Guides / Cost
There Is No Brass MOQ, but Setup Is a Fixed Cost
Published September 27, 2026. Reviewed for the facts in the corrections log.
There is no fixed minimum order quantity for machined brass parts. Shops quote one piece or ten thousand, but setup on a bar-fed lathe is a fixed cost, so price per piece falls steeply between 1 and 1,000 pieces and flattens after that. Prototypes are priced on programming and setup, production on cycle time and metal.
Ask a brass shop for its minimum order quantity and the honest answer is one. Nothing stops a shop from making a single brass part, and most will. What stops it from being cheap is that setting up a bar-fed lathe costs the same hours whether one part or ten thousand comes off it afterwards.
That fixed cost is the whole story of brass MOQ. It is why price per piece falls so steeply between 1 and 1,000 pieces, why the first ten pieces of a part can cost as much as the next hundred and why a shop that quotes happily at 500 sometimes declines at 5.
Where the MOQ feeling comes from
Setup on a bar-fed lathe means writing or loading the program, setting the tools and their offsets, changing the collet and guide bushing to the bar size, loading bar, proving the first article and measuring it. On a Swiss lathe that is often two to four hours for a new part. On a conventional CNC lathe with a chuck it is nearer one to two. Those hours are the same at any quantity.
Shops encode that as a minimum charge or a minimum lot, and that is the MOQ a buyer runs into. It is not a policy about quantity. It is a floor under the setup. The economics are the ordinary economies of scale of any fixed cost spread over a run, and on a brass part the fixed cost is unusually large next to the per-piece cost, because the cutting itself is so quick.
The shape of the curve
Put numbers on it. Take a small turned brass fitting with a 90 second cycle and a three hour setup. The setup is worth 120 cycles of machine time, so at one piece almost the entire machine cost is setup, and at 5,000 pieces the setup is noise.
| Quantity | Setup share of machine cost | Machine cost per piece, relative to 5,000 |
|---|---|---|
| 1 | 99 percent | about 120 times |
| 10 | 92 percent | about 13 times |
| 50 | 71 percent | about 3.3 times |
| 100 | 55 percent | about 2.1 times |
| 500 | 19 percent | about 1.2 times |
| 1,000 | 11 percent | about 1.1 times |
| 5,000 | 2 percent | 1 |
Illustrative model with setup equal to 120 cycles of machine time. Material, finishing and inspection are excluded. The real ratios depend on the part.
Two things the table hides. Material is a constant per piece, so on a heavy part the curve flattens sooner because the metal swamps the setup earlier. And below about 50 pieces the part often runs on a different machine altogether, which is the next section. The full list of what sits inside a brass quote is in what drives the cost of a machined brass fitting.
The prototype route
For one to ten pieces a shop rarely loads a bar feeder. The part runs on a CNC lathe with a chuck, or on a mill-turn machine, from a short length of bar held by hand between parts. A single simple piece sometimes runs on a manual lathe with no program at all.
On that route the cutting is minutes and the quote is programming, setup and a first article inspection. Expect it to look like a fixed charge plus a small per-piece amount, and ask for it split that way, because the split tells you what the next five pieces would cost.
The trade is that the prototype was not made on the production process. A part that will run on a Swiss lathe in volume was proved on a chuck lathe, and threads, cross hole burrs and surface finish can all differ between the two. If the prototype exists to prove function, that does not matter. If it exists to prove the process, it does, and the RFQ should say which.
How a Swiss shop reads 50 against 5,000
At 50 pieces the setup is 71 percent of the machine cost in the model above. A Swiss shop will quote it, often with a minimum lot charge, and some will pass, because the same hours spent setting up a 5,000 piece job earn more. At 5,000 pieces the setup is 2 percent and the quote is cycle time and metal, so the shop starts thinking about running the job unattended and buying bar in bulk.
The band between 500 and 5,000 is where the Swiss advantage is clear, as Swiss turning brass parts sets out, and above 5,000 pieces of a bulky part the conversation moves to forging a near net shape and machining only the sealing features. The quantity band on the RFQ is what puts the part in front of the right kind of shop.
Need a quote for this part? Get a quote for your brass parts
Why a shop declines a low quantity in lead-free brass
This is the one that surprises buyers, and it is about bar, not machining.
C360 is held in every common size and sold by the cut length. Ten pieces need ten pieces of bar. Lead-free grades such as C69300 silicon brass are produced as rod, according to the Copper Development Association alloy listings, but they are stocked in fewer sizes and often sold by the full length or the bundle, sometimes with a mill minimum on an odd diameter. Ten pieces then carry the cost of a full bar the shop may never use again, and the material line on the quote is larger than the machining line. Declining is quicker than explaining it.
