Skip to content
Brass CNC Parts

Guides / Materials

C360 or C385: Two Leaded Brasses, Two Different Jobs

Published September 27, 2026. Reviewed for the facts in the corrections log.

C360 is free-cutting brass bar, machinability 100, the default for turned parts. C385 is architectural bronze, a leaded brass despite the name, machinability 90, supplied as extruded shapes and chosen where the part is seen, polished or plated. Both carry about 3 percent lead, so neither is a potable water alloy. Pick by the form the part starts from.

C385 is called architectural bronze and it is not a bronze. It is a leaded brass, CuZn39Pb3, a close cousin of C360 with a little more zinc and a little less copper. The name is historical, so read the UNS number rather than the word.

The difference that matters is the form. C360 arrives as round, hex and square bar for turning. C385 arrives as extruded angles, channels, tees and custom profiles for hardware that is cut, drilled, milled and polished. Choose the alloy by the shape the part starts from, and most of the rest follows.

The two alloys side by side

C360 free-cutting brass C385 architectural bronze
UNS and EN C36000, CuZn36Pb3, CW603N C38500, CuZn39Pb3, CW614N
Copper 60 to 63 percent 55 to 59 percent
Lead 2.5 to 3.7 percent 2.5 to 3.5 percent
Zinc remainder, about 35 percent remainder, about 39 percent
Machinability, C360 = 100 100 90
Tensile strength 340 to 470 MPa 380 to 480 MPa
Hardness 60 to 80 HRB 65 to 85 HRB
Density 8.49 g/cm3 8.47 g/cm3
Dezincification resistance Poor Poor
Usual forms Round, hex and square bar Extruded shapes, angles, channels, some bar

Published typical values for the alloy, from the Copper Development Association data for C36000 and C38500. Lead is nominal composition, not a lot certificate. They describe the material, not a promise from any shop.

The full datasheets are at C360 free-cutting brass and C385 architectural bronze.

Why the name says bronze

Copper alloy naming is historical rather than logical. Bronze, properly, is copper and tin. C385 contains no tin at all. It was sold to architects as a wrought alloy that matched the colour of older cast bronze hardware, and the trade name stuck. The same composition in Europe is CW614N, which nobody calls bronze.

The practical consequence: when an architectural specification says bronze for a handle, a hinge or a window fitting, ask whether it means C385. It usually does, and it is machined like any other leaded brass. For the real difference between the two families, see brass, bronze and copper for machined parts.

Bar against extruded shapes

Both alloys leave the mill by extrusion. C360 is extruded to round, hex and square bar and then drawn for size and straightness, because its job is to be fed into a lathe.

C385, at about 39 percent zinc, carries more of the beta phase that flows well through a die at extrusion temperature. That is why it extrudes into thin, complex profiles: window and door frames, hinge stock, handrail, thresholds, push plates, lock and latch hardware. A part made from it starts as a length of profile, gets cut, drilled, tapped and milled, then polished or plated. Standard profiles are stocked. A custom profile needs an extrusion die and a minimum run, which is cheap next to a forging die but not nothing.

So a turned fitting starts as C360 bar. A hinge leaf or a threshold starts as C385 profile. A part that could be either is normally C360, because the bar is on the shelf.

Machinability: 100 against 90

The same lead particles do the same job in both alloys. They break the chip short and lubricate the cutting edge, so both run dry, both come off the tool bright and both are among the easiest metals a shop will see that week.

The extra zinc in C385 makes it a little stronger, 380 to 480 MPa against 340 to 470, and a little harder, which is where the 90 comes from. In practice the gap in feeds and speeds is small. What differs is the machine the part lands on. C385 profile work is mostly milling and drilling in a fixture. C360 bar work is mostly turning on a bar-fed lathe, which is the cheapest way any brass part gets made. See why brass machining is cheap and where the cost hides.

Polish and plating

Both polish well and both plate well. C385 is the default alloy for visible hardware because it already comes in the profile the hardware needs and it takes a bright polish straight off the buff.

Colour is the detail that catches people. More zinc gives C385 a slightly paler yellow than C360. On a single part nobody notices. On a door where a machined C360 part sits next to extruded C385 trim, both polished and lacquered, the difference shows. If the part has to match architectural trim, machine it from the same alloy as the trim. Under nickel or chrome plating the base metal is hidden and the question goes away. Both alloys need lacquer to hold a polished colour indoors. See surface finishes and plating on brass parts.

