Part types / Brass threaded inserts
Brass Threaded Inserts for Plastic and Wood
Brass threaded inserts are short knurled bushes with an internal thread, set into plastic or wood so a steel screw can be driven repeatedly without stripping the parent material. Most are turned from C360 free-cutting brass on Swiss lathes in M2 to M12 sizes. Lead-free C69300 is used where a consumer or water contact product requires it.
- Usual gradesC360 free-cutting brass, C69300 silicon brass
- Machine classSwiss lathe, bar fed, most sizes under 16 mm outside diameter
- Typical sizesM2 to M12 thread, 3 to 16 mm outside diameter, 3 to 20 mm long
- Commonly heldOutside diameter over the knurl commonly held to ±0.05 mm, thread to 6H, length to ±0.1 mm
- FinishesAs machined, tumble deburred, clear passivate or thin nickel where the part is visible
- Standards to nameISO 965 and ASME B1.1 thread tolerance classes, RoHS Directive 2011/65/EU exemption 6(c) for electronics, REACH SVHC declaration for lead where a customer asks for one. See the standards index.
- IndustriesConsumer electronics, Injection moulded enclosures, Furniture and joinery, Automotive interior trim, Medical device housings
What a threaded insert does and where it goes
A threaded insert gives a soft material a hard thread. Plastic and wood cannot hold a machine screw through repeated assembly cycles, so a brass bush with a female thread inside and a knurled or grooved outside is set into the parent part. The screw then engages brass, and the plastic or wood only has to hold the insert.
The setting method decides the outside geometry. Heat staked inserts are pressed into an undersized hole with a heated tip and the plastic flows into the knurl as it cools. Ultrasonic inserts are set the same way with an ultrasonic horn instead of heat. Press in inserts rely on interference and a coarse knurl. Moulded in inserts are placed on pins in the mould and the plastic is shot around them, so they carry the deepest undercuts. Inserts for wood usually have a coarse external thread or a hexagonal drive rather than a knurl.
Common homes are electronics enclosures, appliance housings, automotive interior trim, furniture, sports equipment and any moulded part that is opened for service.
Why brass, and which grade
Brass is the default for three reasons. It machines faster than any competing metal, so the price stays low on a part that is bought by the thousand. It does not rust in a damp enclosure. And a steel screw does not gall against it, which stainless inserts sometimes do against stainless screws.
C360 free-cutting brass is the usual grade. Rated 100 for machinability, the figure every other alloy is measured against, it lets a Swiss lathe knurl, drill, tap and part off in one short cycle. Its nominal lead content is 2.5 to 3.7 percent, a published typical value for the alloy.
Lead-free C69300 silicon brass is chosen when the product is a consumer item sold in a market that restricts lead, when the insert is wetted or when a customer declares the whole assembly lead-free. It is rated 80 for machinability and work hardens, so the shop that quotes it should have run it before. Expect a higher piece price and a longer lead time on bar.
How inserts are made and what drives the price
Nearly every insert is turned from bar on a Swiss lathe. The sequence is knurl, drill, tap or thread mill, cut any undercut or flange, then part off. Sizes under about 6 mm outside diameter are the natural territory of a Swiss lathe with a guide bushing, and larger sizes move to a bar fed turret lathe.
Cycle time is the price. A plain straight knurl insert in M3 might cycle in under ten seconds. Every added feature adds seconds: a second knurl band, a helical or diamond pattern, an undercut for a moulded in part, a flange, a blind thread instead of a through thread. Forming the thread with a roll tap is faster than cutting it and leaves a stronger thread, and many shops prefer it in brass.
Volume matters more than on almost any other part type, because the setup is the same for one thousand and for one hundred thousand. Ask for prices at two or three quantity breaks.
The features that go wrong
Burrs at the thread mouth are the most common reject. A rolled or cut thread leaves a wire edge where it meets the chamfer, and a burr there either stops the screw starting or breaks off inside the assembly. Ask for a chamfer on both ends and a deburred thread.
