Skip to content
Brass CNC Parts

Guides / Process

Brass Threaded Inserts for Plastic: Knurl Type, Boss Design and Pull-Out Strength

Published November 10, 2026. Reviewed for the facts in the corrections log.

Pile of small machined brass threaded parts, the same family as brass threaded inserts for plastic

A brass threaded insert holds in plastic by the plastic flowing around its knurl and undercut. Straight knurls resist turning, grooves and diamond patterns resist pull-out. Strength depends on the plastic, the hole size, the boss wall and the setting method, so test the assembly rather than trusting a catalogue figure.

A plastic housing cannot hold a screw through many assembly cycles. The thread wears, the screw strips and the product comes back for repair. A brass insert fixes that by putting a hard, reusable thread into the plastic. The insert is a short brass bush with an internal thread and a knurled outside, and how well it holds depends on a few design choices that a buyer can control.

This post covers the knurl types, the setting methods, the boss and hole design and how to test strength. For the shop side of making inserts, see the brass threaded inserts part page, and for knurl callouts, knurling brass parts.

Diagram: Brass Threaded Inserts for Plastic: Knurl Type and Pull-Out

How an insert holds

An insert holds in two ways. Plastic flows into the knurl grooves and locks against turning. Plastic also flows into undercut grooves and behind flanges, and locks against being pulled out. The more plastic that is trapped and the stronger the plastic, the better the hold. A threaded insert set in a clean hole with enough surrounding plastic can reach the strength of the screw itself.

Knurl and groove types

Feature What it resists Typical use
Straight knurl Turning (torque-out) Inserts that see tightening torque
Diamond knurl Turning and some pull-out General purpose, the most common
Helical knurl, opposed bands Turning and pull-out, both directions Heat-set and ultrasonic inserts
Circumferential groove or undercut Pull-out Molded-in and press-in inserts
Flange or collar Pushing through, sets depth Blind-hole and surface-mount inserts
Tapered body Easier starting, controlled displacement Heat-set inserts

Typical functions of the features. The insert maker’s data sheet takes precedence for each size.

Most catalogue inserts combine a diamond or helical knurl with one or two grooves. A plain straight knurl on its own holds torque but pulls out, which is why it is rarely used alone for a load that acts along the screw axis.

Setting methods

The method decides the insert’s outside shape and the hole design.

  • Heat-set. A heated tip presses the insert into an undersized hole. The plastic softens and flows into the knurl and grooves, then cools and locks. Common for thermoplastics such as ABS, polycarbonate and nylon.
  • Ultrasonic. A horn vibrates the insert, which heats by friction and sinks into the plastic. Fast and well suited to volume assembly.
  • Press-in. The insert is pushed into an undersized hole with no heat. It relies on interference and knurl bite. It suits softer plastics and lower loads.
  • Molded-in. The insert is placed in the mold and the plastic forms around it. Strongest hold, but it slows the molding cycle and the insert must be positioned in the tool.
  • Self-tapping. The insert cuts its own thread in the plastic as it is screwed in. Common in wood and some plastics.

Boss and hole design

Plastic strength around the insert is as important as the insert. A thin boss cracks, and a boss that is too thick sinks on cooling and leaves a dent on the visible face.

Typical guidelines, from insert makers’ data sheets:

  • Boss outer diameter at least twice the insert outer diameter.
  • Hole diameter a little smaller than the insert’s leading diameter, in the range of 0.1 to 0.4 mm smaller, set by the maker for each size and plastic.
  • Hole deeper than the insert by about a millimeter, so displaced plastic has somewhere to go.
  • A lead-in chamfer or taper at the hole mouth to guide the insert.
  • Ribs to support tall bosses, ending below the visible surface to avoid sink marks.

Since plastics differ, one set of dimensions does not fit all. Glass-filled nylon carries a much higher load than polypropylene, and brittle plastics need larger bosses and lower interference. Injection molding describes the process that makes the boss.

Typical strength and why to test

Pull-out strength depends on size, knurl, plastic and setting method, so a general table is only an order of magnitude. Typical figures for heat-set M3 to M5 inserts in common thermoplastics run from a few hundred newtons to over a thousand, and torque-out values run from around one to several newton meters. Reinforced plastics sit at the top of those ranges and unfilled soft plastics at the bottom.

Do not design from those numbers. Build samples with the actual plastic, the actual hole and the real setting process, and test them.