Need a quote for this part? Get a quote for your brass parts

Copper content and price

C385 carries 55 to 59 percent copper against 60 to 63 for C360. Brass is priced by weight and copper is the expensive half, so C385 tracks marginally lower per kilo on the copper component. In practice form and stock decide the price. A stocked standard profile is cheap. A custom profile carries a die and a minimum run. An unusual C385 bar size can cost more than C360 bar because nobody stocks it. See brass bar price and the copper market.

Where each is stocked

In the United States, C360 round and hex bar is stocked by every brass distributor in every common size, and C385 is stocked as standard architectural profiles with a short list of bar sizes.

In Europe it is the other way round. CW614N, which matches C385 in composition, is the standard free-machining bar that every mill and distributor carries. CW603N, the true C360 equivalent, is less common. A drawing that says C360 and lands on a European shop usually comes back in CW614N. For most turned parts that is harmless and it shortens the lead time. Where the exact composition matters, for a colour match or a certificate, write the grade you need and expect to wait for it. Where it does not, write C360 or CW614N and let the shop use what it has. The cross reference lists the UNS and EN pairs.

Neither is a water alloy

Both alloys carry about 3 percent lead and both have poor dezincification resistance. NSF/ANSI 372 sets a 0.25 percent weighted average lead limit on wetted potable water surfaces, and either alloy is more than ten times over it on its own. That is a description of the standard, not legal advice. For a drinking water or hot water part the choice is neither of these, see NSF/ANSI 61 and 372 for brass fittings and which brass alloy to specify.

How to pick

  1. Does the part start as an extruded profile? C385.
  2. Is it turned from bar in the United States? C360.
  3. Is it machined in Europe? CW614N is the stocked bar. Accept it, or specify CW603N and expect lead time.
  4. Is it visible, polished and next to architectural trim? C385, so the colour matches.
  5. Otherwise: C360, because the bar is on the shelf.

What to put on the drawing

The alloy with any alternate you accept, written as C360 or CW614N rather than left for the shop to guess. The form, bar or profile, with the profile number if it is a standard section. The finish, polish grade, lacquer or plating specification, because a plated part is machined differently from a polished one. A colour match sample if the part sits next to other brass. And whether the part is wetted, which rules both of these out.

How these two sit among the other machined brass grades is covered in our guide to brass grades.

Have a hardware or fitting drawing that says bronze, brass or nothing at all? Send the drawing with the finish and the form it starts from, and we quote the finished parts and place the work with one of the partner shops that machine both alloys.

Frequently asked questions

Is C385 a bronze or a brass?

A brass. C385 is copper, zinc and about 3 percent lead with no tin, which makes it a leaded brass on the UNS system, the same family as C360. The name architectural bronze is a trade name from the days when the alloy was sold to architects to match older bronze hardware, and it stuck. Read the UNS number rather than the word. On composition it is nearly identical to CW614N, the standard European machining brass.

Can I machine C385 instead of C360?

Yes. It is rated 90 against 100, the same lead does the same job, and on a lathe or a mill the difference in feeds is small. The reason to choose one over the other is the form the part starts from and where it is stocked. C360 is stocked as round and hex bar for turned parts. C385 is stocked as extruded profiles and a limited range of bar, so a turned part in C385 may mean waiting for stock.

Do C360 and C385 look the same when polished?

Close, but not identical. C385 carries more zinc and a little less copper, which gives it a slightly paler yellow than C360 under polish and clear lacquer. Side by side on a door the difference shows. If a machined part sits next to extruded C385 trim and will be polished or lacquered, machine it from C385 so the colour matches. Under nickel or chrome plating the difference disappears, because nobody sees the base metal.

What does a European shop supply when the drawing says C360?

Often CW614N, CuZn39Pb3, which matches C385 in composition rather than C360, because it is the free-machining brass every European mill stocks as bar. CW603N, the true C360 equivalent, is less common there. For most turned parts that substitution is harmless and it shortens lead time. If the exact alloy matters, write it and expect a longer wait. If it does not, write C360 or CW614N and let the shop use what it has.

Alloys in this guide

AlloyLead %Mach.DZR
C360 free-cutting brassC36000 · CuZn36Pb3 / CW603N2.5 to 3.7100Poor
C385 architectural bronzeC38500 · CuZn39Pb3 / CW614N2.5 to 3.590Poor

Published typical values for the alloy. Machinability against C360 at 100. Not a promise from a shop.

Sources

  1. Copper Development Association, C36000 alloy data alloys.copper.org
  2. Copper Development Association, C38500 alloy data alloys.copper.org

Need a quote for this part?

Send the drawing. We read it, send one itemised quote for the finished parts within 24 business hours and place the work with a partner shop that turns brass. Brass only.

Get a quote for your brass parts

Keep reading

Get a quote