Guides / Materials
C360 or C69300: Choosing Between the Leaded and Lead-Free Defaults
Published September 27, 2026. Reviewed for the facts in the corrections log.
C360 is the leaded free-cutting default, machinability 100, 2.5 to 3.7 percent lead, poor dezincification resistance. C69300 silicon brass is the lead-free default, machinability 80, under 0.09 percent lead, roughly twice the tensile strength and highly dezincification resistant, at a higher bar price. Potable water and hot water parts go to C69300, dry industrial parts stay C360.
C360 is what a brass part is made from unless something says otherwise. C69300 is what it is made from when that something is a drinking water rule, hot water or a strength requirement. Both are yellow brass bar and both turn on the same lathes, but they differ enough that a shop which has only run one should not be assumed to run the other.
The short version: C360 is faster to cut, cheaper to buy and stocked everywhere. C69300 clears the lead limit for wetted potable water surfaces, is about twice as strong and does not dezincify. If nothing on the drawing touches drinking water, hot water or a real load, C360. If something does, C69300 or another compliant grade.
Composition and properties
| C360 free-cutting brass | C69300 silicon brass | |
|---|---|---|
| UNS and EN | C36000, CuZn36Pb3, CW603N | C69300, CuZn21Si3P, CW724R |
| Copper | 60 to 63 percent | 73 to 77 percent |
| Zinc | remainder, about 35 percent | remainder, about 21 percent |
| Lead | 2.5 to 3.7 percent | under 0.09 percent |
| Silicon | none | 2.7 to 3.4 percent |
| Machinability, C360 = 100 | 100 | 80 |
| Tensile strength | 340 to 470 MPa | 600 to 700 MPa |
| Hardness | 60 to 80 HRB | 90 to 100 HRB |
| Density | 8.49 g/cm3 | 8.30 g/cm3 |
| Dezincification resistance | Poor | High |
| Under the NSF/ANSI 372 line | No | Yes |
Published typical values for the alloy, from the Copper Development Association data for C36000 and C69300. Lead is nominal composition, not a lot certificate. They describe the material, not a promise from any shop.
The full datasheets are at C360 free-cutting brass and C69300 silicon brass.
What the lead does, and what the silicon does instead
The 3 percent of lead in C360 does not dissolve into the copper and zinc. It sits in the structure as discrete soft particles. At the cutting edge those particles break the chip into short pieces and smear across the tool face as a lubricant, which is the entire reason C360 is the benchmark at 100.
C69300 replaces that mechanism with silicon. Silicon forms hard intermetallic phases inside the copper zinc matrix. Those phases break the chip mechanically rather than by lubrication, and they strengthen the alloy at the same time. The low zinc content, about 21 percent against 35 in C360, together with a small phosphorus addition, is what gives it its dezincification resistance.
It is not C360 with the lead taken out. It is a different alloy that happens to be the same colour.
Machinability: what 80 means on the floor
The rating says 80 against 100. That does not mean 20 percent longer cycles. It means the shop is cutting a metal that behaves differently.
C69300 work hardens. A tool that rubs instead of cutting leaves a hardened skin for the next pass to fight through, so the alloy wants sharp positive rake tooling and a feed that stays in the cut. Cutting forces are higher, which shows up as deflection on slender parts and shorter tool life everywhere. Small deep holes and tapped threads are the pain points. Rolled threads come out better than cut ones. The chips are short, which is the good news, but they are tougher than C360 chips and harder on chip conveyors.
A shop that has run it prices all of that in. A shop that has not will either quote it at C360 prices and discover the difference on the machine, or decline the job. That is why the useful question is whether a shop has shipped C69300 parts, not whether it can run them. See what a lead-free brass shop needs.
Strength
C69300 sits at 600 to 700 MPa tensile against 340 to 470 MPa for C360, with hardness to match. On a thin walled fitting or a thread under load that is straight margin. On a part that was designed around C360 behaviour it is worth a look before swapping, because a press fit, a crimp or a flare that relied on C360 being soft will behave differently in an alloy twice as strong. C69300 also takes some parts away from bronze and stainless on strength grounds while keeping brass cycle times.
Dezincification
C360 at about 35 percent zinc has poor dezincification resistance. In hot water, soft water or seawater spray the zinc leaches out and leaves a porous copper skeleton that looks like brass and holds no pressure. C69300 is rated highly resistant on the ISO 6509 test, which is why it is a better hot water alloy regardless of the lead question. See dezincification resistant brass.
One distinction is worth keeping straight. CW602N, the European DZR grade, carries 1.7 to 2.8 percent lead and is rated 80 on machinability. It answers the dezincification question and not the lead question. C69300 answers both.
Need a quote for this part? Get a quote for your brass parts
Bar price and availability
C69300 is about 75 percent copper against about 61 percent for C360, and copper is the expensive half of any brass, so the bar costs more per kilo and the gap moves with the copper market. See brass bar price and the copper market.