Two tests cover most needs:

  1. Pull-out test. The insert is set in a sample boss. A screw is threaded in and pulled on a tensile tester until the insert or the plastic fails. Record the force and the failure mode.
  2. Torque-out test. A torque wrench or tester turns a screw in the insert until the insert spins or the plastic cracks. Record the torque.

Both tests should be repeated on several samples, and also after thermal cycling if the product sees heat, since plastic relaxes and the hold can fall.

Need a quote for this part? Get a quote for your brass parts

Brass specifics

Brass suits inserts for the reasons set out in the part page: it turns fast, resists corrosion in a housing and does not gall against a steel screw. Typical grade is C360 free-cutting brass. Where lead is restricted, C69300 silicon brass is the usual lead-free choice, with a longer machining time. For electronics, see RoHS exemption 6(c) on the date after which leaded brass may lose its exemption. This is not legal advice.

Cleanliness helps. Oil and chips on the insert reduce adhesion between plastic and brass in a heat-set process, and chips left in the thread can jam a screw. Specify a wash after machining. Thread and knurl burrs should be removed, since a burr can split the plastic or leave a rough thread.

Plating is uncommon but possible. A thin tin or nickel layer protects against tarnish, and some electronics use inserts as grounding points. Say so on the drawing, with limits after plating.

Common failures

Failure Typical cause
Cracked boss Boss too thin, hole too small, plastic brittle or cold
Insert spins in the boss Knurl too fine or shallow, hole too large, too little plastic
Insert pulls out No groove or undercut, plastic relaxed, load along the axis too high
Sink mark on the visible face Boss wall too thick, insert set too hot
Screw jams Chips in the thread, damaged thread start
Insert tilted Hole not square, no lead-in, setting tool misaligned

Typical causes. Samples tested on the real part find most of them.

What to write on the drawing

Threaded insert M4 x 0.7, 6H, overall length 6.0, outside diameter over knurl 6.0 +/- 0.05.
Diamond knurl and one groove, heat-set type. Material C360, or C69300 where lead-free is required.
Chamfered thread entry. Free of burrs. Washed, no oil or chips.
Sample pull-out test in customer plastic reported at first article.

Checklist

  • Setting method stated: heat-set, ultrasonic, press-in, molded-in or self-tapping.
  • Knurl and groove type chosen for torque, pull-out or both.
  • Boss, hole and depth taken from the insert maker’s data sheet for the actual plastic.
  • Pull-out and torque-out tested on real samples.
  • Grade chosen with the lead requirement in mind.
  • Cleaning, burr limits and plating stated.
  • Volume quoted at two or three price breaks.

Need threaded inserts machined in brass? Send the drawing with the setting method and plastic. We quote the finished parts within 24 business hours and place the work with one of the partner shops that turn brass.

Frequently asked questions

What is the difference between pull-out and torque-out?

Pull-out is the axial force that drags the insert out of the plastic. Torque-out is the turning force that spins it in its hole. Straight knurls resist torque-out well. Grooves and undercuts resist pull-out. Most inserts combine both, and a good design tests for each separately.

How big should the boss be around an insert?

A common rule is a boss outer diameter at least twice the insert outer diameter, with a wall thick enough that the plastic does not crack when the insert is set. The insert maker's data sheet gives the figure for each size and each plastic. Thin bosses are the usual reason for cracked housings.

Do brass inserts need to be lead free?

Not always. Leaded brass inserts in electronics fall under RoHS exemption 6(c), which has an expiry date, and some markets and customers ask for lead-free. Silicon brass is the usual lead-free choice for inserts. State the lead requirement on the drawing so the shop quotes the right grade.

Alloys in this guide

AlloyLead %Mach.DZR
C360 free-cutting brassC36000 · CuZn36Pb3 / CW603N2.5 to 3.7100Poor
C69300 silicon brassC69300 · CuZn21Si3P / CW724Runder 0.0980High

Published typical values for the alloy. Machinability against C360 at 100. Not a promise from a shop.

Sources

  1. Wikipedia, Threaded insert en.wikipedia.org
  2. Wikipedia, Injection moulding en.wikipedia.org

Need a quote for this part?

Send the drawing. We read it, send one itemised quote for the finished parts within 24 business hours and place the work with a partner shop that turns brass. Brass only.

Get a quote for your brass parts

Keep reading

Get a quote