Skip to content
Brass CNC Parts

Part types / Brass bushings and plain bearings

Brass Bushings and Plain Bearings: Where Brass Fits

Brass bushings are sleeve, flanged or thrust plain bearings turned from C360 free-cutting brass for light loads, low speeds and corrosive or damp service. The lead in C360 acts as a solid lubricant. Bronze carries higher loads and speeds, and this site does not match bronze, so a bronze bushing RFQ needs another source.

  • Usual gradesC360 free-cutting brass, C464 naval brass
  • Machine classBar fed turret lathe for most sizes, Swiss lathe under about 16 mm outside diameter, thick wall tube stock where the wall is thin
  • Typical sizes3 to 60 mm bore, wall 1.5 to 8 mm, length 5 to 80 mm, flange up to 1.5 times the outside diameter
  • Commonly heldOutside diameter for a press fit commonly held to ±0.01 mm, bore to H7 by reaming, bore finish Ra 0.8 micron or finer
  • FinishesAs machined with a reamed or burnished bore, oil grooves cut on request, no plating on the bearing surface
  • Standards to nameISO 286 fits and tolerances for the press fit and the running clearance, ISO 4379 dimensions of copper alloy plain bearing bushes, where a standard size will do, NSF/ANSI 372 if the bushing is a wetted part in a US potable water pump or valve. See the standards index.
  • IndustriesMachinery and equipment, Marine hardware, Door and gate hardware, Pumps and valves, Instruments and mechanisms

What a brass bushing does and where it goes

A plain bearing is a sleeve that lets a shaft turn or slide inside it without rolling elements. A sleeve bushing is a plain tube. A flanged bushing adds a lip at one end that takes axial load and stops the bush walking through the housing. A thrust washer or thrust bushing takes axial load only.

Brass bushings appear in gate and door hardware, hand operated mechanisms, marine fittings, pump and valve stems, instrument pivots, agricultural equipment and any place a shaft turns slowly under light load where the environment is damp or corrosive.

Where brass suits and where it should be bronze

Brass is a light duty bearing material. It suits low loads, low sliding speeds, oscillating rather than continuous rotation and service where corrosion resistance matters more than wear life. A door hinge pin, a hand wheel, a pump stem guide and a marine pulley are brass jobs.

The lead in C360 does real work here. Rated 100 for machinability with a nominal 2.5 to 3.7 percent lead, a published typical value, the alloy holds its lead as soft particles that smear over the bearing surface and act as a solid lubricant when the oil film breaks down. That is why a leaded brass bush survives a dry start better than a lead-free one.

Lead-free brass bushings behave differently. Without the lead particles the bore has no built in lubricant, so a C69300 or bismuth brass bush needs a reliable oil or grease supply and a harder shaft. They are used where lead is restricted, not where bearing performance is the goal.

Bronze is the right call when the load or the speed goes up. Tin bronze, leaded bronze and aluminium bronze carry several times the pressure velocity product of brass and are what most engineered bearings are made from. This site supplies brass parts only. If your bushing is bronze, or if the load and speed calculation says it should be, this is not the place to send the RFQ.

How bushings are made and what drives the price

A bushing is turned from round bar or thick wall tube on a bar fed lathe. The outside is turned to the press fit size, the bore is drilled and bored or reamed, the flange is faced and the part is cut off. Long thin bushings come from tube to save material and cycle time.

The bore is the cost. A reamed bore to H7 with a fine finish is routine in C360. A bore that must be honed or burnished for a finer finish, or that must hold a tight clearance to the shaft after press fitting, adds operations. Oil grooves, straight or spiral, are milled with live tooling or cut on a second setup and add time per piece.

C464 naval brass is chosen for seawater and hot water bushings where ordinary brass would dezincify. It is rated 30 for machinability against C360 at 100, so the same bushing costs noticeably more to cut and the chip is long and stringy. Specify it because the environment demands it.

The features that go wrong

Press fit sizing is the usual dispute. A bushing pressed into a housing closes its bore by a proportion of the interference, and the shop cannot know the housing tolerance unless it is on the drawing. Give the housing bore and its tolerance, the interference you want and the finished bore after fitting, or accept that the bore is reamed after assembly at your end.

Bore finish decides wear life. A drilled bore is not a bearing surface. Ask for reamed, bored or burnished, and put a surface finish on the drawing. Ra 0.8 micron or finer is commonly held on a reamed brass bore, never a promise from a single shop.

A thin sleeve distorts during turning, so bushings with a wall under about 1.5 mm are prone to out of round bores. If the design allows, thicken the wall. If it does not, ask the shop how they hold the part. Burrs at the oil groove edges and at the bore chamfer scratch the shaft on first fitting, so ask for both to be deburred and for the bore chamfer to be a lead in rather than a sharp edge.

Standards to name

Fits and tolerances follow ISO 286. Standard bush dimensions are listed in ISO 4379 for copper alloy bushes, which is worth naming if you are not tied to a custom size.

There is no compliance standard for a dry brass bushing, but a bushing in a potable water pump or valve is a wetted part and NSF/ANSI 372 applies in the United States. This is not legal advice.

What to put on the RFQ

The lines that make a quote for this part comparable across shops.

  • 1Sleeve, flanged or thrust, with a drawing showing every diameter
  • 2Housing bore and tolerance, the intended interference and the finished bore after fitting
  • 3Shaft material, hardness and diameter tolerance
  • 4Load, speed and lubrication, so the shop can say whether brass is right
  • 5Bore surface finish and whether oil grooves are needed
  • 6Alloy: C360 for dry service, C464 for seawater or hot water
  • 7Quantity per order

Grades for this part

AlloyLead %Mach.DZRWhy for this part
C360 free-cutting brassC36000 · CuZn36Pb3 / CW603N2.5 to 3.7100PoorThe benchmark every other metal is rated against for machinability, and the default for turned brass parts.
C464 naval brassC46400 · CuZn38Sn1 / CW712Runder 0.2030HighAbout 1 percent tin added for seawater and dezincification resistance, at a heavy cost in machinability.

Published typical values for the alloy. Not a promise from a shop.

Should my bushing be brass or bronze?

Brass for light load, low speed, oscillating motion and damp or corrosive service, for example hinge pins, hand wheels and marine pulleys. Bronze for anything with a sustained load and continuous rotation, where the pressure velocity product is several times higher than brass can carry. If a bearing calculation is driving the choice, it is almost certainly a bronze job. This site supplies brass parts only and does not take bronze bushing RFQs.

Why does lead matter in a bearing brass?

The lead in C360 does not dissolve in the copper and zinc. It sits as soft particles through the structure, and on a bearing surface those particles smear into a thin film that carries the shaft when the oil is thin or absent. That is why a leaded brass bushing tolerates a dry start. A lead-free bushing has no such reserve and depends entirely on its lubricant and a hard, smooth shaft.

How should I specify the bore of a press fit bushing?

Either give the finished bore after fitting and let the shop calculate the pre fit size from the housing and interference you provide, or specify the bore as machined and ream it to size in the housing at your end. The second route is more common on small runs and gives a rounder bore. What does not work is a tight bore tolerance with no housing information, because the bore closes on fitting by an amount the shop cannot predict.

Have a drawing for this kind of part?

Send it. We place the work with a partner shop that has shipped this class of brass part and reply within 24 business hours with one itemised quote. Brass only.

Get a quote