Skip to content
Brass CNC Parts

Guides / Materials

Machined Brass or Zinc Die Casting: Where Each One Belongs

Published September 27, 2026. Reviewed for the facts in the corrections log.

Machined brass wins on strength at temperature, creep, thread quality, corrosion in water and dimensional accuracy, with no tooling to pay for. Zinc die casting in Zamak 3 or 5 wins on per part cost once a die is paid off, usually at tens of thousands of decorative parts a year. Fittings that seal or carry pressure stay brass.

A zinc die casting and a machined brass part can look identical on a shelf, especially once both are plated. They behave differently in service and they are priced in opposite ways. Brass turned from bar has no tooling and a real per part cost. A zinc die casting has a die to pay for and then a very low per part cost.

So the decision is partly arithmetic, volume against tooling, and partly engineering. A part that seals, carries pressure, runs warm or holds a thread under load for years is a brass part. A decorative handle made in the hundreds of thousands is a zinc part. Most fittings and hardware sit between those two, and that gap is what this article walks through.

What zinc die casting is

The alloys are Zamak 3 and Zamak 5, both about 96 percent zinc with 4 percent aluminium and a trace of magnesium. Zamak 5 adds about 1 percent copper, which makes it a little stronger, harder and more creep resistant. Both melt around 385 degrees Celsius, low enough for hot chamber die casting, where molten zinc is injected into a hardened steel die under pressure and the part is ejected seconds later. See the Zamak family for the full range.

The result is a near net shape with thin walls, fine detail and cast in holes and logos. Very little machining is left to do.

Machined brass is the opposite process. Take a bar of C360 free-cutting brass, or a hot forged C377 blank, and cut away everything that is not the part. No die, no minimum run, tolerances to a hundredth of a millimetre and a part that is wrought metal all the way through.

Tooling against per part cost

A die casting die is a hardened steel tool with cavities, slides, ejectors and cooling channels. It is a serious one off charge and it takes weeks to make. Once it is cut, the part cannot change without cutting the tool again. After that, each part costs seconds of machine time and a few grams of a cheap metal.

Machined brass has no tooling at all. Each part costs its bar plus its minutes on the lathe, and that cost never falls much below what the first hundred pieces cost. See what actually drives the cost of a brass part.

Those two curves cross. Where they cross depends on the die cost, the part size and how much machining the casting still needs, but for small decorative hardware the crossover often sits in the tens of thousands of pieces a year. Below a few thousand pieces, brass wins outright. Above a hundred thousand, zinc is far cheaper per piece. A design that may still change stays brass longer, because the die locks it.

Strength, creep and temperature

Property C360 free-cutting brass Zamak 3 Zamak 5
Density 8.49 g/cm3 about 6.6 g/cm3 about 6.7 g/cm3
Tensile strength 340 to 470 MPa about 280 MPa about 330 MPa
Lead, nominal 2.5 to 3.7 percent under 0.005 percent under 0.005 percent
Melting range about 885 to 900 C about 380 to 390 C about 380 to 390 C
Creep at room temperature None in practice Yes, under sustained load Yes, less than Zamak 3
Strength at 100 C Retained Falls sharply above about 90 C Falls sharply above about 90 C
Tooling None Die required Die required

Published typical values for the alloys, C360 from the Copper Development Association. They describe the material, not a promise from any shop or foundry.

The tensile numbers are the trap. Zamak 5 looks close to C360 on paper. The difference is what happens after the test. Zinc alloys creep at room temperature under sustained load, so a clamped or threaded zinc part relaxes over months and a joint that was tight loosens. Strength falls quickly above about 90 degrees Celsius. Impact strength drops as the casting ages, and the part shrinks slightly over years as the alloy structure settles.

Brass does none of that. C360 holds its strength across the whole temperature range a fitting sees, does not creep at room temperature and does not change dimension on the shelf.

Corrosion

Zinc is the metal used to protect steel sacrificially, and it does the same job unasked inside a fitting. In soft or slightly acidic water, outdoors or in a damp cabinet, a zinc die casting corrodes to a white powder. In a wet assembly coupled to brass, copper or steel it is the anode, so it goes first. Castings poured from scrap with lead, tin or cadmium above the specification limits also suffer intergranular corrosion, a swelling and cracking failure that starts from inside the part.

Brass has one water problem, dezincification, and it is slow, understood and fixable by choosing a DZR or silicon brass grade. See dezincification resistant brass. A wetted fitting is a brass fitting.

Plating adhesion

Both metals plate, but not on the same terms.

Zinc die castings are plated copper, then nickel, then chrome, and the copper strike is not optional. Surface porosity in the casting traps plating solution and blisters later, so the casting has to be sound and the pre-treatment careful. On zinc the plating is the corrosion protection. Where it is chipped or worn through, corrosion starts underneath and lifts the plating around it.

Brass plates with less preparation and forgives more. If the plating on a brass part is scratched, the metal underneath is still brass. See surface finishes and plating on brass parts.