Three ways round it. Pay for the full bar and own the remnant, which is the honest answer when the part will repeat and the remnant becomes the first production lot. Combine the prototype and the first production run on one bar purchase. Or prototype in C360 for form and fit only, and never for a compliance test or a threading trial, because a lead-free grade machines and threads differently, as leaded and lead-free brass compared explains. NSF/ANSI 372 sets a 0.25 percent weighted average lead limit on wetted surfaces, so a C360 prototype cannot stand in for the production alloy anywhere that limit applies. That is a description of the standard, not legal advice.
Writing an RFQ for a prototype that will repeat
Say so. A shop that knows the part comes back quotes the setup differently, keeps the program and tooling standing and may propose making the prototype on the production route so the first article proves the process. A shop that thinks it is quoting ten pieces and done quotes ten pieces and done.
Ask for two prices on one RFQ: the prototype quantity now and the production band later. Give the timing and say whether the design is frozen, because a shop invests in a frozen design and hedges on a moving one. Accept that a prototype made on the production route costs more than one made on a chuck lathe, and decide whether proving the process is worth it.
The four quantity bands on this site
The RFQ form asks for a quantity band rather than an exact number, because the band is what a shop needs to decide in ten seconds whether the part is for them.
1 to 50. Prototype and pre-production. Shops read this as chuck work or a short bar run, and the shops that take it are the ones set up for it.
51 to 500. First production. A fixed headstock bar lathe, or a Swiss lathe if the part is slender or carries features on several faces.
501 to 5,000. Swiss territory. Setup is amortised, cycle time is what gets quoted.
5,000 plus. Swiss running unattended, or forge and machine if the part is bulky.
If the prototype is going to repeat, pick the band for the quantity you want now and put the production band in the description. Partner shops see both on the work request and quote both.
Quantity now: 10 prototype pieces.
Production: 501 to 5,000 per year from next
quarter, design frozen after prototype approval.
Please quote both. Prototype on the production
route if practical, so the first article proves
the process.
Six lines, and the quote that comes back is the one you can actually plan against.
Have a prototype that is going to repeat? Send the drawing with the quantity you need now, put the production band in the description and we will quote both and place the work with a partner shop that can run both. We reply within 24 business hours.
Frequently asked questions
Is there a minimum order quantity for machined brass parts?
Not a fixed one. A shop can make a single brass part, and many will. What you meet instead is a minimum charge, because programming, tooling and setup cost the same hours whether one piece or a thousand follows. That charge is spread across the run, so price per piece falls steeply up to about 1,000 pieces and then flattens toward cycle time plus metal.
How much does a brass prototype cost compared with production?
Per piece, many times more, and the ratio is set by the part. On a small turned fitting where setup is worth a hundred or so cycles of machine time, a single piece can cost a hundred times the per-piece price at 5,000, ten pieces around a tenth of that and fifty pieces three or four times the volume price. Ask the shop to show the setup as a separate line so the arithmetic is visible.
Why did a shop decline my ten-piece lead-free order?
Almost always the bar. C360 is held in every size and sold by the cut length, so ten pieces cost ten pieces of bar. Lead-free grades such as C69300 are stocked in fewer sizes and often sold by the full length or the bundle, sometimes with a mill minimum on an odd diameter. Ten pieces then carry the cost of a bar the shop may never use again, and declining is cheaper than explaining that.
Which quantity band should I pick on the RFQ form if I need prototypes first?
Pick the band for the quantity you want made now, usually 1 to 50, and put the production band and its timing in the description. Partner shops see the quantity on the work request, so the band decides which shops look at it. A prototype that says it will repeat at 501 to 5,000 pieces a year reaches the shops with bar-fed lathes, and they quote both prices together.
Alloys in this guide
| Alloy | Lead % | Mach. | DZR |
|---|---|---|---|
| C69300 silicon brassC69300 ยท CuZn21Si3P / CW724R | under 0.09 | 80 | High |
Published typical values for the alloy. Machinability against C360 at 100. Not a promise from a shop.
Sources
- Wikipedia, Economies of scale en.wikipedia.org
- Copper Development Association, product forms by alloy copper.org
Need a quote for this part?
Send the drawing. We read it, send one itemised quote for the finished parts within 24 business hours and place the work with a partner shop that turns brass. Brass only.