places. The thread on a thumb screw stud is rolled or single pointed, and a long fine thread takes longer. A blind tapped hole in a knob must stop short of the face, and a deep blind tap in brass needs chip clearing. A cross drilled and tapped hole for a set screw is a second operation on a live tool or a separate machine and adds more than any other feature.
Finish is often the largest single cost. Polishing is hand or vibratory work, plating goes to a separate plating house and lacquer is a further step. On a decorative knob the finish can cost more than the turning. Ask for the price with and without finish so the two are visible.
The features that go wrong
Knurl quality is the first complaint. A knurl rolled with the wrong pitch for the diameter comes out with a double tracked, smeared pattern. A knurl rolled too deep on a thin wall crushes the bore. Name the pitch and the pattern from DIN 82 or ANSI B94.6 rather than writing knurled and hoping.
The knurl edge is sharp when rolled. A chamfer or a radius on both ends of the knurl is what stops it cutting fingers and what makes plating cover evenly. Ask for it.
Set screw holes drilled off centre or at the wrong angle leave the knob loose or cocked on its shaft. Dimension the hole from the bore, not from the outside. Plating fills a tapped hole, so specify whether the thread is to be masked, chased after plating or made oversize before plating. Tolerances quoted here are values commonly held on this class of part, not a promise from any single shop.
Standards to name
Knurl profile and pitch follow DIN 82 in Europe and ANSI B94.6 in the United States. The two do not map one to one, so pick one and name it. Threads follow ISO 965 or ASME B1.1.
Where a standard thumb screw or knurled nut will do, DIN 464, 465, 466 and 467 define sizes and a shop can quote against the number. No compliance standard applies to a dry decorative knob.
What to put on the RFQ
The lines that make a quote for this part comparable across shops.
- 1Knurl pattern and pitch from DIN 82 or ANSI B94.6, and the knurl length
- 2Thread size and class, stud length or blind hole depth
- 3Set screw hole size, position from the bore and angle, if any
- 4Finish: bright lacquered, nickel, chrome, black or none, plus whether threads are masked
- 5Alloy: C360 for plated parts, C385 for polished bare brass
- 6Chamfer or radius on the knurl edges
- 7Quantity, and whether a finished sample is wanted before the run
Grades for this part
| Alloy | Lead % | Mach. | DZR | Why for this part |
|---|---|---|---|---|
| C360 free-cutting brassC36000 · CuZn36Pb3 / CW603N | 2.5 to 3.7 | 100 | Poor | The benchmark every other metal is rated against for machinability, and the default for turned brass parts. |
| C385 architectural bronzeC38500 · CuZn39Pb3 / CW614N | 2.5 to 3.5 | 90 | Poor | A brass despite the name, supplied mainly as extruded shapes and the default where the part is seen. |
Published typical values for the alloy. Not a promise from a shop.
Questions buyers ask about brass knurled knobs and thumb screws
Further reading: Finishing a Machined Brass Part: Tumbling to Chrome, Swiss Turning Brass Parts and When It Is the Cheaper Route, Which Brass Alloy to Specify for a Machined Part.
What is the difference between DIN 82 and ANSI B94.6 knurls?
Both define straight, diagonal and diamond knurl patterns by pitch and profile angle, but the pitches are not the same numbers. DIN 82 works in millimetre pitch, for example RGE 0.8, and ANSI B94.6 in diametral pitch, for example 96 DP diamond. A shop tools for one system, so name the standard and the pitch on the drawing rather than converting between them.
Can a brass knob be plated and still show the knurl?
Yes. Nickel and chrome plating are thin, a few microns to about 25 microns, so a knurl with a pitch of 0.5 mm or coarser shows through clearly. Very fine knurls under 0.5 mm pitch soften visibly under a heavy plate. Plating also collects at the sharp knurl tips, so a chamfered or radiused knurl edge plates more evenly. Ask for a plated sample before the run if appearance is the point.
Should a bare brass knob be lacquered?
Bare brass tarnishes within weeks of handling. A clear lacquer keeps the polish for years indoors, and it is the usual finish on instrument and furniture knobs that are meant to look like brass. It wears through at the fingers on a heavily used knob, so on those a bright nickel or a deliberately aged finish is more durable. State which look you want, because a shop cannot guess it from the drawing.
Have a drawing for this kind of part?
Send it. We place the work with a partner shop that has shipped this class of brass part and reply within 24 business hours with one itemised quote. Brass only.