Brass Standoffs and Spacers for PCBs and Enclosures

Brass standoffs are threaded hex or round pillars that hold a circuit board at a fixed height from a chassis or a second board. They are turned from C360 free-cutting brass on Swiss lathes in M2.5 to M6 and 4-40 to 1/4-20, usually nickel plated. Leaded brass in EU electronics relies on RoHS exemption 6(c).

  • Usual gradesC360 free-cutting brass
  • Machine classSwiss lathe from hex or round bar, bar fed turret lathe above about 12 mm across flats
  • Typical sizesM2.5 to M6 and 4-40 to 1/4-20 thread, 4 to 10 mm across flats, 3 to 50 mm long
  • Commonly heldLength commonly held to ±0.1 mm, across flats to the bar tolerance, tapped thread to 6H or 2B, male stud to 6g or 2A
  • FinishesBright nickel, electroless nickel, tin, clear passivate or bare brass for a short life indoors
  • Standards to nameISO 965 and ASME B1.1 thread tolerance classes, ASTM B689 electroplated nickel or ASTM B733 electroless nickel where a named plating spec is needed, RoHS Directive 2011/65/EU exemption 6(c). See the standards index.
  • IndustriesElectronics assembly, Telecoms and networking hardware, Industrial control cabinets, Test and measurement, Lighting

What a standoff does and where it goes

A standoff sets the gap between a printed circuit board and whatever it mounts to. A spacer is the same part without a thread, or with a plain bore. Together they are the most common turned brass part in an electronics assembly, and usually the cheapest.

The three forms are male-female with a stud at one end and a tapped hole at the other, female-female with a tapped hole at each end and male-male with studs at both ends. Hex bodies take a spanner during assembly. Round bodies are used where the standoff is visible or where a hex would foul a component.

They appear in control cabinets, network equipment, lighting drivers, test instruments, automotive electronics and anywhere two boards stack.

Why brass

Brass is used because standoffs are bought in quantity and cycle time is the whole price. C360 free-cutting brass is rated 100 for machinability, so a hex bar can be drilled, tapped and parted in a few seconds a piece. It does not rust, it is not magnetic and it conducts, which suits a standoff that is also part of the ground path.

Steel standoffs are cheaper by weight but cost more to machine and need plating to survive. Aluminium is lighter but galls against steel screws. Stainless is used where corrosion is severe. For a normal indoor electronics assembly brass is the default and no other grade on this site needs considering. The nominal lead in C360 is 2.5 to 3.7 percent, a published typical value for the alloy.

How standoffs are made and what drives the price

Hex standoffs start as hex bar of the finished across flats size, so the outside is never cut. On a Swiss lathe the cycle is face, drill, tap and part off. A male-female part adds a turn and a thread roll on the stud. Rolling the stud thread is faster than single point threading and gives a stronger thread.

The cost drivers are length, thread size and plating. A long standoff means a deep tapped hole and a slower drill. A small tap breaks more often than a large one. Nickel plating is a separate operation at a plating house and adds a fixed handling cost per batch. Ask for a quote with and without plating if the volume is small.

Unified sizes such as 4-40 and 6-32 are as common as metric in North American electronics. A shop that runs mostly metric will need to buy taps, so state the thread system clearly.

The features that go wrong

Length is the dimension that matters, because a stack of standoffs sets the board spacing and a 0.2 mm error on each one adds up. Length is commonly held to ±0.1 mm on this class of part, and tighter is possible but should be specified only where the stack needs it.

Thread depth on a female-female part is the second problem. Two blind tapped holes from either end must leave a wall between them, or the shop drills through and the part becomes a through threaded spacer. Say on the drawing whether a through thread is acceptable. It usually is, and it is cheaper.

Plating on threads changes the fit. A bright nickel deposit of 5 to 10 microns tightens a 6H tapped hole noticeably. Ask for threads to be gauged after plating, or specify the pre-plate tolerance so the finished thread lands in class. These are values commonly held, not a promise from any single shop.

Standards and compliance to name

Threads follow ISO 965 for metric and ASME B1.1 for unified. Plating can be called out to ASTM B689 for electroplated nickel or ASTM B733 for electroless nickel. It can also be given simply as a thickness and a finish.

For electronics sold in the EU, leaded brass is covered by RoHS exemption 6(c), which allows up to 4 percent lead in copper alloys. Its expiry was set for 30 June 2027 and a renewal request was submitted in December 2025. Standoffs are a low risk item because they are not wetted and not handled by the end user, but a product compliance file should note the exemption. This is not legal advice.

What to put on the RFQ

The lines that make a quote for this part comparable across shops.

  • 1Form: male-female, female-female or male-male
  • 2Thread size and system, metric or unified, and the class if it matters
  • 3Across flats or outside diameter, and overall length with its tolerance
  • 4Whether a through thread is acceptable on a female-female part
  • 5Plating: bright nickel, electroless nickel, tin or none, and the thickness
  • 6Quantity per order and annual volume

Grades for this part

AlloyLead %Mach.DZRWhy for this part
C360 free-cutting brassC36000 · CuZn36Pb3 / CW603N2.5 to 3.7100PoorThe benchmark every other metal is rated against for machinability, and the default for turned brass parts.

Published typical values for the alloy. Not a promise from a shop.

Should standoffs be brass or steel?

Brass for almost any indoor electronics assembly. It machines faster, so the part is cheaper in the quantities standoffs are bought in, it does not rust, it is not magnetic and it conducts a ground path. Steel or stainless is worth the cost only where the standoff carries structural load or lives in a corrosive environment. This site supplies brass parts only, so a stainless standoff RFQ would need another source.

Do brass standoffs need plating?

Not always. Bare brass tarnishes to a dull brown indoors within months, but the tarnish does not affect function or conductivity in a meaningful way. Nickel plating is specified where the standoff is visible, where the assembly will be handled or where a customer specification calls for it. Tin is used where solderability matters. Plating adds a batch cost, so on small runs ask for the price both ways.

Are brass standoffs RoHS compliant?

Leaded brass such as C360 is permitted in EU electronics under RoHS exemption 6(c), which allows up to 4 percent lead in copper alloys. The exemption has an expiry set for 30 June 2027 with a renewal request submitted in December 2025. Until a decision is published, a standoff in C360 is used under that exemption, and a compliance file should say so. This is not legal advice.