Availability matters more than the price on a repeating part. Mills run less C69300, so it is stocked in fewer diameters and hex sizes, with longer lead times. A size that is routine in C360 may not exist, and the part gets machined down from the next bar up, which adds cycle time and chips. On the drawing, allowing an equivalent lead-free grade instead of naming one alloy gives the shop room to use the bar it can actually get that week.
When each is right
C360. Dry industrial parts, electrical connectors, pneumatic fittings, hydraulic adapters, gas fittings where the code allows it, hardware and any part not wetted by drinking water. One caveat for electrical equipment sold in the EU: RoHS exemption 6(c) for leaded copper alloys was set to expire on 30 June 2027 with a renewal request submitted, see RoHS exemption 6(c) and leaded brass.
C69300. Wetted potable water surfaces in the United States, hot water, soft water, marine spray, food and medical fluid contact and any part that needs more strength than C360 can give.
What to write on the drawing
For C360 the callout is simple, and the temper is worth including because free-cutting brass rod is sold in more than one:
Material: C36000 free-cutting brass per ASTM B16, half hard.
For C69300 the drawing should carry the standard, not only the alloy, because the standard is the requirement and the alloy is one way to meet it:
Wetted component, potable water service.
Material shall comply with NSF/ANSI 372
(0.25 percent weighted average lead, wetted surfaces).
Suggested alloy: C69300 (CW724R) or equivalent lead-free brass.
Mill certificate EN 10204 3.1 required with each lot.
NSF/ANSI 372 sets the 0.25 percent weighted average lead limit on wetted surfaces. It is a composition limit, not a certification of any part or shop, and this is a description of the standard rather than legal advice. For the rod specification itself, ask which one the mill certificate references and write that. See material certificates for brass parts.
The question that decides it
- Is the surface wetted by drinking water in the United States? C69300 or another grade under the NSF/ANSI 372 line.
- Hot water, soft water or marine spray? C69300, or a DZR grade where lead is allowed.
- Thin walls, a thread under load or a strength margin the design needs? C69300.
- None of those? C360, and the quote will be lower for it.
To choose between the lead-free grades after the rule is known, start from the guide to lead free brass.
Not sure which side your part falls on? Send the drawing with the fluid and the service temperature, leave the grade as Not sure, and we quote the finished parts and place the work with one of the partner shops that run the alloy it needs.
Frequently asked questions
Is C69300 harder to machine than C360?
Yes, and the rating of 80 against 100 understates the difference on the floor. C69300 work hardens, so it wants sharp positive rake tooling, a feed that keeps the tool cutting rather than rubbing and more care on small deep holes and tapped threads. Chips are short but tougher and tool life is shorter. A shop that has run it prices those things in. A shop that has not will either quote it like C360 and struggle, or decline.
Can I just replace C360 with C69300 on an existing drawing?
For the lead question, yes, and it is the usual answer. For the mechanical side, review it first. C69300 is roughly twice as strong and noticeably harder, which is good for thin walls and threads under load but changes how the part machines and how it behaves in a press fit. Stock is also thinner, so a bar diameter that was routine in C360 may not exist in C69300 and the part gets machined down from the next size up.
Is C69300 the only lead-free brass?
No. Bismuth brass in the C49300 family also clears the 0.25 percent line and behaves closer to C360 on the lathe, with thinner stock availability. Several other silicon brasses exist under other trade names. That is why the drawing should name the standard, NSF/ANSI 372, with C69300 as a suggested alloy and equivalents allowed, rather than lock the shop to one bar it may not be able to source that week.
Why is C69300 bar more expensive than C360?
Copper. C69300 is 73 to 77 percent copper against 60 to 63 percent for C360, and copper is the expensive half of any brass. The silicon and phosphorus additions cost a little more on top, and mills run smaller volumes of it, so it is stocked in fewer diameters and hex sizes. The per kilo gap moves with the copper market, so ask for the material line separately on the quote rather than assuming a fixed uplift.
Alloys in this guide
| Alloy | Lead % | Mach. | DZR |
|---|---|---|---|
| C360 free-cutting brassC36000 · CuZn36Pb3 / CW603N | 2.5 to 3.7 | 100 | Poor |
| C69300 silicon brassC69300 · CuZn21Si3P / CW724R | under 0.09 | 80 | High |
Published typical values for the alloy. Machinability against C360 at 100. Not a promise from a shop.
Sources
- Copper Development Association, C36000 alloy data alloys.copper.org
- Copper Development Association, C69300 alloy data alloys.copper.org
Need a quote for this part?
Send the drawing. We read it, send one itemised quote for the finished parts within 24 business hours and place the work with a partner shop that turns brass. Brass only.
Get a quote for your brass parts