Skip to content
Brass CNC Parts

Guides / Materials

When a Machined Part Should Be Brass, and When Aluminum

Published September 27, 2026. Reviewed for the facts in the corrections log.

Brass wins per minute of machine time and on threads, plating, soldering and contact surfaces. Aluminum costs a fraction of brass per kilo and weighs a third as much, so the crossover is part mass. Small threaded fittings and connectors favor brass. Large housings, heat sinks and anything weight critical favor aluminum.

Brass and aluminum are the two metals a buyer reaches for when a part has to be machined quickly and cheaply. Per minute of machine time, brass usually wins. Per kilogram of bar, aluminum wins by a wide margin. Which one wins on the finished part depends mostly on how much metal is in it.

A small threaded fitting is nearly all machine time, so it is cheaper in brass. A large housing is nearly all metal, so it is cheaper in aluminum. The rest of this article is about where that line sits, and about the properties that override it: threads, contact surfaces, plating, weight and heat.

Two machinability charts that do not share a ruler

This site rates every alloy against free-cutting brass C360 at 100, the scale used across the alloy comparison and the machining guide. Nothing on that chart is rated above 100.

Aluminum is usually rated on a different chart, one that puts free-cutting steel at 100. On that chart a free-machining aluminum such as 2011 or 6262 scores well above 100, and some published tables push aluminum alloys to 300 and beyond. Read side by side, that makes aluminum look three times easier to cut than brass. It is not. The two charts use different reference metals and weigh tool life, chip form and surface finish differently, so the numbers cannot be compared by arithmetic.

What happens on the machine is more useful than either number. C360 runs dry, breaks its own chip and comes off the tool bright. Free-machining aluminum grades chip reasonably well. General purpose 6061 does not. It is gummy, it welds to the cutting edge, it throws long chips and it wants flood coolant. On a bar-fed lathe that has to run unattended, chip control decides whether the machine runs overnight. That is why brass usually wins per minute of machine time on small turned parts, even though aluminum spindle speeds are high.

The bar price, and why mass decides

Brass is roughly 60 percent copper, so the bar price follows the copper market and has historically sat several times above aluminum bar per kilogram. See what the copper market does to brass quotes.

Density widens the gap. C360 is 8.49 g/cm3 and 6061 is 2.70 g/cm3, so the same part weighs about three times as much in brass. Per part, the material line in brass is several times the per kilo gap again.

On a 10 gram fitting that hardly matters. Setup, cycle time and the thread gauge check dominate the quote, and brass wins on all three. On a 2 kilogram housing the metal is most of the quote and aluminum wins by a distance. The crossover is not a fixed number of grams, because it moves with the copper price and with how much of the bar ends up as chips. A working rule: if the finished brass part would weigh more than a few hundred grams and nothing on the drawing needs brass, ask for an aluminum quote as well.

The two alloys side by side

Property C360 free-cutting brass 6061-T6 aluminum
Density 8.49 g/cm3 2.70 g/cm3
Tensile strength 340 to 470 MPa about 310 MPa
Electrical conductivity about 26 percent IACS about 40 percent IACS
Thermal conductivity about 115 W/m K about 167 W/m K
Machinability 100 on the brass scale rated on the steel scale, not comparable
Magnetic No No
Surface treatment Plates directly, polishes, lacquers Anodizes, plating needs a zincate step first
Threads Seal and survive repeated assembly Strip and gall, inserts are common

Published typical values for the alloy, from the Copper Development Association for C360 and from published 6061 data for the aluminum. They describe the material, not a promise from any shop.

Conductivity: the number that surprises people

Aluminum conducts electricity and heat better than C360 by volume, and far better by weight. That is why bus bars, heat sinks and enclosures that have to shed heat are aluminum rather than brass.

Brass wins on contact surfaces, which is a different question. Aluminum grows an oxide film within seconds of meeting air. The film raises contact resistance, and aluminum creeps under a clamped terminal, so aluminum connections need specific plating, hardware and torque to stay reliable. Brass makes contact, solders and plates without any of that. Connectors, pins, terminals and RF bodies stay brass. Anything whose job is to move heat away or carry bulk current is aluminum.

Threads

Aluminum threads strip. A tapped hole in aluminum that will be assembled and taken apart more than a few times usually gets a helical insert, which is another part and another operation. Aluminum also galls against stainless and against itself. A tapered pipe thread driven into a thin aluminum wall can split it.

Brass threads seal, survive repeated makeup and run against steel without galling. That is why pipe fittings, hose barbs, pneumatic fittings and valve bodies are brass, and why a part with a sealing thread on it should stay brass unless something else forces the change. See NPT and BSP threads on brass fittings for the callouts.

Need a quote for this part? Get a quote for your brass parts

Corrosion

Aluminum protects itself with its oxide film in dry and neutral environments and pits in chlorides. In a wet assembly coupled to brass, copper or steel it is the anode, so it corrodes first and fastest. Keep aluminum out of mixed metal wet assemblies unless it is isolated.

