Guides / For Shops
Reading a Brass Fitting Drawing From a US or EU Buyer: Threads, Units and Test Notes
Published November 21, 2026. Reviewed for the facts in the corrections log.

Read a foreign brass fitting drawing in this order: title block for units, projection symbol and general tolerance, then each thread callout for its family and sealing method, then the notes for leak test, plating and certificate. Anything you cannot read with certainty becomes a written question before you quote.
A drawing from a US or EU fitting buyer packs a lot of agreement into a few lines. The shop that reads it wrongly cuts a good-looking part that the buyer cannot use, and the lot comes back. Most of those mistakes are not machining mistakes. They are reading mistakes made before the first bar was loaded.
This post gives a reading order for a brass fitting drawing and lists what to confirm in writing before you send a quote.
Start with the title block
The title block holds the agreements that apply to the whole drawing. An engineering drawing typically states the measurement units, the default tolerances and general specification callouts there, with a revision block nearby that lists the versions of the drawing. Read these before any dimension.
Units. The block should name the unit, inches or millimetres. Do not assume. A fitting drawn in inches can carry a few metric callouts, such as a metric thread, and the reverse happens too. Mark each dimension in your own working copy with its unit.
Projection symbol. Third-angle projection is the standard in the United States and in Japan. First-angle projection is used in Europe and most of Asia outside Japan. Both give the same six views and arrange them differently, so the right-side view of a fitting can sit on either side of the front view. The symbol is a small truncated cone shown in two views. If you read a first-angle drawing as third angle, a port can end up on the wrong side of the body.
General tolerance. A US drawing usually ties default tolerances to the number of decimal places shown, so 1.50 and 1.500 are different demands. A European drawing often cites ISO 2768 with a letter. The lowercase letter is the class for linear and angular sizes that carry no tolerance of their own: f fine, m medium, c coarse and v very coarse. For class m the published limits are 0.1 mm for sizes over 0.5 to 3 mm, 0.2 mm over 6 to 30 mm and 0.3 mm over 30 to 120 mm.
A callout such as ISO 2768-mK still turns up on older drawings. The capital K comes from part 2 of the standard, which has been withdrawn and replaced by ISO 22081:2021. If a drawing cites it, ask the buyer which geometric limits they mean.
Revision. Check that the revision on the drawing equals the revision on the purchase order or RFQ. A fitting made to revision B and judged against revision C is a common reason for a dispute that nobody caused on purpose.
Read each thread callout as a family and a seal
Brass fittings exist to seal, so thread callouts matter more than any other line. The key point is that a callout names a thread family, and the family decides how the joint seals. The table lists the families you meet most often on US and EU drawings.
| Callout looks like | Family | How it seals | Confirm before you quote |
|---|---|---|---|
| 1/2-14 NPT | US tapered pipe thread, ASME B1.20.1, 60 degree angle, taper 1 in 16 | The tapered flanks wedge together, usually with tape or paste | Gauge type and position tolerance |
| 1/2-14 NPTF | Dryseal, ASME B1.20.3 | Crest and root heights are adjusted so the flanks interfere and seal without sealant | Whether the buyer means dryseal or plain NPT |
| G 1/2 or 1/2 BSPP | Parallel pipe thread, ISO 228-1, 55 degree flank angle | Not on the thread. A washer or O-ring seals against a face | Sealing face, spot face and surface finish |
| R 1/2, Rc or Rp | Tapered or parallel thread to ISO 7-1, 55 degree flank angle | R and Rc seal on the thread. Rp is the internal parallel thread | Which letter, since taper and parallel gauge differently |
| 7/8-14 UNF with O-ring | Unified straight thread, as in an SAE O-ring boss port | The O-ring compresses into a chamfer. The thread only holds | Groove or chamfer drawing and O-ring size |
| M12 x 1.5 | Metric ISO thread | Depends on the design, often a washer or an O-ring | Tolerance class such as 6g or 6H |
Two points save the most rework. First, an NPT and a BSP thread are not interchangeable, even when the nominal size looks the same: the thread angles differ and one family is tapered where the other is parallel. Second, a parallel thread does not seal by itself. If the callout is G or UNF, look for the sealing face, the O-ring groove or the chamfer on the drawing. If you cannot find it, ask. For the gauges that check each family, see thread gauging brass fittings, and for the family differences see NPT vs BSP brass fittings.
Read the test notes as a method
A note such as “100% leak test” is an instruction without a method. Two shops can read it in two ways and both think they comply. Pull out the four missing items and ask for them.
- Medium. Air, nitrogen, water or helium.
- Pressure and hold time. The value and how long the part is held at it.
- Acceptance rule. No bubbles, or a leak rate limit.
- Order of operations. Before or after plating, and before or after final cleaning.