Knurl fill matters for holding power. A knurl that is too shallow pulls out under screw torque, and one that is too coarse cracks a thin plastic boss. The knurl pitch and depth should match the hole size and the setting method, and the moulder or the plastics supplier often has a recommendation.
Thread class is the other point of dispute. Most inserts are tapped to 6H or 2B and that is enough for a machine screw. Specifying a tighter class than the screw needs raises the reject rate for no gain. Tolerances quoted here are values commonly held on this class of part, never a promise from any single shop.
Standards and compliance to name
No standard governs threaded insert geometry as a whole, and most are made to a supplier catalogue or a customer drawing. Threads follow ISO 965 for metric and ASME B1.1 for unified sizes.
Electronic products sold in the EU under RoHS rely on exemption 6(c) to allow up to 4 percent lead in copper alloys. That exemption carries an expiry set for 30 June 2027, with a renewal request submitted in December 2025. If the product will still be sold after that date, decide now whether the insert should be lead-free. REACH may also require an SVHC declaration for lead. This is not legal advice.
What to put on the RFQ
The lines that make a quote for this part comparable across shops.
- 1Setting method: heat staked, ultrasonic, press in, moulded in or for wood
- 2Thread size and class, and whether it is through or blind
- 3Outside diameter over the knurl, length and any flange
- 4Parent material and the hole or boss size it will go into
- 5Alloy: C360 unless lead-free is required, then C69300
- 6Chamfer and deburring on both thread ends
- 7Annual volume and the first order quantity
Grades for this part
| Alloy | Lead % | Mach. | DZR | Why for this part |
|---|---|---|---|---|
| C360 free-cutting brassC36000 · CuZn36Pb3 / CW603N | 2.5 to 3.7 | 100 | Poor | The benchmark every other metal is rated against for machinability, and the default for turned brass parts. |
| C69300 silicon brassC69300 · CuZn21Si3P / CW724R | under 0.09 | 80 | High | The usual lead-free answer for potable water, roughly twice as strong as C360 and highly dezincification resistant. |
Published typical values for the alloy. Not a promise from a shop.
Questions buyers ask about brass threaded inserts
Further reading: Swiss Turning Brass Parts and When It Is the Cheaper Route, RoHS Exemption 6(c) and What Happens to Leaded Brass in 2027, The Burr Inside the Bore Nobody Can See.
Can a threaded insert be made in lead-free brass?
Yes. C69300 silicon brass is the usual lead-free choice, with under 0.09 percent nominal lead against the 0.25 percent NSF/ANSI 372 line. It is rated 80 for machinability so the cycle is a little longer, and it work hardens, so ask whether the shop has shipped it before. Bar stock costs more and is held in fewer sizes.
Should the insert be heat staked or moulded in?
Moulded in inserts hold most securely because plastic flows fully into the undercut, but they slow the moulding cycle and a misplaced insert scraps the shot. Heat staked and ultrasonic inserts are set after moulding, which keeps the mould simple and lets you add inserts only to the parts that need them. Most electronics enclosures use heat staking. Ask the moulder which they prefer before the drawing is fixed.
What thread class should I specify?
For a machine screw in an insert, 6H metric or 2B unified is the normal class and it is what a rolled or cut tap produces without extra effort. Tighter classes such as 5H or 3B raise the reject rate and the price and add nothing unless the mating screw is also made to that class. State the class on the drawing so every shop quotes the same thing.
Does RoHS affect a brass insert in an electronic product?
It can. Leaded brass is allowed in EU electronics through RoHS exemption 6(c), which permits up to 4 percent lead in copper alloys. That exemption has an expiry set for 30 June 2027 and a renewal request was submitted in December 2025. If your product ships after that date and the exemption is not renewed, the insert would need a lead-free grade. This is not legal advice.
Have a drawing for this kind of part?
Send it. We place the work with a partner shop that has shipped this class of brass part and reply within 24 business hours with one itemised quote. Brass only.