Brass is the default in water, gas and air. Ordinary yellow brass dezincifies in hot or aggressive water, which is what the DZR and silicon brass grades exist to fix. See dezincification resistant brass. Neither metal is a shortcut on drinking water. Brass has the lead question, and aluminum is not a material the plumbing codes are written around.

Finish: anodizing against plating

Anodizing converts the surface of aluminum into a hard, colored, electrically insulating oxide. It cannot be applied to brass. If the drawing says anodize, the part is aluminum.

Brass plates directly with nickel, chrome, tin, silver or gold, polishes to a mirror and lacquers to hold the color. Aluminum can be plated, but it needs a zincate pre-treatment and the adhesion is less forgiving. If the drawing calls for a plated or polished surface, brass is the easier route. See surface finishes and plating on brass parts.

Weight and magnetism

Both metals are non-magnetic. Machining does not change that for either, so a part that lives near a sensor or a compass can be made from either without a note on the drawing.

Weight belongs to aluminum without argument. Anything carried, flown or moved by a small motor benefits from a part that weighs a third as much.

Where aluminum wins

  • Weight critical parts. Drones, handheld equipment, anything on a vehicle.
  • Heat sinks and thermal paths. Higher thermal conductivity at a third of the mass.
  • Large housings and enclosures. The metal dominates the price and aluminum is cheap by volume.
  • Structural brackets. 7075-T6 has a strength to weight ratio that no brass approaches.
  • Anodized parts. There is no brass equivalent.

If the part is one of these, aluminum is right and the machining argument does not reopen it.

The question that decides it

  1. Does the part have a sealing thread, an electrical contact surface or a solder joint? Brass.
  2. Is it plated, polished or lacquered? Brass, almost always.
  3. Does it carry heat away, or does weight matter? Aluminum.
  4. Is it large? Weigh the finished part. Over a few hundred grams with no property reason for brass, aluminum wins on material.
  5. Otherwise: brass, on cycle time and chip control alone.

What to put on the RFQ

Write the alloy, not the metal. C360 or 6061-T6, not “brass” or “aluminum”. Give the finished part mass, or let the shop calculate it from the model, because mass is the number that decides the crossover. Call out threads in full, including whether they seal, and put the finish on the drawing rather than in an email. A shop quoting a plated part machines it differently from a bare one.

This site only supplies brass parts. If the checklist above has taken your part to aluminum, we do not quote it and you should send it to an aluminum shop directly. If the part stays brass, send the drawing with the mass and the finish, and we quote the finished parts and place the work with one of the partner shops that turn brass every day.

Frequently asked questions

Is brass or aluminum cheaper to machine?

Per minute of machine time, brass. C360 runs dry, breaks its own chip and comes off the tool with a bright finish, so a bar-fed lathe can run it unattended. Per kilogram of bar, aluminum, by several times, and the same part weighs about three times as much in brass. On a small threaded part the machine time decides it and brass is cheaper. On a heavy part the metal decides it and aluminum is cheaper.

Why do machinability charts show aluminum above brass?

Because most aluminum charts rate alloys against free-cutting steel at 100, while brass is rated against free-cutting brass C360 at 100. A free-machining aluminum such as 2011 scores well above 100 on the steel chart, which makes it look easier to cut than brass. The two charts use different reference metals and weigh tool life, chip form and finish differently, so the numbers cannot be compared by arithmetic.

Does aluminum conduct better than brass?

By volume, yes. 6061-T6 sits around 40 percent IACS against about 26 percent for C360, and it conducts heat better too. By weight the gap is wider still, which is why heat sinks and bus bars are aluminum. Brass wins on contact surfaces, because aluminum grows an insulating oxide film within seconds and creeps under a clamped terminal, so connectors, pins and terminals stay brass.

Can a brass part be anodized?

No. Anodizing grows a hard oxide layer out of the aluminum itself, and brass has no equivalent process. A drawing that calls for anodize is an aluminum drawing. Brass takes nickel, chrome, tin, silver or gold plating directly, polishes to a mirror and lacquers to hold the color. Aluminum can be plated, but it needs a zincate pre-treatment first and the adhesion is less forgiving than on brass.

Alloys in this guide

AlloyLead %Mach.DZR
C360 free-cutting brassC36000 · CuZn36Pb3 / CW603N2.5 to 3.7100Poor

Published typical values for the alloy. Machinability against C360 at 100. Not a promise from a shop.

Sources

  1. Copper Development Association, C36000 alloy data alloys.copper.org
  2. Wikipedia, 6061 aluminium alloy en.wikipedia.org

Need a quote for this part?

Send the drawing. We read it, send one itemised quote for the finished parts within 24 business hours and place the work with a partner shop that turns brass. Brass only.

Get a quote for your brass parts

Keep reading

Get a quote