The acceptance rule decides the equipment. A bubble test pressurises the part under water and shows leaks and where they are, but the result depends on the operator and gives only an estimate of size. A pressure decay test pressurises and isolates the part and measures the loss of pressure over time. It gives a repeatable leak rate, but it does not show where the leak is. A drawing that says “no leakage” with no method leaves you to guess which of the two the buyer will repeat at incoming inspection. The worked case for valve bodies is in leak and pressure testing brass valve bodies.
Turn brass every week? Apply as a partner shop
Material, certificate and finish notes
Notes in the margin often carry the strictest demands. Read them in this order.
- Material. The callout names an alloy, a product standard, an edition and a temper. The guide to brass callouts on a foreign drawing explains what a shop may and may not substitute.
- Lead. A potable water part for the US market falls under the Safe Drinking Water Act, which defines lead free as a weighted average of 0.25 percent lead across the wetted surfaces. A note that says “lead free” is a compliance demand, not a grade name. Ask which grade and which standard.
- Certificate. “Certificate 3.1” refers to EN 10204. A type 3.1 certificate gives results from the delivered heat or lot and is signed by the manufacturer’s authorised representative. A 2.2 report may come from a different lot of the same grade. The certificates post covers the types.
- Finish. Nickel or chrome plating changes thread size. Ask whether the thread must gauge after plating, or whether it is masked.
- Edges. “Break all sharp edges” gives no size. Ask for a limit, and ask whether cross hole burrs inside the bore are in scope.
What to send back before you quote
A short written list protects both sides. Send only the points you could not read with certainty.
Drawing 1234 rev C. Questions before we quote:
1. Unit is mm. The 1/2-14 callout is NPT, not NPTF. Please confirm.
2. G 1/4 port: please send the sealing face detail.
3. Leak test: medium, pressure, hold time and acceptance rule?
4. Is the thread gauged after plating?
5. Certificate: EN 10204 3.1 per lot. Please confirm the grade.
Keep the answers with the purchase order. They are your reference if the lot is judged against a different reading later.
Checklist
- Units, projection symbol, general tolerance and revision read first.
- Every thread callout matched to a family and a sealing method.
- Test notes turned into medium, pressure, hold time and acceptance rule.
- Lead, certificate and plating notes read as separate demands.
- Open points sent to the buyer in writing before the quote.
Talk to us
If you turn brass fittings for buyers in the US or Europe and want to talk about the drawings you handle, apply through the shop page. We reply within 24 business hours.
Frequently asked questions
How do I tell first-angle from third-angle projection on a drawing?
Look for the projection symbol near the title block, a small truncated cone drawn in two views. Third angle is the US and Japanese default and first angle is the usual choice in Europe. The two arrange the same views in a different order, so a side view can sit on the opposite side. Check the symbol before you read the views.
Is a 1/2 NPT thread the same as a 1/2 BSP thread?
No. NPT has a 60 degree thread angle and is tapered. BSP threads have a 55 degree flank angle, and the G version is parallel. A fitting cut to one family will not seal in the other, even when the nominal size looks the same. The callout on the drawing decides which family to cut.
What should I ask when a drawing says 100 percent leak tested?
Ask for the test medium, the pressure, the hold time and the acceptance rule. A bubble test and a pressure decay test judge a part in different ways, so the note is not complete without them. Also ask whether the test is made before or after plating.
What does ISO 2768-mK on a drawing mean?
The lowercase m means medium general tolerances for linear and angular sizes without their own tolerance. The capital K comes from ISO 2768 part 2, which has been withdrawn and replaced by ISO 22081. Older drawings still carry it, so ask the buyer how the geometric part should be read.
Alloys in this guide
| Alloy | Lead % | Mach. | DZR |
|---|---|---|---|
| C360 free-cutting brassC36000 · CuZn36Pb3 / CW603N | 2.5 to 3.7 | 100 | Poor |
Published typical values for the alloy. Machinability against C360 at 100. Not a promise from a shop.
Sources
- Wikipedia, Multiview orthographic projection en.wikipedia.org
- Wikipedia, Engineering drawing en.wikipedia.org
- Wikipedia, National pipe thread en.wikipedia.org
- Wikipedia, British standard pipe thread en.wikipedia.org
- Wevolver, ISO 2768 general tolerances, classes and current status wevolver.com
- US EPA, Use of lead free pipes, fittings, fixtures, solder and flux for drinking water epa.gov
- Cincinnati Test Systems, 5 most common types of leak testing cincinnati-test.com
- JR Fluid, SAE straight thread O-ring port (supplier page) jrfluid.com
Turn brass every week?
Brass CNC Parts sends brass work requests and nothing else. We are your customer: you quote us and we place the purchase order. No fee to join.