Need a quote for this part? Get a quote for your brass parts

Dimensional accuracy and threads

A new die holds about 0.05 to 0.1 mm on small features, plus draft angles, a parting line and ejector marks, and the tolerance opens as the die wears. A machined brass part holds 0.01 mm routinely on turned features, with no draft and no parting line.

Threads are where the difference bites. External threads can be cast in zinc, but they carry draft, a parting line across the flanks and a rounded crest. Internal threads are normally tapped after casting. A tapered pipe thread that has to seal, NPT or BSPT, needs to be cut and gauged, and zinc under sustained thread load creeps. Cast threads are for decorative assembly. Sealing threads are cut in brass. See NPT and BSP threads on brass fittings.

The lead question is not the reason to choose zinc

Zamak is specified with a lead limit of 0.005 percent, so the NSF/ANSI 372 arithmetic that dominates brass alloy selection, the 0.25 percent weighted average lead limit on wetted surfaces, is not a constraint for zinc. That does not make zinc a drinking water material. It corrodes in water, and NSF/ANSI 61 still applies to whatever a wetted part leaches. A potable water fitting is lead-free brass, not zinc. See NSF/ANSI 61 and 372 for brass fittings. This is a description of the standards, not legal advice.

Where zinc wins

  • Decorative hardware in very high volume. Handles, knobs, buckles, badges, trim, zipper pulls.
  • Thin walls and complex shapes. Cast in features that would need several machining setups.
  • Lowest per part cost once the die is paid for. Indoor, dry, room temperature, no sustained load.

Where brass wins

  • Anything that seals or holds pressure.
  • Threads that are made up more than once, or that stay under load.
  • Hot, wet or outdoor service.
  • Runs under a few thousand pieces, or a design that may still change.
  • Any part where a scratch through the plating must not matter.

The question that decides it

  1. Does it seal, carry pressure or hold a thread under load? Brass.
  2. Does it run above about 80 degrees Celsius, sit in water or live outdoors? Brass.
  3. Is the annual volume in the tens of thousands, the design frozen and the part decorative? Zinc.
  4. Otherwise: brass, with no die to pay for.

What to put on the RFQ

The annual quantity and how many years it repeats, because that is the whole tooling argument. The service environment, wet or dry, hot or cold, indoors or out. Whether each thread seals or only holds. The finish, plated or bare. With those four lines a shop can tell you which side of the crossover your part sits on.

This site only supplies brass parts. If the checklist has taken your part to a zinc die casting, we do not quote it and you should go to a die caster directly. If the part stays brass, send the drawing with the yearly quantity and the environment, and we quote the finished parts and place the work with one of the partner shops that turn brass.

Frequently asked questions

Is zinc die cast stronger than brass?

On a datasheet the two look close. Zamak 5 is rated around 330 MPa tensile as cast and C360 brass at 340 to 470 MPa. The difference is what happens after the test. Zinc alloys creep at room temperature under sustained load, lose strength quickly above about 90 degrees Celsius and lose impact strength as they age. Brass holds its properties across the whole range a fitting sees, which is why a threaded or pressurised part stays brass.

Why do zinc die cast fittings fail in water?

Zinc is the metal used to protect steel sacrificially, and it does the same thing unasked inside a fitting. In soft or slightly acidic water it corrodes to a white powder, and in a wet assembly next to brass, copper or steel it is the anode and goes first. Castings that carry lead, tin or cadmium above the specification limits also suffer intergranular corrosion, which swells and cracks the part from inside. Brass has its own water problem, dezincification, but a DZR or silicon grade fixes it.

Can a zinc die casting have a sealing thread?

Not a reliable one as cast. External threads can be cast, but they carry draft, a parting line across the flanks and a rounded crest, and internal threads are normally tapped after casting anyway. A tapered pipe thread that has to seal, NPT or BSPT, needs to be cut and gauged, and zinc under sustained thread load creeps. Fittings with sealing threads are machined brass for that reason.

At what volume does zinc die casting become cheaper than machined brass?

There is no single number, because it depends on the die cost, the part size and how much machining the zinc part still needs. As a planning figure, small decorative hardware often crosses over in the tens of thousands of pieces a year with a frozen design. Below a few thousand pieces, machined brass wins outright because it has no tooling to repay. The die also locks the design, so a part that may change stays brass longer.

Alloys in this guide

AlloyLead %Mach.DZR
C360 free-cutting brassC36000 ยท CuZn36Pb3 / CW603N2.5 to 3.7100Poor

Published typical values for the alloy. Machinability against C360 at 100. Not a promise from a shop.

Sources

  1. Wikipedia, Zamak zinc alloys en.wikipedia.org
  2. Copper Development Association, C36000 alloy data alloys.copper.org

Need a quote for this part?

Send the drawing. We read it, send one itemised quote for the finished parts within 24 business hours and place the work with a partner shop that turns brass. Brass only.

Get a quote for your brass parts

Keep reading